# US 2026/0158532 A1 · Harmless-treatment chemical agent for phosphogypsum and engineering application method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0158532 A1
- Document ID: US20260158532A1
- Status: Published application
- Kind: A1
- Application number: 19/446,085
- Filed: 2026-01-12
- Published: 2026-06-11
- Earliest claimed: 2023-07-12
- Assignees: BCEG Environmental Remediation Co., Ltd
- Applicants: Bceg Environmental Remediation Co., Ltd.
- Inventors: Shaoguo KANG; Peng LIU; Bosheng ZHOU; Jiaoyan KONG; Liping LIU; Songlin YANG; Li QIN; Xin LI; Yuanwen LIU; Shupeng LI; Lili GUO
- Web page: https://patentgrep.com/patent/US20260158532A1

## CPC

- B09B 3/70: Chemical treatment, e.g. pH adjustment or oxidation (involving an extraction step B09B3/80)
- B09B 3/25: using mineral binders or matrix
- B09B 3/30: involving mechanical treatment (involving an extraction step B09B3/80)
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- B09B: DISPOSAL OF SOLID WASTE NOT OTHERWISE PROVIDED FOR
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

The present invention belongs to the technical field of solid waste treatment and disposal, concerning a harmless-treatment chemical agent for phosphogypsum and an engineering application method thereof. The chemical agent consists of a powder component and a liquid component, the powder component consists of an alkaline component and talc powder, and the alkaline component is at least one of calcium oxide, magnesium oxide, calcium hydroxide and magnesium hydroxide; the liquid component is an aqueous solution of at least one of a soluble iron salt, a soluble aluminum salt and a soluble calcium salt. The engineering application method comprises: S1 breaking and sieving phosphogypsum into a particle size of 1-5 mm, meanwhile adjusting a content of adsorbed water to 5-10%; S2 mixing evenly the pretreated phosphogypsum with the powder component; S3 adding a liquid component and adjusting a content of adsorbed water to 12-20%; and S4 maintenance and preparation for inspection. It is possible to make full use of the synergistic effects of the components by combining the powder component with the liquid component, and realize a more environmentally friendly and efficient engineering application by adding and mixing the powder and liquid components step by step.

## Claims

### Claim 1

A harmless-treatment chemical agent for phosphogypsum consisting of a powder component and a liquid component,
wherein the powder component consists of an alkaline component and talc powder, and the alkaline component is at least one of calcium oxide, magnesium oxide, calcium hydroxide and magnesium hydroxide; the liquid component is an aqueous solution of at least one of a soluble iron salt, a soluble aluminum salt and a soluble calcium salt;
wherein in the powder component, a weight ratio of the alkaline component to the phosphogypsum to be treated is 0.2%˜1.0%; a weight ratio of the talc powder to the phosphogypsum to be treated is 0.1%˜0.6%; a weight ratio of the liquid component, calculated as solids, to the phosphogypsum to be treated is 0.2˜0.6%.

### Claim 2 (depends on 1)

The harmless-treatment chemical agent for phosphogypsum according to claim 1, wherein the soluble aluminum salt includes at least one of aluminum sulfate, aluminum chloride and poly-aluminum chloride;
the soluble iron salt includes at least one of ferric sulfate, ferric chloride, ferrous sulfate and poly-ferric sulfate;
the soluble calcium salt is calcium chloride.

### Claim 3 (depends on 1)

The harmless-treatment chemical agent for phosphogypsum according to claim 1, wherein in the powder component, a weight ratio of the alkaline component to the talc powder is 2˜5:1.

### Claim 4 (depends on 3)

The harmless-treatment chemical agent for phosphogypsum according to claim 3, wherein the powder component consists of calcium oxide with a weight ratio of 0.40% in proportion of the phosphogypsum to be treated, magnesium oxide with a weight ratio of 0.10% in proportion of the phosphogypsum to be treated, and talc powder with a weight ratio of 0.10% in proportion of the phosphogypsum to be treated, and the liquid component consists of aluminum sulfate with a weight ratio of 0.15% in proportion of the phosphogypsum to be treated and ferric chloride with a weight ratio of 0.10% in proportion of the phosphogypsum to be treated;
or wherein the powder component consists of calcium oxide with a weight ratio of 0.48% in proportion of the phosphogypsum to be treated and talc powder with a weight ratio of 0.12% in proportion of the phosphogypsum to be treated, and the liquid component is polymeric alumina with a weight ratio of 0.40% in proportion of the phosphogypsum to be treated;
or wherein the powder component consists of calcium oxide with a weight ratio of 0.40% in proportion of the phosphogypsum to be treated and talc powder with a weight ratio of 0.20% in proportion of the phosphogypsum to be treated, and the liquid component consists of poly-ferric chloride with a weight ratio of 0.10% in proportion of the phosphogypsum to be treated and ferrous sulfate with a weight ratio of 0.20% in proportion of the phosphogypsum to be treated.

### Claim 5 (depends on 1, 2, 3, 4)

The harmless-treatment chemical agent for phosphogypsum according to any one of claims 1-4, wherein a divergence between distributions of the particle size of the alkaline component and the particle size of the phosphogypsum to be treated is not more than +5%, and a content of active ingredients of the alkaline component is not less than 80%, and fineness of the talc powder is not less than 400 mesh.

### Claim 6

An engineering application method of a harmless-treatment chemical agent for phosphogypsum consisting of a powder component, which consists of an alkaline component selected from at least one of calcium oxide, magnesium oxide, calcium hydroxide and magnesium hydroxide, and talc powder, and a liquid component, which is an aqueous solution of at least one of a soluble iron salt, a soluble aluminum salt and a soluble calcium salt; comprising:
S1 a step of pretreating phosphogypsum, including the processes of breaking and sieving phosphogypsum into a particle size of 1-5 mm, meanwhile adjusting a content of adsorbed water to 5-10%, so as to obtain pretreated phosphogypsum;
S2 a step of adding a powder component, including the process of mixing evenly the pretreated phosphogypsum obtained in step S1 with the powder component of the harmless-treatment chemical agent for phosphogypsum, so as to obtain a mixture;
S3 a step of adding a liquid component, including the processes of adding the liquid component of the harmless-treatment chemical agent for phosphogypsum to the mixture obtained in step S2, and adjusting a content of adsorbed water to 12-20%, so as to obtain a material; and
S4 a step of maintenance and preparation for inspection, including the processes of piling the material obtained in step S3 for maintenance and maintaining moisture of the material to enable sufficient reaction, then carrying out comprehensive utilization as needed after achievability to a standard.

### Claim 7 (depends on 6)

The engineering application method of a harmless-treatment chemical agent for phosphogypsum according to claim 6, wherein the soluble aluminum salt includes at least one of aluminum sulfate, aluminum chloride and poly-aluminum chloride;
the soluble iron salt includes at least one of ferric sulfate, ferric chloride, ferrous sulfate and poly-ferric sulfate;
the soluble calcium salt is calcium chloride.

### Claim 8 (depends on 6)

The engineering application method of a harmless-treatment chemical agent for phosphogypsum according to claim 6, wherein in the powder component, a weight ratio of the alkaline component to the phosphogypsum to be treated is 0.2%˜1.0%; a weight ratio of the talc powder to the phosphogypsum to be treated is 0.1%˜0.6%; a weight ratio of the liquid component, calculated as solids, to the phosphogypsum to be treated is 0.2˜0.6%.

### Claim 9 (depends on 8)

The engineering application method of a harmless-treatment chemical agent for phosphogypsum according to claim 8, wherein in the powder component, a weight ratio of the alkaline component to the talc powder is 2˜5:1.

### Claim 10 (depends on 9)

The engineering application method of a harmless-treatment chemical agent for phosphogypsum according to claim 9, wherein the powder component consists of calcium oxide with a weight ratio of 0.40% in proportion of the phosphogypsum to be treated, magnesium oxide with a weight ratio of 0.10% in proportion of the phosphogypsum to be treated, and talc powder with a weight ratio of 0.10% in proportion of the phosphogypsum to be treated, and the liquid component consists of aluminum sulfate with a weight ratio of 0.15% in proportion of the phosphogypsum to be treated and ferric chloride with a weight ratio of 0.10% in proportion of the phosphogypsum to be treated;
or wherein the powder component consists of calcium oxide with a weight ratio of 0.48% in proportion of the phosphogypsum to be treated and talc powder with a weight ratio of 0.12% in proportion of the phosphogypsum to be treated, and the liquid component is polymeric alumina with a weight ratio of 0.40% in proportion of the phosphogypsum to be treated;
or wherein the powder component consists of calcium oxide with a weight ratio of 0.40% in proportion of the phosphogypsum to be treated and talc powder with a weight ratio of 0.20% in proportion of the phosphogypsum to be treated, and the liquid component consists of poly-ferric chloride with a weight ratio of 0.10% in proportion of the phosphogypsum to be treated and ferrous sulfate with a weight ratio of 0.20% in proportion of the phosphogypsum to be treated.

### Claim 11 (depends on 6, 7, 8, 9, 10)

The engineering application method of a harmless-treatment chemical agent for phosphogypsum according to any one of claims 6-10, wherein a divergence between distributions of the particle size of the alkaline component and the particle size of the phosphogypsum to be treated is not more than +5%, and a content of active ingredients of the alkaline component is not less than 80%, and fineness of the talc powder is not less than 400 mesh.

### Claim 12 (depends on 6, 7, 8, 9, 10)

The engineering application method of a harmless-treatment chemical agent for phosphogypsum according to any one of claims 6-10, wherein in step S3, the process of adding the liquid component during discharging or transferring the mixture obtained in step S2 is executed by means of spraying.

### Claim 13 (depends on 12)

The engineering application method of a harmless-treatment chemical agent for phosphogypsum according to claim 12, wherein in step S4, the surface of the material is coated with a layer of matter, which may be a plastic film, a HDPE film, a non-woven fabric or a plant straw, so as to maintain moisture of the material.

### Claim 14 (depends on 6, 7, 8, 9, 10, 13)

The engineering application method of a harmless-treatment chemical agent for phosphogypsum according to any one of claims 6-10 and 13, wherein in step S4, the process of piling the material is executed for 2-14 days.