# US 2026/0151829 A1 · Articles for containing a molten material and methods of producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0151829 A1
- Document ID: US20260151829A1
- Status: Published application
- Kind: A1
- Application number: 19/406,715
- Filed: 2025-12-02
- Published: 2026-06-04
- Earliest claimed: 2024-12-03
- Assignees: Battelle Energy Alliance, LLC
- Applicants: Battelle Energy Alliance, LLC
- Inventors: Prabhat K. Tripathy; Kenneth C. Marsden; James A. King; David D. Tolman; Kevin R. Tolman
- Web page: https://patentgrep.com/patent/US20260151829A1

## CPC

- B22D 41/02: Linings
- C25D 3/66: from melts
- C25D 5/50: by heat-treatment
- C25D 5/54: Electroplating of non-metallic surfaces (C25D7/12 takes precedence)
- C25D 7/04: Tubes; Rings; Hollow bodies
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR

## Abstract

An article comprises a crucible and a composite coating having a first surface adjacent an inner surface of the crucible and a second surface opposite the first surface. The second surface of the composite coating defines an exposed interior surface of the article. The composite coating comprises at least one carbide of a transition metal. The composite coating includes a gradient of carbon across a thickness of the composite coating between the first surface and the second surface of the composite coating. A method of producing the article comprises electroplating a transition metal on a surface of a crucible from a molten salt electrolyte to form a coated crucible. The method further comprises annealing the coated crucible under an inert atmosphere to form an annealed crucible comprising a composite coating on the surface of the annealed crucible. The composite coating comprises at least one carbide of the transition metal.

## Claims

### Claim 1

An article for containing a molten material, comprising:
a crucible; and
a composite coating having a first surface adjacent an inner surface of the crucible and a second surface opposite the first surface, the second surface of the composite coating defining an exposed interior surface of the article,
the composite coating comprising at least one carbide of a transition metal, the composite coating including a gradient of carbon across a thickness of the composite coating between the first surface and the second surface of the composite coating.

### Claim 2 (depends on 1)

The article of claim 1, wherein the first surface of the composite coating comprises a greater carbon content than the second surface of the composite coating.

### Claim 3 (depends on 1)

The article of claim 1, wherein the crucible comprises a high-density graphite.

### Claim 4 (depends on 1)

The article of claim 1, wherein the composite coating and the crucible exhibit substantially a same thermal expansion coefficient value.

### Claim 5 (depends on 1)

The article of claim 1, wherein the transition metal comprises yttrium (Y), niobium (Nb), tantalum (Ta), titanium (Ti), tungsten (W), molybdenum (Mo), hafnium (Hf), vanadium (Va), Zirconium (Zr), or a combination thereof.

### Claim 6 (depends on 1)

The article of claim 1, wherein the composite coating comprises at least one yttrium carbide including YC, Y2C, YC2, or a combination thereof.

### Claim 7 (depends on 1)

The article of claim 1, wherein the composite coating further comprises the transition metal, an oxide of the transition metal, a rare earth element, an oxide of the rare earth element, or any combination thereof.

### Claim 8 (depends on 1)

The article of claim 1, wherein the composite coating comprises:
niobium (Nb) and at least one metal carbide chosen from NbC and Nb2C;
tantalum (Ta) and at least one metal carbide chosen from TaC and Ta2C;
niobium (Nb) and at least one metal carbide chosen from TaC, Ta2C, NbC, and Nb2C;
hafnium (Hf) and hafnium carbide (HfC);
at least one metal carbide chosen from MoC and Mo2C; or
tungsten (W) and at least one metal carbide chosen from WC and W2C.

### Claim 9 (depends on 1)

The article of claim 1, further comprising a topcoat adjacent to the second surface of the composite coating.

### Claim 10 (depends on 9)

The article of claim 9, wherein the topcoat comprises a metal, a metal alloy, a metal oxide, a metal nitride, a metal boride, or a combination thereof.

### Claim 11 (depends on 10)

The article of claim 10, wherein the topcoat comprises magnesium oxide, calcium oxide, aluminum titanium oxide (Al2TiO3), scandium oxide, yttrium oxide, hafnium oxide, zirconium oxide, thorium oxide, an oxide of a lanthanide metal, hafnium nitride, hafnium boride, molybdenum boride, niobium boride, nickel boride, tantalum boride, titanium nitride, titanium boride, vanadium boride, zirconium nitride, zirconium boride, or a combination thereof.

### Claim 12

An article for containing a molten material, comprising:
a crucible;
a composite coating including one side adjacent to an inner surface of the crucible and another side defining an exposed interior surface of the article, the composite coating comprising:
one or more layers of at least one carbide of a transition metal proximal to the inner surface of the crucible; and
at least one layer of the transition metal distal from the inner surface of the crucible; and
at least one layer of an oxide of the transition metal adjacent to the another side of the composite coating.

### Claim 13 (depends on 12)

The article of claim 12, wherein the composite coating comprises:
layers of TaC, Ta2C, and Ta;
layers of NbC, Nb2C, and Nb;
layers of TaC, Ta2C, NbC, Nb2C, and Nb;
layers of HfC and Hf;
layers of MoC and Mo2C;
layers of YC, Y2C, and YC2; or
layers of WC, W2C, and W.

### Claim 14 (depends on 12)

The article of claim 12, wherein the composite coating is in contact with the crucible.

### Claim 15

A method of producing an article for containing a molten material, comprising:
electroplating a transition metal on a surface of a crucible from a molten salt electrolyte to form a coated crucible; and
annealing the coated crucible under an inert atmosphere to form an annealed crucible comprising
a composite coating on the surface of the annealed crucible, the composite coating
comprising at least one carbide of the transition metal.

### Claim 16 (depends on 15)

The method of claim 15, wherein the electroplating the transition metal on the surface of the crucible comprises conducting the electroplating at a temperature of from about 350° C. to about 450° C.

### Claim 17 (depends on 15)

The method of claim 15, wherein annealing the coated crucible under the inert atmosphere comprises converting at least a portion of the coated crucible to the at least one carbide of the transition metal.

### Claim 18 (depends on 15)

The method of claim 15, wherein annealing the coated crucible under the inert atmosphere to form the annealed crucible comprises heating the coated crucible to a temperature of from about 500° C. to about 700° C. for up to about 12 hours.

### Claim 19 (depends on 15)

The method of claim 15, further comprising repeating the electroplating and the annealing for at least one more time.

### Claim 20 (depends on 15)

The method of claim 15, further comprising anodizing the annealed crucible to form an oxide layer on an exposed surface of the composite coating.