# US 2026/0152869 A1 · Surface-treated steel sheet and method of producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0152869 A1
- Document ID: US20260152869A1
- Status: Published application
- Kind: A1
- Application number: 19/122,753
- Filed: 2023-07-07
- Published: 2026-06-04
- Earliest claimed: 2022-11-24
- Assignees: Jfe Steel Corporation
- Applicants: Jfe Steel Corporation
- Inventors: Takashi UENO; Yusuke NAKAGAWA
- Web page: https://patentgrep.com/patent/US20260152869A1

## CPC

- C23C 28/345: {with at least one oxide layer}
- C25D 5/48: After-treatment of electroplated surfaces
- C23C 22/36: containing also phosphates
- C23C 28/321: {with at least one metal alloy layer}
- C23C 28/322: {only coatings of metal elements only}
- C25D 5/12: at least one layer being of nickel or chromium
- C25D 7/00: Electroplating characterised by the article coated
- C25D 9/08: by cathodic processes
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR

## Abstract

Provided is a surface-treated steel sheet that can be produced without the use of hexavalent chromium and that has excellent adhesion to BPA-free paint. A surface-treated steel sheet having, on at least one surface of a steel sheet, a Sn plating layer and a coating layer disposed on the Sn plating layer and containing at least one of Zr oxide and Ti oxide, wherein a contact angle of ethylene glycol is 50° or less, and a total atomic ratio of K, Na, Mg, and Ca adsorbed on a surface of the steel sheet to all elements is 5.0% or less.

## Claims

### Claim 1

A surface-treated steel sheet comprising, on at least one side of a steel sheet,
a Sn plating layer; and
a coating layer disposed on the Sn plating layer and containing at least one of Zr oxide and Ti oxide, wherein
a contact angle of ethylene glycol is 50° or less, and
a total atomic ratio of K, Na, Mg, and Ca adsorbed on a surface of the steel sheet to all elements is 5.0% or less.

### Claim 2 (depends on 1)

The surface-treated steel sheet according to claim 1, wherein the Sn plating layer has a Sn coating weight of 0.1 g/m2 to 20.0 g/m2 per side of the steel sheet.

### Claim 3 (depends on 1)

The surface-treated steel sheet according to claim 1, wherein a total coating weight of Zr oxide and Ti oxide in the coating layer is 0.3 mg/m2 to 50.0 mg/m2 per side of the steel sheet in terms of amount of metal Zr and amount of metal Ti.

### Claim 4 (depends on 1)

The surface-treated steel sheet according to claim 1, wherein the coating layer further contains P, and a P coating weight is 50.0 mg/m2 or less per side of the steel sheet.

### Claim 5 (depends on 1)

The surface-treated steel sheet according to claim 1, wherein the coating layer further contains Mn, and a Mn coating weight is 50.0 mg/m2 or less per side of the steel sheet.

### Claim 6 (depends on 1)

The surface-treated steel sheet according to claim 1, further comprising a Ni-containing layer disposed below the Sn plating layer.

### Claim 7 (depends on 6)

The surface-treated steel sheet according to claim 6, wherein the Ni-containing layer has a Ni coating weight of 2 mg/m2 to 2000 mg/m2 per side of the steel sheet.

### Claim 8

A method of producing a surface-treated steel sheet including, on at least one side of a steel sheet, a Sn plating layer, and a coating layer disposed on the Sn plating layer and containing at least one of Zr oxide and Ti oxide, the method comprising:
a coating formation process of treating a surface of a steel sheet having a Sn plating layer on at least one side with an aqueous solution containing at least one of Zr ions and Ti ions to form the coating layer on the Sn plating layer;
a surface conditioning process of holding the aqueous solution at 1.0 g/m2 to 30.0 g/m2 on a surface of the coating layer for 0.1 seconds to 20.0 seconds; and
a water washing process of subjecting the steel sheet after the surface conditioning process to water washing at least once, wherein
in the water washing process,
water with an electrical conductivity of 100 μS/m or less is used at least in the last water washing.

### Claim 9 (depends on 8)

The method of producing a surface-treated steel sheet according to claim 8, wherein the surface-treated steel sheet further includes a Ni-containing layer disposed below the Sn plating layer.