# US 2026/0152440 A1 · Composite wallboard and a preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0152440 A1
- Document ID: US20260152440A1
- Status: Published application
- Kind: A1
- Application number: 19/361,050
- Filed: 2025-10-17
- Published: 2026-06-04
- Earliest claimed: 2024-11-29
- Assignees: China State Construction Hailong Technology Company Limited; Harbin Institute of Technology; Guangdong Hailong Construction Technology Co., Ltd.
- Applicants: China State Construction Hailong Technology Company Limited; Harbin Institute of Technology; Guangdong Hailong Construction Technology Co., Ltd.
- Inventors: Baojun ZHAO; Xiaodong HE; Liping SHI; Xiaoguang WANG; Xiaoliang MA; Yesheng ZHONG; Wenqi ZHANG; Han YANG; Yangyu FU; Weilai ZENG; Zongjun ZHANG; Qiong WANG
- Web page: https://patentgrep.com/patent/US20260152440A1

## CPC

- C04B 28/14: containing calcium sulfate cements {(gypsum-paper plates E04C)}
- B28B 1/087: by means acting on the mould {; Fixation thereof to the mould}
- B28B 19/0015: {on multilayered articles}
- C04B 12/04: Alkali metal or ammonium silicate cements {; Alkyl silicate cements; Silica sol cements; Soluble silicate cements (alkali metal silicates per se, their preparation C01B33/32; ammonium silicates per se, their preparation C01C1/00)}
- C04B 14/42: Glass
- C04B 14/46: Rock wool {; Ceramic or silicate fibres (C04B14/40, C04B14/42 take precedence)}
- C04B 22/0013: {Boron compounds}
- C04B 22/10: containing carbon in the anion, e.g. carbonates
- C04B 22/16: containing phosphorus in the anion, e.g. phosphates
- C04B 24/06: containing hydroxy groups
- C04B 24/16: Sulfur-containing compounds
- C04B 24/2641: {Polyacrylates; Polymethacrylates}
- C04B 24/42: Organo-silicon compounds
- C04B 28/26: Silicates of the alkali metals
- C04B 40/0028: {Aspects relating to the mixing step of the mortar preparation}
- C04B 40/0067: {making use of vibrations}
- B28B 19/0092: {to webs, sheets or the like, e.g. of paper, cardboard}
- C04B 2103/20: Retarders
- C04B 2111/0062: {Gypsum-paper board like materials}
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- B28B: SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS; SHAPING SLAG; SHAPING MIXTURES CONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER (foundry moulding B22C; working stone or stone-like material B28D; shaping of substances in a plastic state, in general B29C; making layered products not composed wholly of these substances B32B)

## Abstract

Provided is a composite wallboard and a preparation method thereof. The composite wallboard is prepared from raw materials. The raw materials include in parts by mass: 700 to 800 parts of calcined gypsum powder, 0.1 to 1.0 part of a retarder, 0.3 to 0.5 part of a foaming agent, 50 to 70 parts of inorganic fiber, 600 to 700 parts of water, 200 to 400 parts of a binder, 20 to 30 parts of a hydrophobic agent, 3 to 5 parts of an acid agent, and 3 to 5 parts of a pH regulator.

## Claims

### Claim 1

A composite wallboard, wherein the composite wallboard is prepared from raw materials, wherein the raw materials comprise in parts by mass: 700 to 780 parts of calcined gypsum powder, 0.1 to 0.40 part of a retarder, 0.3 to 0.45 part of a foaming agent, 50 to 65 parts of inorganic fiber, 600 to 680 parts of water, 200 to 390 parts of a binder, 20 to 24 parts of a hydrophobic agent, 3 to 4.5 parts of an acid agent, and 3.3 to 4.3 parts of a pH regulator;
wherein the retarder is a mixture of citric acid and sodium hexametaphosphate in a mass ratio of 1:(0.3 to 0.5); the foaming agent is sodium dodecyl sulfate; the inorganic fiber is ceramic fiber or glass fiber; and the hydrophobic agent is a mixture of vinyltrimethoxysilane, methyltrimethoxysilane, and hexadecyltrimethoxysilane in a mass ratio of 1:(0.2 to 0.5):(0.1 to 0.3);
wherein the composite wallboard is prepared by a process including:
preparing the raw materials according to the parts by mass;
mixing the water with the hydrophobic agent and the acid agent, stirring until completely hydrolyzed to obtain a solution, standing the solution, then adding the pH regulator to adjust a pH value of the solution to be neutral, then adding the retarder, adding the inorganic fiber after the retarder is completely dissolved, adding the calcined gypsum powder after the inorganic fiber is uniformly dispersed, stirring to obtain a slurry, adding the binder and the foaming agent after the slurry is uniform, and uniformly stirring to obtain a gypsum slurry;
placing a plate or wallpaper at a bottom of a mold, pouring part of the gypsum slurry into the mold for a first casting, placing a first board in the part of the gypsum slurry after a first vibrating, and standing to obtain a first semi-finished product;
performing a second casting on the first semi-finished product, pouring the remaining gypsum slurry into the mold for the second casting, after a second vibrating, obtaining a second semi-finished product, wherein the second vibrating is performed in conditions of vibrating at a vibration frequency of 10 to 15 Hz for 5 to 10 s, and then at a vibration frequency of 50 Hz for 3 to 4 s; and
standing the second semi-finished product at room temperature until completely hardened, then demolding, and drying to obtain the composite wallboard.

### Claim 2

(canceled)

### Claim 3 (depends on 1)

The composite wallboard according to claim 1, wherein the calcined gypsum powder is hemihydrate gypsum, and a main component of the hemihydrate gypsum is CaSO4·1/2H2O;
the binder is a mixture of sodium acrylate, polyvinyl alcohol, and Arabic gum in a mass ratio of 1:(0.5 to 1):(0.5 to 2);
the acid agent is acetic acid; and
the pH regulator is sodium carbonate.

### Claim 4

(canceled)

### Claim 5 (depends on 1)

The composite wallboard according to claim 1, wherein a time of standing the solution is 18 to 24 h, and the pH value is 7.

### Claim 6 (depends on 1)

The composite wallboard according to claim 1, wherein a height of the first casting is 5 to 10 cm, after the first casting, the first vibrating is performed after waiting for 2 to 3 mins, and the first vibrating is performed in conditions that the gypsum slurry is vibrated at a vibration frequency of 10 to 15 Hz for 5 to 10 s, and then vibrated at a vibration frequency of 50 Hz for 3 to 4 s.

### Claim 7 (depends on 1)

The composite wallboard according to claim 1, wherein the first board is an aluminum silicate fiber board or a vacuum insulation board; a thickness of the first board is 5 to 10 mm; and a time of the first board being placed in the part of the gypsum slurry for standing is 1 to 2 h.

### Claim 8 (depends on 1)

The composite wallboard according to claim 1, wherein a height of the second casting is 10 to 25 cm, after the second casting, the second vibrating is performed after waiting for 2 to 3 mins; and a condition of the drying is drying at a temperature of 40 to 60°C for 24 to 48 h.

### Claim 9

A composition for preparing a composite board, wherein the composition comprises the following components in parts by mass: 700 to 780 parts of calcined gypsum powder, 0.1 to 0.40 part of a retarder, 0.3 to 0.45 part of a foaming agent, 50 to 65 parts of inorganic fiber, 600 to 680 parts of water, 200 to 390 parts of a binder, 20 to 24 parts of a hydrophobic agent, 3 to 4.5 parts of an acid agent, and 3.3 to 4.3 parts of a pH regulator;
wherein the calcined gypsum powder is hemihydrate gypsum, and a main component of the hemihydrate gypsum is CaSO4·1/2H2O; the retarder is a mixture of citric acid and sodium hexametaphosphate in a mass ratio of 1:(0.3 to 0.5); the foaming agent is sodium dodecyl sulfate; the inorganic fiber is ceramic fiber or glass fiber; the binder is a mixture of sodium acrylate, polyvinyl alcohol, and Arabic gum in a mass ratio of 1:(0.5 to 1):(0.5 to 2); the hydrophobic agent is a mixture of vinyltrimethoxysilane, methyltrimethoxysilane, and hexadecyltrimethoxysilane in a mass ratio of 1:(0.2 to 0.5):(0.1 to 0.3); the acid agent is acetic acid; and the pH regulator is sodium carbonate.

### Claim 10

(canceled)