# US 2026/0151856 A1 · Method for producing a welded steel blank and associated welded steel blank

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0151856 A1
- Document ID: US20260151856A1
- Status: Published application
- Kind: A1
- Application number: 19/460,537
- Filed: 2026-01-27
- Published: 2026-06-04
- Earliest claimed: 2018-12-24
- Assignees: ArcelorMittal
- Applicants: ArcelorMittal
- Inventors: Francis SCHMIT; Maria POIRIER; Cristian ALVAREZ; Lucille GOUTON; Thierry DAVID; Ivan VIAUX
- Web page: https://patentgrep.com/patent/US20260151856A1

## CPC

- B23K 26/26: of rectilinear seams
- B23K 26/123: {in an atmosphere of particular gases}
- B23K 26/322: involving coated metal parts (using absorbing layers on the workpiece B23K26/18)
- B23K 26/36: Removing material (B23K26/55, B23K26/57 take precedence)
- B23K 26/60: Preliminary treatment
- B23K 33/00: Specially-profiled edge portions of workpieces for making soldering or welding connections; Filling the seams formed thereby
- B23K 26/361: for deburring or mechanical trimming (B23K26/351 takes precedence)
- B23K 33/008: {for automotive applications}
- B23K 2101/006: {Vehicles}
- B23K 2101/18: Sheet panels
- B23K 2101/185: {Tailored blanks}
- B23K 2101/34: Coated articles {; Surface treated articles}
- B23K 2103/04: Steel {or steel} alloys
- B23K 2103/10: Aluminium or alloys thereof
- C22C 38/06: containing aluminium
- F16B 5/08: by means of welds or the like (welding B23K)
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- F16B: DEVICES FOR FASTENING OR SECURING CONSTRUCTIONAL ELEMENTS OR MACHINE PARTS TOGETHER, e.g. NAILS, BOLTS, CIRCLIPS, CLAMPS, CLIPS OR WEDGES; JOINTS OR JOINTING (couplings for transmitting rotation F16D)

## Abstract

A method for producing a welded steel blank (1) includes providing two precoated sheets (2), each comprising a steel substrate (3) having a precoating (5) on each of its two main faces (4), each sheet (2) comprising, on each main face (4), at a weld edge (14), a removal zone (18) in which the precoating (5) is removed over a removal fraction; and butt welding the sheets (2) using a filler wire (20) so as to create a weld joint (22) having an aluminum content AlWJ comprised between 0.1 wt. % and 1.2 wt. %. The composition of the wire (20) and the proportion of wire (20) added is such that the weld joint (22) has: (a) a quenching factor FTWJ such that FTWJ−0.96FTBM≥0, (b) a nickel content NiWJ≤14−3.4×AlWJ and a chromium content CrWJ≤5−2×AlWJ, where AlWJ is the aluminum content of the weld joint (22).

## Claims

### Claim 1

A welded, hot press-formed and cooled steel part comprising:
a first coated steel part portion; and
a second coated steel part portion, each of the first and second coated steel part portions comprising a steel substrate having, on at least one of its main faces, a coating comprising at least iron and aluminum, the first and second coated steel part portions being joined by a weld joint, the weld joint being obtained by laser welding, the laser welding not being a hybrid laser-arc welding, the weld joint having a mean aluminum content AlWJ comprised between 0.1 wt. % and 1.2 wt. %, and the weld joint being further characterized by at least one of:
a quenching factor FTWJ of the weld joint that FTWJ−0.96×FTBM≥0,
where:
FTBM is a quenching factor of a least hardenable steel substrate among the steel substrates of the first and second coated steel part portions, and
the quenching factors FTWJ and FTBM are determined using the following formula: FT=128+1553×C+55×Mn+267×Si+49×Ni+5×Cr−79×Al−2×Ni2−1532×C2−5×Mn2−127×Si2−40×C×Ni−4×Ni×Mn, where Al, Cr, Ni, C, Mn and Si are, respectively, a mean aluminum, chromium, nickel, carbon, manganese and silicon content, expressed in weight percent, of an area whose quenching factor is to be determined, the area being the weld joint in the case of FTWJ and the least hardenable substrate in the case of FTBM,
a mean nickel content NiWJ of the weld joint fulfilling the following relationship: NiWJ≤14−3.4×AlWJ, where AlWJ is the mean aluminum content of the weld joint; or
a mean chromium content CrWJ of the weld joint fulfilling the following relationship: CrWJ≤5−2×AlWJ, where AlWJ is the mean aluminum content of the weld joint, and
each coated steel part portion comprising, on each main face thereof, adjacent the weld joint, an intermediate zone in which a thickness of the coating is strictly smaller than in adjacent zones of the coated steel part portion located at a greater distance from the weld joint than the intermediate zone or in which the coating is absent.

### Claim 2 (depends on 1)

The welded, hot press-formed and cooled steel part according to claim 1, wherein the steel of the substrate of at least one of the first and second steel part portions comprising, by weight:
0.1
%
≤
C
≤
0.5
%
0.5
%
≤
Mn
≤
4.5
%
0.1
%
≤
Si
≤
1
⁢
%
B
≤
0.01
%
.

### Claim 3 (depends on 1)

The welded, hot press-formed and cooled steel part according to claim 1, wherein each intermediate zone comprises solidification striations, the solidification striations on adjacent main faces of the two coated steel part portions being symmetrical relative to a vertical median plane between the two coated steel part portions.

### Claim 4 (depends on 1)

The welded, hot press-formed and cooled steel part according to claim 1, wherein each intermediate zone comprises an inner edge located at the weld joint and an outer edge located away from the weld joint, wherein a distance between the outer edges of the adjacent intermediate zones of the two coated steel part portions is constant along a longitudinal direction of the weld joint.

### Claim 5 (depends on 1)

The welded, hot press-formed and cooled steel part according to claim 1, wherein a mean hardness HVmean(WJ) in the weld joint is smaller than or equal to 700 HV.

### Claim 6 (depends on 1)

The welded, hot press-formed and cooled steel part according to claim 1, wherein the mean nickel content NiWJ of the weld joint is comprised between 0.1 wt. % and 13.6 wt. %.

### Claim 7 (depends on 1)

The welded, hot press-formed and cooled steel part according to claim 1, wherein:
a Charpy energy of the weld joint at 20° C. is greater than or equal to 25 J/cm2; and
an ultimate tensile strength of the welded, hot press-formed and cooled steel part is greater than or equal to an ultimate tensile strength of a weakest substrate among the substrates of the coated steel part portions, the weakest substrate being the substrate for which a product of a thickness of the substrate and the ultimate tensile strength of the substrate is the lowest.

### Claim 8 (depends on 1)

The welded, hot press-formed and cooled steel part according to claim 1, wherein a maximum hardness variation ΔHV(WJ) across the weld joint is smaller than or equal to 20% of a mean hardness HVmean(WJ) of the weld joint.

### Claim 9 (depends on 1)

The welded, hot press-formed and cooled steel part according to claim 1, wherein the steel of the substrate of one among the first and the second coated steel part portions comprises, by weight:
0.04
%
≤
C
≤
0.1
%
0.8
%
≤
Mn
≤
2.
%
Si
≤
0.3
%
.

### Claim 10 (depends on 1)

The welded, hot press-formed and cooled steel part according to claim 1, wherein the substrate has a thickness between 0.8 mm and 3.0 mm.

### Claim 11 (depends on 1)

A method for producing an anti-intrusion part or an energy-absorption part for a motor vehicle comprising:
producing the anti-intrusion part or an energy-absorption part using the welded, hot press-formed and cooled steel part according to claim 1,
wherein the substrate has a thickness between 0.8 mm and 3.0 mm.

### Claim 12

A method for producing a welded steel blank comprising the successive steps of:
providing two precoated sheets, each precoated sheet comprising a steel substrate having a precoating on each of its two main faces, the precoating comprising an intermetallic alloy layer comprising at least iron and aluminum, each precoated sheet comprising, on each main face thereof, at a weld edge configured for being incorporated at least partially into a weld joint, a removal zone in which the precoating has been removed over a removal fraction comprised from 30% to 100% of a thickness of the precoating;
butt welding the precoated sheets using a filler wire so as to create the weld joint at a junction between the precoated sheets, the weld joint having a mean aluminum content AlWJ comprised between 0.1 wt. % and 1.2 wt. %, the composition of the filler wire and a proportion of filler wire added to the weld pool being such that the created weld joint is characterized by at least one of the following:
a quenching factor FTWJ of the weld joint such that FTWJ−0.96×FTBM≥0,
where:
FTBM is a quenching factor of a least hardenable steel substrate among the steel substrates of the two precoated sheets, and
the quenching factors FTWJ and FTBM are determined using the following formula: FT=128+1553×C+55×Mn+267×Si+49×Ni+5×Cr−79×Al−2×Ni2−1532×C2−5×Mn2−127×Si2−40×C×Ni−4×Ni×Mn, where Al, Cr, Ni, C, Mn and Si are, respectively, a mean aluminum, chromium, nickel, carbon, manganese and silicon content, expressed in weight percent, of an area whose quenching factor is to be determined, the area being the weld joint in a case of FTWJ and the least hardenable steel substrate in the case of FTBM,
a mean nickel content NiWJ of the weld joint fulfilling the following relationship: NiWJ≤14−3.4×AlWJ, where AlWJ is the mean aluminum content of the weld joint; or
a mean chromium content CrWJ of the weld joint fulfilling the following relationship: CrWJ≤5−2×AlWJ, where AlWJ is the mean aluminum content of the weld joint.

### Claim 13 (depends on 12)

The method according to claim 12, wherein the filler wire has a carbon content comprised between 0.01 wt. % and 0.45 wt. %.

### Claim 14 (depends on 12)

The method according to claim 12, wherein, for at least one of the precoated sheets, the removal fraction is strictly smaller than 100% of the thickness of the precoating.

### Claim 15 (depends on 14)

The method according to claim 14, wherein, for at least one of the precoated sheets, the precoating comprises a metallic alloy layer extending atop the intermetallic alloy layer, the metallic alloy layer being a layer of aluminum, a layer of aluminum alloy or a layer of aluminum-based alloy and wherein, for at least one of the precoated sheets, the metallic alloy layer has been removed over the entire thickness of the metallic alloy layer, while the intermetallic alloy layer remains integral in the removal zone on each main face of the precoated sheet.

### Claim 16 (depends on 12)

The method according to claim 12, wherein the welding step is performed using a laser beam.

### Claim 17 (depends on 12)

The method according to claim 12, wherein, for at least one of the precoated sheets, the steel of the substrate comprises, by weight:
0.1
%
≤
C
≤
0.5
%
0.5
%
≤
Mn
≤
4.5
%
0.1
%
≤
Si
≤
1
⁢
%
B
≤
0.01
%
.

### Claim 18

A welded steel blank comprising:
two precoated sheets, each precoated sheet comprising a steel substrate having a precoating on each of its main faces, the precoating comprising an intermetallic alloy layer comprising at least iron and aluminum, the precoated sheets being joined by a weld joint, the weld joint being obtained by laser welding, the laser welding not being a hybrid laser-arc welding, the weld joint having a mean aluminum content AlWJ comprised between 0.1 wt. % and 1.2 wt. %, and the weld joint being further characterized by at least one of:
a quenching factor FTWJ of the weld joint such that FTWJ−0.96×FTBM≥0,
where:
FTBM is a quenching factor of a least hardenable steel substrate among the steel substrates of the two precoated sheets, and
the quenching factors FTWJ and FTBM are determined using the following formula: FT=128+1553×C+55×Mn+267×Si+49×Ni+5×Cr−79×Al−2×Ni2−1532×C2−5×Mn2−127×Si2−40×C×Ni−4×Ni×Mn, where Al, Cr, Ni, C, Mn and Si are, respectively, a mean aluminum, chromium, nickel, carbon, manganese and silicon content, expressed in weight percent, of an area whose quenching factor is to be determined, the area being the weld joint in the case of FTWJ and the least hardenable steel substrate in the case of FTBM,
a mean nickel content NiWJ of the weld joint fulfilling the following relationship: NiWJ≤14−3.4×AlWJ, where AlWJ is the mean aluminum content of the weld joint; or
a mean chromium content CrWJ of the weld joint fulfilling the following relationship: CrWJ≤5−2×AlWJ, where AlWJ is the mean aluminum content of the weld joint, and
each precoated sheet comprising, on each main face thereof, adjacent the weld joint, an intermediate zone in which the precoating has been removed over a removal fraction comprised from 30% to 100% of a thickness of the precoating.

### Claim 19 (depends on 18)

The welded steel blank according to claim 18, wherein the steel of the substrate of at least one of the precoated sheets comprises, by weight:
0.1
%
≤
C
≤
0.5
%
0.5
%
≤
Mn
≤
4.5
%
B
≤
0.01
%
.

### Claim 20 (depends on 18)

The welded steel blank according to claim 18, wherein the substrate has a thickness between 0.8 mm and 3.0 mm.