# US 2026/0151756 A1 · Method for preparing catalyst using recycled waste batteries and application of the catalyst

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0151756 A1
- Document ID: US20260151756A1
- Status: Published application
- Kind: A1
- Application number: 18/966,579
- Filed: 2024-12-03
- Published: 2026-06-04
- Earliest claimed: 2024-12-03
- Assignees: Guizhou Normal University
- Applicants: Guizhou Normal University
- Inventors: Wei Gong; Mo Liu; Yang Dai; Zhen Yao
- Web page: https://patentgrep.com/patent/US20260151756A1

## CPC

- B01J 23/8986: {with manganese, technetium or rhenium}
- B01J 23/8892: {Manganese}
- B01J 35/397: {Egg shell like}
- B01J 35/40: characterised by dimensions, e.g. grain size (in a colloidal state B01J35/23; crystallite size B01J35/77)
- B01J 37/0036: {Grinding}
- B01J 37/0236: {Drying, e.g. preparing a suspension, adding a soluble salt and drying}
- B01J 37/04: Mixing {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- C22B 7/007: {by acid leaching}
- H01M 10/54: Reclaiming serviceable parts of waste accumulators
- Y02W 30/84: Recycling of batteries or fuel cells
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

Provided herein is a method for preparing a catalyst form recycled waste batteries, which includes the preparation of a NiCoMnOx composite oxide, and further extends to the preparation of a perovskite catalyst and a core-shell loaded noble catalyst.

## Claims

### Claim 1

A catalyst prepared from recycled waste batteries, comprising:
a shell structure,
a core structure prepared from valuable components of waste ternary lithium power batteries, and
a gap layer between the core structure and the shell structure,
wherein the core structure is composed of a composite metal oxide consisting of NiO, Co3O4 and MnO2,
wherein the shell structure is a manganese dioxide layer covering a surface of the core structure, and the manganese dioxide layer is provided with at least two through-channels,
wherein noble metals Pt and/or Ru are loaded on an outer surface of the manganese dioxide layer and inside the gap layer.

### Claim 2 (depends on 1)

The catalyst according to claim 1, wherein the through-channels are formed by thermal decomposition of polymethylmethacrylate microspheres in the shell structure during calcination.

### Claim 3 (depends on 1)

The catalyst according to claim 1, wherein the noble metals Pt and Ru have amounts of 0.2% and 0.6% respectively.

### Claim 4 (depends on 1)

The catalyst according to claim 1, wherein the composite metal oxide is extracted from the waste ternary lithium power batteries, wherein a mass fraction of NiO is 20%-40%, a mass fraction of Co3O4 is 30%-50% and a mass fraction of MnO2 is 20%-30%.

### Claim 5 (depends on 4)

The catalyst according to claim 4, wherein the mass fractions of NiO, Co3O4 and MnO2 in the composite metal oxide are 20% NiO, 50% Co3O4, and 30% MnO2.

### Claim 6

A method for preparing a catalyst form recycled waste batteries, comprising:
extracting valuable metals from cathode materials of waste ternary power batteries with an inorganic acid to form Ni, Co, and Mn precursor salts, wherein the inorganic acid is selected from the group consisting of H2SO4, HNO3 and HCl;
adding a precipitant to the precursor salts to generate a composite metal precipitate, wherein the precipitant is selected from the group consisting of Na2CO3, saturated NH4(NO3)2, NH3·H2O and NaOH;
calcining the composite metal precipitate to prepare a NiCoMnOx composite metal oxide containing NiO, Co3O4 and MnO2;
pulverizing the composite metal oxide to a particle size of 200 μm-250 μm to obtain a powder of the composite metal oxide, uniformly dispersing polymethyl methacrylate microspheres, manganese dioxide particles and α-hemihydrate gypsum in anhydrous ethanol to obtain a mixed material, spraying the mixed material on a surface of the powder of the composite metal oxide, and drying to form a mixed material layer on the surface of the powder of the composite metal oxide to obtain a composite intermediate;
adding 0.3 g-1.2 g of potassium permanganate into 20 g-25 g of 0.2 mol/L sodium hydroxide solution to obtain an alkaline potassium permanganate solution;
dispersing the composite intermediate in the anhydrous ethanol, then adding 0.2 mol/L sodium hydroxide solution, and stirring to form a suspension, wherein a mass ratio of the composite intermediate, the anhydrous ethanol, and the sodium hydroxide solution is 1:(80-100):(2.5-5);
dropping slowly the alkaline potassium permanganate solution into the suspension, wherein the volume ratio of the suspension to the alkaline potassium permanganate solution is 100:(5-10), then stirring them and allowing the reaction to proceed for 300 minutes, filtering out a first solid after the reaction, repeatedly washing the first solid with deionized water, and then drying at 80° C. to obtain composite microspheres;
adding the composite microspheres into deionized water, dissolving α-hemihydrate gypsum, filtering out a second solid, washing the second solid with deionized water to obtain a catalyst microsphere intermediate I, calcining the catalyst microsphere intermediate I at 280° C. for 2 to 3 hours, then cooling, and then adding deionized water for ultrasonic washing and drying to obtain a catalyst microsphere intermediate II;
immersing the catalyst microsphere intermediate II in a noble metal precursor solution, filtering out a third solid, then drying and grinding the third solid and placing them it into a tube furnace, and then introducing a 10% H2/Ar gas mixture and maintaining at 400° C. for 4 hours to obtain a core-shell loaded noble metal catalyst.

### Claim 7 (depends on 6)

The method according to claim 6, wherein, a particle size of the polymethyl methacrylate microspheres is 80 μm-100 μm, a particle size of the manganese dioxide particles is 100 nm-200 nm, a particle size of the α-hemihydrate gypsum is 5 μm-10 μm, and a thickness of the mixed material layer is 70 μm-160 μm.

### Claim 8 (depends on 6)

The method according to claim 6, wherein, a mass ratio of the polymethyl methacrylate microspheres, the manganese dioxide particles, the α-hemihydrate gypsum, and the anhydrous ethanol is 1:(0.5-1): 3: 6.

### Claim 9 (depends on 6)

The method according to claim 6, wherein, the noble metal precursor solution is at least one of: H2PtCl6 or RuCl3 solution, and wherein the noble metals Pt and Ru have amounts of 0.2% and 0.6% respectively.

### Claim 10 (depends on 1)

Use of the catalyst according to claim 1 for catalysis of at least one of: VOCs catalytic combustion, CO oxidation and alkane catalytic oxidation.