# US 2026/0145278 A1 · Sulfur-resistant and corrosion-resistant low-carbon alloy-based coiled tubing and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0145278 A1
- Document ID: US20260145278A1
- Status: Published application
- Kind: A1
- Application number: 19/107,281
- Filed: 2024-11-28
- Published: 2026-05-28
- Earliest claimed: 2024-11-26
- Assignees: Shinda (Tangshan) Creative Oil & Gas Equipment Co., Ltd.
- Applicants: Shinda (Tangshan) Creative Oil & Gas Equipment Co., Ltd.
- Inventors: Jianliang DUAN; Runqiu GAO; Wenbin WU; Jianlei ZHAN; Guogang LIU; Jian DONG; Yueming LIU
- Web page: https://patentgrep.com/patent/US20260145278A1

## CPC

- B23K 31/027: {Making tubes by soldering or welding}
- B23K 10/02: Plasma welding
- B23K 35/0261: {Rods, electrodes or wires}
- B23K 35/3053: {Fe as the principal constituent}
- B23K 37/06: for positioning the molten material, e.g. confining it to a desired area
- C21D 1/84: Controlled slow cooling (cooling-beds for metal rolling B21B43/00)
- C21D 6/004: {containing Cr and Ni}
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 8/10: during manufacturing of tubular bodies
- C21D 9/08: for tubular bodies or pipes
- C21D 9/085: {Cooling or quenching}
- C21D 9/14: wear-resistant or pressure-resistant pipes
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/22: with molybdenum or tungsten
- C22C 38/24: with vanadium
- C22C 38/42: with copper
- C22C 38/44: with molybdenum or tungsten
- C22C 38/46: with vanadium
- C22C 38/48: with niobium or tantalum
- C22C 38/50: with titanium or zirconium
- C22C 38/58: with more than 1.5% by weight of manganese
- B23K 13/025: {for tubes}
- B23K 26/262: of longitudinal seams of tubes
- B23K 2101/06: Tubes
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

Provided are a sulfur-resistant and corrosion-resistant low-carbon alloy-based coiled tubing and a preparation method thereof. The sulfur-resistant and corrosion-resistant low-carbon alloy-based coiled tubing is prepared by subjecting a steel strip to butt welding, curling molding, tube blank welding, extrusion molding, weld heat treatment, and cooling in sequence, and the sulfur-resistant and corrosion-resistant low-carbon alloy-based coiled tubing includes the following components by mass percentage: 0.04% to 0.08% of C, 1.5% to 2.0% of Mn, 0.1% to 0.3% of Si, 0.1% to 0.3% of Cr, 0.05% to 0.3% of Mo, 0.04% to 0.07% of Nb, 0.005% to 0.025% of Ti, 0.01% to 0.05% of Al, not greater than 0.3% of Ni, not greater than 0.3% of Cu, not greater than 0.02% of P, not greater than 0.02% of S, and Fe and unavoidable impurities as a balance.

## Claims

### Claim 1

A sulfur-resistant and corrosion-resistant low-carbon alloy-based coiled tubing, the sulfur-resistant and corrosion-resistant low-carbon alloy-based coiled tubing being prepared by subjecting a steel strip to butt welding, curling molding, tube blank welding, extrusion molding, weld heat treatment, and cooling in sequence, and the sulfur-resistant and corrosion-resistant low-carbon alloy-based coiled tubing comprising the following components by mass percentage:
0.04% to 0.08% of C, 1.5% to 2.0% of Mn, 0.1% to 0.3% of Si, 0.1% to 0.3% of Cr, 0.05% to 0.3% of Mo, 0.04% to 0.07% of Nb, 0.005% to 0.025% of Ti, 0.01% to 0.05% of Al, not greater than 0.3% of Ni, not greater than 0.3% of Cu, not greater than 0.02% of P, not greater than 0.02% of S, and Fe and unavoidable impurities as a balance.

### Claim 2 (depends on 1)

A method for preparing the sulfur-resistant and corrosion-resistant low-carbon alloy-based coiled tubing of claim 1, comprising the following steps:
S1, extending the steel strip by the butt welding, and then subjecting a resulting weld region to rolling and deformation heat treatment;
S2, subjecting a treated steel strip obtained in S1 to the curling molding to obtain a round tube blank with a weld;
S3, welding the round tube blank obtained in S2, and then adding an extrusion roller to a rear side of a resulting molten pool before solidification and conducting the extrusion molding on the weld; and
S4, subjecting an extrusion molded weld obtained in S3 to the weld heat treatment and then air cooling to room temperature to obtain the sulfur-resistant and corrosion-resistant low-carbon alloy-based coiled tubing.

### Claim 3 (depends on 2)

The method of claim 2, wherein in S1, the butt welding is conducted by plasma welding using a copper-plated welding wire of a manganese-molybdenum steel as a welding wire.

### Claim 4 (depends on 2)

The method of claim 2, wherein in S1, the rolling is conducted at a pressure of 4 tonnes to 8 tonnes and is reciprocated once.

### Claim 5 (depends on 2)

The method of claim 2, wherein in S1, the rolling and the deformation heat treatment refer to rolling the weld region while conducting a heat treatment, the rolling is conducted at a pressure of 4 tonnes to 8 tonnes and is reciprocated once, and the rolling and the deformation heat treatment are conducted at a temperature of 600° C. to 750° C., and the rolling and the deformation heat treatment are conducted for 10 seconds each time.

### Claim 6 (depends on 2)

The method of claim 2, wherein in S2, the weld has a gap of 1 mm to 2 mm.

### Claim 7 (depends on 2)

The method of claim 2, wherein in S3, the welding is conducted by laser welding or high-frequency welding.

### Claim 8 (depends on 2)

The method of claim 2, wherein in S4, the weld heat treatment comprises simulated normalizing and tempering, the simulated normalizing is conducted at a temperature of 900° C. to 940° C., and the tempering is conducted at a temperature of 500° C. to 600° C.

### Claim 9 (depends on 8)

The method of claim 8, wherein the simulated normalizing is conducted at 910° C. and the tempering is conducted at 550° C.

### Claim 10 (depends on 8)

The method of claim 8, wherein the simulated normalizing is conducted at 940° C. and the tempering is conducted at 550° C.