# US 2026/0150319 A1 · Method for producing a semiconductor structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0150319 A1
- Document ID: US20260150319A1
- Status: Published application
- Kind: A1
- Application number: 19/396,572
- Filed: 2025-11-21
- Published: 2026-05-28
- Earliest claimed: 2024-11-27
- Assignees: Imec Vzw
- Applicants: Imec Vzw
- Inventors: Jishnu Ganguly; Naoto Horiguchi; Joao Bastos
- Web page: https://patentgrep.com/patent/US20260150319A1

## CPC

- H10D 30/0245: {by further thinning the channel after patterning the channel, e.g. using sacrificial oxidation on fins}
- G11C 5/063: {Voltage and signal distribution in integrated semi-conductor memory access lines, e.g. word-line, bit-line, cross-over resistance, propagation delay}
- H10B 41/41: of a memory region comprising a cell select transistor, e.g. NAND
- H10B 43/40: characterised by the peripheral circuit region
- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 62/83: being Group IV materials, e.g. B-doped Si or undoped Ge
- H10P 14/6309: {of silicon in uncombined form, i.e. pure silicon}
- H10B 41/20: characterised by three-dimensional [3D] arrangements, e.g. with cells on different height levels
- H10B 43/20: characterised by three-dimensional [3D] arrangements, e.g. with cells on different height levels
- H10D 30/6213: {having rounded corners}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- G11C: STATIC STORES (semiconductor memory devices H10B)
- H10B: ELECTRONIC MEMORY DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The present disclosure relates to method for producing a semiconductor structure. The method comprises: providing a semiconductor fin on a substrate, the semiconductor fin comprising a first side surface, a second side surface opposing the first side surface, and a top surface, wherein a mask covers the top surface of the semiconductor fin; exposing a portion of the top surface of the semiconductor fin by removing a portion of the mask, the exposed portion of the top surface and the first side surface forming an exposed top corner of the semiconductor fin; rounding the exposed top corner of the semiconductor fin by oxidizing the exposed portion of the top surface and the first side surface.

## Claims

### Claim 1

A method for producing a semiconductor structure, the method comprising:
providing a semiconductor fin on a substrate, the semiconductor fin comprising a first side surface, a second side surface opposing the first side surface, and a top surface, wherein a mask covers the top surface of the semiconductor fin;
exposing a portion of the top surface of the semiconductor fin by removing a portion of the mask, the exposed portion of the top surface and the first side surface forming an exposed top corner of the semiconductor fin; and
rounding the exposed top corner of the semiconductor fin by oxidizing the exposed portion of the top surface and the first side surface.

### Claim 2 (depends on 1)

The method according to claim 1, wherein a width of the exposed portion of the top surface of the semiconductor fin is at least 5% of a width of the fin.

### Claim 3 (depends on 2)

The method according to claim 2, wherein removing the portion of the mask comprises laterally etching at least part of the mask.

### Claim 4 (depends on 3)

The method according to claim 3, wherein laterally etching the mask comprises wet etching.

### Claim 5 (depends on 1)

The method according to claim 1, wherein removing the portion of the mask comprises laterally etching at least part of the mask.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the mask comprises a first layer and a second layer, the first layer being arranged between the top surface of the semiconductor fin and the second layer,
wherein removing the portion of the mask comprises
removing a first portion of the first layer of the mask; and
removing a first portion of the second layer of the mask;
wherein the first portion of the second layer of the mask is a portion above the first portion of the first layer of the mask.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the mask comprises a first layer and a second layer, the first layer being arranged between the top surface of the semiconductor fin and the second layer,
wherein removing the portion of the mask comprises
removing a first portion of the first layer of the mask; and
removing a first portion of the second layer of the mask;
wherein the first portion of the second layer of the mask is a portion above the first portion of the first layer of the mask.

### Claim 8 (depends on 7)

The method according to claim 7, wherein a width of the removed first portion of the second layer of the mask is larger than a width of the removed first portion of the first layer of the mask.

### Claim 9 (depends on 7)

The method according to claim 7, wherein
removing the first portion of the first layer of the mask is performed in a first etch process; and
removing the first portion of the second layer of the mask is performed in a second etch process, the second etch process being subsequent to the first etch process.

### Claim 10 (depends on 9)

The method according to claim 9, wherein oxidizing the exposed portion of the top surface and the first side surface is performed by wet oxidation.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the wet oxidation comprises an in-situ steam generation, ISSG, process.

### Claim 12 (depends on 1)

The method according to claim 1, wherein oxidizing the exposed portion of the top surface and the first side surface is performed by wet oxidation.

### Claim 13 (depends on 1)

The method according to claim 1, further comprising conformally coating the semiconductor fin with a gate oxide layer.

### Claim 14 (depends on 13)

The method according to claim 13, the method further comprising removing oxide formed during the step of oxidizing the exposed portion of the top surface and the first side surface, wherein removing said oxide is performed before the step of conformally coating the semiconductor fin with the gate oxide layer.

### Claim 15 (depends on 14)

The method according to claim 14, wherein the gate oxide layer has a thickness of at least 10 nm.

### Claim 16 (depends on 13)

The method according to claim 13 wherein the gate oxide layer has a thickness of at least 10 nm.

### Claim 17 (depends on 13)

The method according to claim 13, wherein a length of the fin is at least 100 nm.

### Claim 18 (depends on 1)

The method according to claim 1, wherein a length of the fin is at least 100 nm.

### Claim 19 (depends on 1)

The method according to claim 1, wherein the semiconductor fin comprises silicon.

### Claim 20 (depends on 1)

The method according to claim 1, further comprising:
forming a 3D-NAND memory system on the substrate; and
forming a wordline transistor on the substrate, wherein a channel region of the wordline transistor comprises the semiconductor fin.