# US 2026/0148994 A1 · Negative electrode for all-solid-state battery, all-solid-state battery containing the same, and method for manufacturing a negative electrode for all-solid-state battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0148994 A1
- Document ID: US20260148994A1
- Status: Published application
- Kind: A1
- Application number: 19/395,567
- Filed: 2025-11-20
- Published: 2026-05-28
- Earliest claimed: 2024-11-25
- Assignees: Samsung SDI Co., Ltd.
- Applicants: Samsung SDI Co., Ltd.
- Inventors: Jiwon HAN; Seunghyun OH; Jangwook LEE; Bohyung LEE
- Web page: https://patentgrep.com/patent/US20260148994A1

## CPC

- H01M 4/628: {Inhibitors, e.g. gassing inhibitors, corrosion inhibitors}
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/0442: {Anodisation, Oxidation (electrolytic coating by anodisation C25D9/00)}
- H01M 4/13: Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/625: {Carbon or graphite}
- H01M 10/052: Li-accumulators
- H01M 10/0562: Solid materials
- H01M 2004/027: {Negative electrodes}
- H01M 2300/0068: inorganic
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Provided is a negative electrode for an all-solid-state battery, an all-solid-state battery including the negative electrode, and a method for manufacturing a negative electrode for an all-solid-state battery, and more particularly to a negative electrode for an all-solid-state battery including a negative electrode current collector and a coating layer on the negative electrode current collector. The negative electrode current collector includes a first region and a second region surrounding the first region, and the second region includes a plurality of irregularities, an all-solid-state battery including the negative electrode, and a method for manufacturing a negative electrode for an all-solid-state battery.

## Claims

### Claim 1

A negative electrode for an all-solid-state battery, the negative electrode comprising:
a negative electrode current collector; and
a coating layer on the negative electrode current collector,
wherein the negative electrode current collector comprises a first region and a second region surrounding the first region, and
the second region comprises a plurality of irregularities.

### Claim 2 (depends on 1)

The negative electrode of claim 1, wherein an adhesive force between the coating layer and the second region is greater than an adhesive force between the coating layer and the first region.

### Claim 3 (depends on 1)

The negative electrode of claim 1, wherein a surface roughness (Sa) of the first region is less than a surface roughness of the second region.

### Claim 4 (depends on 1)

The negative electrode of claim 1, wherein the plurality of irregularities is formed through a plasma treatment.

### Claim 5 (depends on 1)

The negative electrode of claim 1, wherein a ratio of an area of the second region to an area of the first region is in a range of about 0.5 to about 1.

### Claim 6 (depends on 1)

The negative electrode of claim 1, wherein the coating layer comprises a metal and a carbon-based material.

### Claim 7 (depends on 6)

The negative electrode of claim 6, wherein:
the coating layer further comprises a binder; and
an amount of the binder in the coating layer is in a range of about 1 wt % to about 8 wt % on the basis of 100 wt % of the coating layer.

### Claim 8 (depends on 1)

The negative electrode of claim 1, further comprising a lithium metal layer between the negative electrode current collector and the coating layer.

### Claim 9 (depends on 1)

An all-solid-state battery comprising:
the negative electrode according to claim 1;
a positive electrode; and
a solid electrolyte layer between the negative electrode and the positive electrode.

### Claim 10 (depends on 9)

The all-solid-state battery of claim 9, wherein the solid electrolyte layer comprises a sulfide-based solid electrolyte.

### Claim 11 (depends on 9)

The all-solid-state battery of claim 9, wherein the positive electrode comprises a positive electrode active material and a sulfide-based solid electrolyte.

### Claim 12

A method for manufacturing a negative electrode for an all-solid-state battery, the method comprising:
preparing a negative electrode current collector comprising a first region and a second region surrounding the first region;
performing a plasma treatment selectively on the second region excluding the first region; and
forming a coating layer on the negative electrode current collector;
wherein an adhesive force between the coating layer and the second region is greater than an adhesive force between the coating layer and the first region.

### Claim 13 (depends on 12)

The manufacturing method of claim 12, wherein the performing of the plasma treatment selectively on the second region comprises applying a frequency in a range of about 1 kHz to about 100 kHz to a discharge electrode.

### Claim 14 (depends on 12)

The manufacturing method of claim 12, wherein the performing of the plasma treatment selectively on the second region comprises supplying at least one of oxygen, inert gas, and a combination thereof, at a flow rate in a range of about 10 sccm to about 1000 sccm.

### Claim 15 (depends on 12)

The manufacturing method of claim 12, wherein the plasma treatment is performed for a duration in a range of about 1 second to about 3000 seconds.

### Claim 16 (depends on 12)

The manufacturing method of claim 12, wherein the performing of the plasma treatment selectively on the second region comprises providing a masking member onto the first region to mask the first region.

### Claim 17 (depends on 12)

The manufacturing method of claim 12, wherein the performing of the plasma treatment selectively on the second region comprises forming a plurality of irregularities on the second region.

### Claim 18 (depends on 12)

The manufacturing method of claim 12, wherein a ratio of an area of the second region to an area of the first region is in a range of about 0.5 to about 1.

### Claim 19 (depends on 12)

The manufacturing method of claim 12, wherein the coating layer comprises a metal and a carbon-based material.

### Claim 20 (depends on 12)

The manufacturing method of claim 12, wherein the coating layer further comprises a binder.