# US 2026/0143825 A1 · Solar cell and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0143825 A1
- Document ID: US20260143825A1
- Status: Published application
- Kind: A1
- Application number: 18/705,794
- Filed: 2023-08-24
- Published: 2026-05-21
- Earliest claimed: 2022-10-27
- Assignees: Tongwei Solar (Meishan) Co., Ltd.
- Applicants: Tongwei Solar (Meishan) Co., Ltd.
- Inventors: Wenzhou XU; Guoqiang XING
- Web page: https://patentgrep.com/patent/US20260143825A1

## CPC

- H10F 10/14: Photovoltaic cells having only PN homojunction potential barriers
- H10P 32/16: between a solid phase and a liquid phase
- H10F 71/00: Manufacture or treatment of devices covered by this subclass (patterning processes to connect thin photovoltaic cells in integrated devices, or assemblies of multiple devices, having photovoltaic cells H10F19/33; manufacture or treatment of encapsulations or containers for integrated devices, or assemblies of multiple devices, having photovoltaic cells H10F19/80; manufacture or treatment of integrated devices, or assemblies of multiple devices, comprising at least one element in which radiation controls the flow of current H10F39/00)
- H10F 71/121: {The active layers comprising only Group IV materials}
- H10F 71/128: {Annealing}
- H10F 71/129: {Passivating}
- H10F 77/1223: characterised by the dopants
- H10F 77/211: {for photovoltaic cells}
- H10F 77/30: Coatings (arrangements for preventing damage to photovoltaic cells caused by corpuscular radiation H10F77/80)
- H10F 77/311: {for photovoltaic cells}
- H10F 77/315: {the coatings being antireflective or having enhancing optical properties}
- H10P 32/12: between a solid phase and a gaseous phase
- H10P 32/171: {being group IV material}
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A solar cell includes: an N-type silicon wafer, where a front surface of the N-type silicon wafer is provided with a doped region containing boron, the doped region is divided into a lightly doped region and a heavily doped region, a boron concentration of the lightly doped region is less than a boron concentration of the heavily doped region, a junction depth of the lightly doped region is less than a junction depth of the heavily doped region; a passivation layer and a first anti-reflection layer that are sequentially stacked on the front surface of the N-type silicon wafer. An area of a surface of the first anti-reflection layer corresponding to the heavily doped region is provided with an electrode. The electrode extends through the first anti-reflection layer and the passivation layer, and is in an ohmic contact with the heavily doped region.

## Claims

### Claim 1

A solar cell, comprising:
an N-type silicon wafer, wherein a front surface of the N-type silicon wafer is provided with a doped region containing boron; the doped region is divided into a lightly doped region and a heavily doped region; a boron concentration of the lightly doped region is less than a boron concentration of the heavily doped region; a junction depth of the lightly doped region is less than a junction depth of the heavily doped region; and
a passivation layer and a first anti-reflection layer that are sequentially stacked on the front surface of the N-type silicon wafer; wherein an area of a surface of the first anti-reflection layer corresponding to the heavily doped region is provided with an electrode; the electrode extends through the first anti-reflection layer and the passivation layer, and is in an ohmic contact with the heavily doped region.

### Claim 2 (depends on 1)

The solar cell according to claim 1, wherein the boron concentration of the lightly doped region is in a range from 1018 cm−3 to 1019 cm−3, and the boron concentration of the heavily doped region is in a range from 1019 cm−3 to 1020 cm−3.

### Claim 3 (depends on 1)

The solar cell according to claim 1, wherein the junction depth of the lightly doped region is in a range from 0.4 μm to 0.8 μm; and the junction depth of the heavily doped region is in a range from 1.0 μm to 1.4 μm.

### Claim 4 (depends on 1)

The solar cell according to claim 1, wherein a polysilicon layer and a second anti-reflection layer are sequentially stacked on a back surface of the N-type silicon wafer.

### Claim 5 (depends on 1)

A preparation method of the solar cell according to claim 1, comprising the following steps:
using a gas phase boron source to perform a first boron diffusion on the front surface of the N-type silicon wafer, to form the lightly doped region and a borosilicate glass layer with a thickness of no more than 10 nm on the front surface of the N-type silicon wafer;
coating a boron paste onto a surface of the borosilicate glass layer, and performing a second boron diffusion using the boron paste to form the heavily doped region; and
removing the borosilicate glass layer, forming the passivation layer and the first anti-reflection layer sequentially on the front surface of the N-type silicon wafer, and printing the electrode on the area of the surface of the first anti-reflection layer corresponding to the heavily doped region, and enabling the electrode to extend through the first anti-reflection layer and the passivation layer, and be in an ohmic contact with the heavily doped region.

### Claim 6 (depends on 5)

The preparation method of the solar cell according to claim 5, wherein in the step of the first boron diffusion, a temperature is in range from 850° C. to 1000° C.

### Claim 7 (depends on 5)

The preparation method of the solar cell according to claim 5, wherein in the step of the first boron diffusion, the gas phase boron source is at least one of BCl3, BBr3, and BH3.

### Claim 8 (depends on 5)

The preparation method of the solar cell according to claim 5, wherein in the step of the second boron diffusion, oxygen is introduced at 700° C. to to 800° C. for 30 min to 60 min to remove impurities in the boron paste, and then the oxygen is stopped from being introduced, and a treatment is performed at 900° C. to 1100° C. for 10 min to 60 min under anaerobic condition.

### Claim 9 (depends on 5)

The preparation method of the solar cell according to claim 5, wherein the passivation layer or the first anti-reflection layer is formed using a vapor deposition.

### Claim 10 (depends on 5)

The preparation method of the solar cell according to claim 5, wherein after forming the heavily doped region, the method further comprises the following step:
forming a polysilicon layer and a second anti-reflection layer sequentially on a back surface of the N-type silicon wafer.