# US 2026/0152589 A1 · Polyethylene compositions and films made therefrom

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0152589 A1
- Document ID: US20260152589A1
- Status: Published application
- Kind: A1
- Application number: 19/102,947
- Filed: 2023-07-17
- Published: 2026-06-04
- Earliest claimed: 2022-08-22
- Applicants: ExxonMobil Chemical Patents Inc.
- Inventors: Martin ANTENSTEINER; Aaron C. MCGINNIS; Wen LI
- Web page: https://patentgrep.com/patent/US20260152589A1

## CPC

- C08F 210/16: Copolymers of ethene with alpha-alkenes, e.g. EP rubbers
- C08F 4/65922: {containing at least two cyclopentadienyl rings, fused or not}
- C08J 5/18: Manufacture of films or sheets
- C08F 2500/08: Low density, i.e. < 0.91 g/cm3
- C08F 2500/26: Use as polymer for film forming
- C08J 2323/08: Copolymers of ethene (C08J2323/16 takes precedence)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)

## Abstract

A polyethylene copolymer useful in producing blown films may include: ethylene units; and 0.1 mol % to 15 wt % of C3-C18 alpha-olefin comonomer units, the polyethylene copolymer having: a density of 0.900 g/cm3 to 0.915 g/cm3, a melt index (MI, determined per ASTM D1238-20 at 190° C. and 2.16 kg loading) (12) of 0.5 g/10 min to 1.5 g/10 min. a melt index ratio of 15 to 40, a cross-fractional chromatography (CFC) central cross moment covariance of less than −500K (kg/mol), a CFC correlation of −0.3 or less, a CFC equal halves Tw1-Tw2 of −30° C. or less and Mw1/Mw2 of 2 or greater, and a temperature rising elution fraction (TREF) T75-T25 30° C. to 36° C.

## Claims

### Claim 1

A polyethylene copolymer comprising:
ethylene units; and
0.1 mol % to 15 wt % of C3-C18 alpha-olefin comonomer units, the polyethylene copolymer having:
a density of 0.900 g/cm3 to 0.915 g/cm3,
a melt index (MI, determined per ASTM D1238-20 at 190° C. and 2.16 kg loading) (12) of 0.5 g/10 min to 1.5 g/10 min,
a melt index ratio of 15 to 40,
a cross-fractional chromatography (CFC) central cross moment covariance of less than −500 K (kg/mol),
a CFC correlation of −0.3 or less,
a CFC equal halves Tw1-Tw2 of −30° C. or less and Mw1/Mw2 of 2 or greater, and
a temperature rising elution fraction (TREF) T75-T25 of 30° C. to 36° C.

### Claim 2 (depends on 1)

The polyethylene copolymer of claim 1, wherein the polyethylene copolymer has density of 0.900 g/cm3 to 0.914 g/cm3.

### Claim 3 (depends on 1)

The polyethylene copolymer of claim 1, wherein the polyethylene copolymer has density of 0.900 g/cm3 to 0.912 g/cm3.

### Claim 4 (depends on 1)

The polyethylene copolymer of claim 1, wherein the polyethylene copolymer has a solubility distribution breadth index (SDBI) of 21.0° C. to 25.0° C.

### Claim 5 (depends on 1)

The polyethylene copolymer of claim 1, wherein the polyethylene copolymer has a short chain branching of 20 branch/1000C to 25 branch/1000C.

### Claim 6 (depends on 1)

The polyethylene copolymer of claim 1, wherein the polyethylene copolymer comprises mol % to 15 mol % of C3-C18 alpha-olefin comonomer units.

### Claim 7 (depends on 1)

The polyethylene copolymer of claim 1, wherein the polyethylene copolymer has a Mw/Mn of 3.7 to 4.3.

### Claim 8

A blown film comprising:
a polyethylene copolymer comprising:
ethylene units; and
0.1 mol % to 15 wt % of C3-C18 alpha-olefin comonomer units, the polyethylene copolymer having:
a density of 0.900 g/cm3 to 0.915 g/cm3,
a melt index (MI, determined per ASTM D1238-20 at 190° C. and 2.16 kg loading) (12) of 0.5 g/10 min to 1.5 g/10 min,
a melt index ratio of 15 to 40,
a cross-fractional chromatography (CFC) central cross moment covariance of less than −500 K (kg/mol),
a CFC correlation of −0.3 or less,
a CFC equal halves Tw1-Tw2 of 30° C. or less and Mw1/Mw2 of 2 or greater, and
a temperature rising elution fraction (TREF) T75-T25 30° C. to 36° C.

### Claim 9 (depends on 8)

The blown film of claim 8, wherein the blown film has one or more of the following properties:
(a) a seal initiation temperature of about 80° C. or less;
(b) a max hot tack force of 13 N/25 mm or greater;
(c) an Elmendorf tear in a machine direction (MD Elmendorf tear) of 200 g/mil or greater;
(d) a dart drop of 500 g/mil to 1200 g/mil;
(e) a puncture peak force of 10.5 lbf/mil to 14.0 lbf/mil; and
(f) a puncture break energy of 35 in*lbs/mil to 47 in*lbs/mil.

### Claim 10 (depends on 9)

The blown film of claim 9, having all of the properties (a)-(f).

### Claim 11 (depends on 9)

The blown film of claim 9, wherein the seal initiation temperature of the blown film is 75° C. or less; and/or wherein the blown film has a max hot tack force of 17 N/25 mm to 22 N/25 mm.

### Claim 12 (depends on 9)

The blown film of claim 9, wherein the MD Elmendorf tear of the blown film is 250 g/mil or greater.

### Claim 13 (depends on 12)

The blown film of claim 12, wherein the MD Elmendorf tear of the blown film is 300 g/mil or greater.