# US 2026/0142162 A1 · Method for preparing positive electrode material, positive electrode material, positive electrode plate, battery, and electric apparatus

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0142162 A1
- Document ID: US20260142162A1
- Status: Published application
- Kind: A1
- Application number: 19/452,426
- Filed: 2026-01-19
- Published: 2026-05-21
- Earliest claimed: 2023-12-01
- Assignees: Jiangsu Contemporary Amperex Technology Limited; Jiangsu Lithitech Co., Ltd.
- Applicants: Jiangsu Contemporary Amperex Technology Limited; Jiangsu Lithitech Co., Ltd.
- Inventors: Yongnan Guo; Caijun Wang; Houyong Li; Yinjun Zhu; Jiawei Li; Jiale Lv; Yutao Pan; Jiecheng Cai; Huaiyu Sun; Jicheng Zhang
- Web page: https://patentgrep.com/patent/US20260142162A1

## CPC

- H01M 4/366: {as layered products}
- C01B 25/45: containing plural metal, or metal and ammonium
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/0497: {Chemical precipitation}
- H01M 4/136: Electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/1397: of electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 4/587: for inserting or intercalating light metals
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2004/60: Particles characterised by their size
- C01P 2006/12: Surface area
- C01P 2006/40: Electric properties
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for preparing a positive electrode material, a positive electrode material, a positive electrode plate, a battery, and an electric apparatus are provided. The method for preparing a positive electrode material includes: mixing a precursor lithium manganese iron phosphate, a carbon source, and a source of a doping element in a solvent, drying, and sintering to obtain a positive electrode material. The positive electrode material includes a core and a coating layer coating the core; the core includes LiMnxFe1-xPO4, where 0<x<1; the coating layer includes carbon and a doping element; and the doping element includes one or more of Group IIA elements, Group IIIA elements, Group IVA elements, and transition metal elements. The method reduces the powder resistivity and specific surface area of the positive electrode material, and improves the gram capacity and cycling performance of a battery.

## Claims

### Claim 1

A method for preparing a positive electrode material, comprising:
mixing a precursor lithium manganese iron phosphate, a carbon source, and a source of a doping element in a solvent, drying, and sintering to obtain a positive electrode material; wherein
the positive electrode material comprises a core and a coating layer coating the core; the core comprises LiMnxFe1-xPO4, wherein 0<x<1; the coating layer comprises carbon and a doping element; and the doping element comprises one or more of Group IIA elements, Group IIIA elements, Group IVA elements, and transition metal elements.

### Claim 2 (depends on 1)

The method according to claim 1, wherein
0
.
1
≤
x
≤
0
.
9
;
the doping element comprises one or more elements of Mg, Ti, V, Si, Cr, Mn, Fe, Co, Ni, and B.

### Claim 3 (depends on 1)

The method according to claim 1, wherein a molar ratio of the precursor to a carbon element in the carbon source is 1:1.5 to 1:0.001; and/or
a molar ratio of the precursor to a doping element in the source of the doping element is 1:0.25 to 1:0.00001.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the mixing is performed at 5° C. to 70° C.; and/or
a mixing duration is 0.5 hours to 12 hours; and/or
the mixing is performed by grinding.

### Claim 5 (depends on 1)

The method according to claim 1, wherein a sintering temperature is 350° C. to 950° C.; and/or
a sintering duration is 2 hours to 20 hours; and/or
the sintering is performed in an inert atmosphere.

### Claim 6 (depends on 1)

The method according to claim 1, wherein a drying temperature is 150° C. to 400° C.; and/or
the drying is performed by spray drying or oven drying; and/or
the method further comprises sieving a mixture before the drying and collecting a sieved portion; and/or
the method further comprises crushing after the sintering; and/or
the carbon source comprises one or more of an organic carbon source and an inorganic carbon source; and/or
the source of the doping element comprises one or more of a hydroxide of the doping element, an oxide of the doping element, an acid of the doping element, and a salt of the doping element; and/or
the solvent comprises one or more of water and an organic solvent.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the precursor is prepared by the following:
reacting a lithium source, a manganese source, an iron source, and a phosphorus source in a solvent, performing solid-liquid separation, and collecting a solid-phase material; and
drying and sintering the solid-phase material to obtain the precursor.

### Claim 8 (depends on 7)

The method according to claim 7, wherein the precursor comprises LiMnxFe1-xPO4, wherein 0<x<1.

### Claim 9 (depends on 7)

The method according to claim 7, wherein in the steps of preparing the precursor, a reaction is performed at 5° C. to 60° C.;
a reaction duration is 10 minutes to 8 hours;
a drying temperature is 50° C. to 250° C.;
a drying duration is 10 minutes to 12 hours;
a sintering temperature is 150° C. to 800° C.;
a sintering duration is 1 hour to 12 hours; and/or
the sintering is performed in an inert atmosphere.

### Claim 10 (depends on 7)

The method according to claim 7, wherein in the steps of preparing the precursor, the solid-liquid separation is performed by filtration or centrifugation; and/or
before the drying, the solid-phase material is ball-milled;
before the drying, the solid-phase material is washed;
between the drying and the sintering, the solid-phase material is crushed;
the lithium source comprises one or more of a hydroxide, oxide, inorganic acid salt, and organic acid salt of a lithium element;
the manganese source comprises one or more of an organic acid salt, inorganic acid salt, oxide, and hydroxide of a manganese element;
the iron source comprises one or more of an organic acid salt, inorganic acid salt, oxide, and hydroxide of an iron element;
the phosphorus source comprises one or more of phosphoric acid, phosphate, hydrogen phosphate, and dihydrogen phosphate; and/or
a carbon source is added during a reaction process.

### Claim 11

A positive electrode material, comprising a core and a coating layer coating the core, wherein the core comprises LiMnxFe1-xPO4, wherein 0<x<1.

### Claim 12 (depends on 11)

The positive electrode material according to claim 11, wherein a molar ratio of LiMnxFe1-xPO4 in the core to a carbon element in the coating layer is 1:1.5 to 1:0.001; and/or
a molar ratio of LiMnxFe1-xPO4 in the core to a doping element in the coating layer is 1:0.25 to 1:0.00001.

### Claim 13 (depends on 1, 11)

The positive electrode material according to claim 11, wherein a particle size Dv50 of the positive electrode material is 0.1 μm to 13 μm; and/or
a BET specific surface area of the positive electrode material is 10 m2/g to 27 m2/g; and/or
a powder resistivity of the positive electrode material is less than or equal to 1200 Ω·cm; and/or
the positive electrode material is prepared by the method claim 1.

### Claim 14 (depends on 1, 11)

A positive electrode plate, comprising a positive electrode material prepared by the method according to claim 1 or the positive electrode material according to claim 11.

### Claim 15 (depends on 1, 11, 14)

A battery, comprising a positive electrode material prepared by the method according to claim 1, the positive electrode material according to claim 11, or the positive electrode plate according to claim 14.

### Claim 16 (depends on 15)

An electric apparatus, comprising the battery according to claim 15.