# US 2026/0158478 A1 · Tungsten-modified hzsm-5 catalysts and methods for their preparation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0158478 A1
- Document ID: US20260158478A1
- Status: Published application
- Kind: A1
- Application number: 19/368,148
- Filed: 2025-10-24
- Published: 2026-06-11
- Earliest claimed: 2024-10-28
- Assignees: PT Harapan Interaksi Swadaya
- Applicants: PT Harapan Interaksi Swadaya
- Inventors: Sugianto Tandio; Tommy Tjiptadjaja; Hardaning Pranamuda; Eman Suryana; Daffa Dewa Saputra; Rochmadi Rochmadi; Iman Prasetyo; Teguh Ariyanto; Dhea Atika Risnawati; Nova Yoga Pradana
- Web page: https://patentgrep.com/patent/US20260158478A1

## CPC

- B01J 29/48: containing arsenic, antimony, bismuth, vanadium, niobium tantalum, polonium, chromium, molybdenum, tungsten, manganese, technetium or rhenium
- B01J 20/0218: {Compounds of Cr, Mo, W}
- B01J 20/186: {Chemical treatments in view of modifying the properties of the sieve, e.g. increasing the stability or the activity, also decreasing the activity}
- B01J 20/3078: {Thermal treatment, e.g. calcining or pyrolizing}
- B01J 20/3236: {containing metal, other than zeolites, e.g. oxides, hydroxides, sulphides or salts}
- C01B 39/40: using at least one organic template directing agent
- B01J 2229/18: to introduce other elements into or onto the molecular sieve itself
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}

## Abstract

A method of preparing an impregnated catalyst including heating a HZSM-5 material at a temperature of from 50° C. to 60° C. in a vacuum having a pressure of −0.5 bar; dripping a solution of a tungsten-containing compound into the HZSM-5 material at a temperature of 50° C. to impregnate tungsten metal from the tungsten-containing compound into the HZSM-5 material and form the impregnated catalyst so that a ratio of tungsten metal contained in the HZSM-5 material is from 0.1% weight/weight to 2% weight/weight; keeping the impregnated catalyst for 24 hours at room temperature and atmospheric pressure; drying the impregnated catalyst in an oven for 24 hours at a temperature of from 60° C. to 70° C.; and calcining the impregnated catalyst by heating at a heating rate of 2° C./minute until the impregnated catalyst reaches a temperature of 350° C. and then maintaining the impregnated catalyst at a temperature of 350° C.

## Claims

### Claim 1

A method of preparing an impregnated catalyst, the method comprising:
heating a HZSM-5 material at a temperature of from 50° C. to 60° C. in a vacuum having a pressure of −0.5 bar;
dripping a solution of a tungsten-containing compound into the HZSM-5 material at a temperature of 50° C. to impregnate tungsten metal from the tungsten-containing compound into the HZSM-5 material and form the impregnated catalyst so that a ratio of tungsten metal contained in the HZSM-5 material is from 0.1% weight/weight to 2% weight/weight;
keeping the impregnated catalyst for 24 hours at room temperature and atmospheric pressure;
drying the impregnated catalyst in an oven for 24 hours at a temperature of from 60° C. to 70° C.; and
calcining the impregnated catalyst by heating at a heating rate of 2° C./minute until the impregnated catalyst reaches a temperature of 350° C. and then maintaining the impregnated catalyst at a temperature of 350° C.

### Claim 2 (depends on 1)

The method of claim 1, further including mixing the tungsten-containing compound and distilled water.

### Claim 3 (depends on 1)

The method of claim 1, wherein drying occurs at a temperature of 60° C.

### Claim 4 (depends on 1)

The method of claim 1, wherein the tungsten-containing compound is selected from a heteropolyacid and salt forms of the heteropolyacid.

### Claim 5 (depends on 4)

The method of claim 4, wherein the tungsten-containing compound is selected from phosphotungstic acid, silicotungstic acid, tungstic acid, and salt forms of the heteropolyacid.

### Claim 6 (depends on 5)

The method of claim 5, wherein the tungsten-containing compound is phosphotungstic acid having a chemical formula of H3PW12O40.

### Claim 7 (depends on 1)

The method of claim 1, wherein the ratio of tungsten metal contained in the HZSM-5 material is from 0.9% wt/wt to 1.1% wt/wt.

### Claim 8 (depends on 1)

The method of claim 1, wherein the HZSM-5 material before dripping has a Si/Al ratio of from 30 to 62.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the Si/Al ratio is from 32 to 38.

### Claim 10 (depends on 1)

A HZSM-5 catalyst impregnated with the tungsten-containing compound prepared by the method of claim 1.