# US 2026/0139401 A1 · Preparation method for aluminum electrolysis metal anode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0139401 A1
- Document ID: US20260139401A1
- Status: Published application
- Kind: A1
- Application number: 19/452,283
- Filed: 2026-01-17
- Published: 2026-05-21
- Earliest claimed: 2023-07-17
- Assignees: Shandong Hongqiao New Material Co., Ltd.; Central South University
- Applicants: Shandong Hongqiao New Material Co., Ltd.; Central South University
- Inventors: Bo ZHANG; Congsen YANG; Quanlin LI; Qingshen XIE; Huiwen XIONG; Yong HE; Kechao ZHOU; Lei ZHANG
- Web page: https://patentgrep.com/patent/US20260139401A1

## CPC

- B22F 1/108: {Mixtures obtained by warm mixing}
- C25C 7/02: Electrodes (consumable anodes for the refining the metals C25C1/00 - C25C5/00); Connections thereof
- B22F 1/05: Metallic powder characterised by the size or surface area of the particles
- B22F 1/103: containing an organic binding agent comprising a mixture of, or obtained by reaction of, two or more components other than a solvent or a lubricating agent
- B22F 3/10: Sintering only
- B22F 7/06: of composite workpieces or articles from parts, e.g. to form tipped tools {(B22F7/002 takes precedence)}
- B22F 9/04: starting from solid material, e.g. by crushing, grinding or milling ({C22C1/1084 takes precedence}; crushing, grinding or milling, in general, see the relevant subclasses, e.g. B02C)
- C25C 3/12: Anodes
- B22F 2009/043: {by ball milling}
- B22F 2301/35: Iron
- B22F 2304/054: Particle size between 1 and 100 nm
- B22F 2304/056: Particle size above 100 nm up to 300 nm
- B22F 2304/058: Particle size above 300 nm up to 1 micrometer
- C25C 1/02: of light metals
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C25C: PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY OR REFINING OF METALS; APPARATUS THEREFOR

## Abstract

Provided is a preparation method for aluminum electrolysis metal anode, including mixing metal shell powder with a thermoplastic binder to obtain a semisolid hot mixture; crushing the semisolid hot mixture to obtain metal shell feedstock granules; preheating a mold; filling preheated metal shell feedstock granules into the mold; applying pressure and heating a temperature 5-50° C. higher than a softening point temperature of the thermoplastic binder, and performing rheological pressing to obtain a metal shell green body; filling alloy inner core powder into a core part of the metal shell green body to obtain an inert anode green body with an alloy inner core; and sintering the inert anode green body with the alloy inner core to obtain an inert anode for aluminum electrolysis. It achieves near-net-shape forming of a metal anode shell with a special-shaped structure through a rheological pressing manner. By adopting a two-step sintering manner, densification of an aluminum electrolysis metal anode shell and electric connection is simultaneously completed. The process is simple in operation and short in process and the obtained anode has high strength and high precision.

## Claims

### Claim 1

An integrated preparation method for aluminum electrolysis metal anode shell and electric connection, comprising:
mixing a metal shell powder with a thermoplastic binder to obtain a semisolid hot mixture;
crushing the semisolid hot mixture to obtain metal shell feedstock granules;
preheating a mold to a temperature 20-50° C. higher than a softening point temperature of the thermoplastic binder, filling preheated metal shell feedstock granules into the mold, applying pressure and heating to a temperature 5-50° C. higher than the softening point temperature of the thermoplastic binder, and performing a rheological pressing to obtain a metal shell green body;
filling an alloy inner core powder into a core part of the metal shell green body to obtain an inert anode green body with an alloy inner core; and
sintering the inert anode green body with the alloy inner core to obtain an integrated inert anode for aluminum electrolysis metal anode shell and electric connection; wherein
the metal shell powder, in mass percentage, has a composition as follows: 10-60% of Ni, 5-30% of M, and a balance of Fe, wherein M is selected from at least one of Cu, Co, Cr, Mn, Al, Ag, Zn, Ti, Sn, W, Mo, Zr, or Nb;
a particle size of the metal shell feedstock granules is within a range of −10 mesh to +200 mesh;
the metal shell feedstock granules are preheated to 60-80° C., and the mold is preheated to 60-100° C.;
a pressure of 20-60 MPa is applied along a shell pressing direction, and a temperature is increased to 120-170° C., and the rheological pressing is performed for 10-40 min to obtain the metal shell green body; and
the sintering is performed in a protective atmosphere, and a process of the sintering includes: first increasing a temperature to 400-600° C., holding for 8-12 h, then further increasing the temperature to K1, then decreasing the temperature to K2, holding for 4-6 h, and cooling to a room temperature; wherein K 1-K2≥50° C., K1 is 1300-1400° C., and K2 is 1150-1350° C.

### Claim 2 (depends on 1)

The integrated preparation method for aluminum electrolysis metal anode shell and electric connection according to claim 1, wherein
a particle size of the metal shell powder is within a range of 0.05-1 μm;
the metal shell powder is obtained by pulverizing and classifying a metal powder, wherein the pulverizing is performed by nano grinding using a turbine nano sand mill, and working parameters for the nano grinding include a rotational speed of 580-1500 rpm and a flow rate of 50-500 L/H; and
the classifying is performed using a jet air classifier, and working parameters for the classifying include a feed rate of 50-100 kg/h, a working pressure of 1.5-20 MPa, and an air pressure of a cyclone collector of 1.5-20 kPa.

### Claim 3 (depends on 1)

The integrated preparation method for aluminum electrolysis metal anode shell and electric connection according to claim 1, wherein a volume fraction of the metal shell powder in the semisolid hot mixture is 60%-80%.

### Claim 4 (depends on 1)

The integrated preparation method for aluminum electrolysis metal anode shell and electric connection according to claim 1, wherein the thermoplastic binder, in volume percentage, has a composition as follows: 70-85 vol % of a filler binder, 10-20 vol % of a backbone binder, 2˜5 vol % of a surfactant, and 0.5-2 vol % of a plasticizer; and
the filler binder has a melt index greater than or equal to 80 g/min, and the backbone binder has a melt index greater than or equal to 35 g/min.

### Claim 5 (depends on 4)

The integrated preparation method for aluminum electrolysis metal anode shell and electric connection according to claim 4, wherein
the filler binder is selected from at least one of paraffin wax, carnauba wax, microcrystalline wax, polyethylene wax, polyethylene glycol, polyoxymethylene, ethylene-vinyl acetate copolymer, ethylene-ethyl acrylate, or methyl cellulose;
the backbone binder is selected from at least one of polypropylene, high-density polyethylene, low-density polyethylene, polystyrene, or polymethyl methacrylate;
the surfactant is selected from at least one of stearic acid, zinc stearate, glycerol, castor oil, or peanut oil; and
the plasticizer is selected from at least one of dibutyl phthalate, dioctyl phthalate, isodecyl β-(3,5-di-tert-butyl-4-hydroxyphenyl)propionate, pentaerythritol tetrakis(β-(3,5-di-tert-butyl-4-hydroxyphenyl)propionate), 4,4′-methylenebis(2,6-di-tert-butylphenol), or n-octadecyl 3-(3,5-di-tert-butyl-4-hydroxyphenyl)propionate.

### Claim 6 (depends on 5)

The integrated preparation method for aluminum electrolysis metal anode shell and electric connection according to claim 5, wherein the filler binder is selected from at least one of carnauba wax, polyoxymethylene, or polyethylene glycol.

### Claim 7 (depends on 6)

The integrated preparation method for aluminum electrolysis metal anode shell and electric connection according to claim 6, wherein the filler binder is polyoxymethylene.

### Claim 8 (depends on 1)

The integrated preparation method for aluminum electrolysis metal anode shell and electric connection according to claim 1, wherein
the mixing is performed at a temperature of 120-200° C. for 30-60min; and
the crushing is performed at a heating temperature of 60-150° C. and a screw rotational speed of 400-600 r/min.

### Claim 9 (depends on 1)

The integrated preparation method for aluminum electrolysis metal anode shell and electric connection according to claim 1, wherein the mold is a modular heatable mold, and the mold includes a modular female die A, a modular female die B, an upper punch, a lower punch, a core rod, and a heating jacket.

### Claim 10 (depends on 1)

The integrated preparation method for aluminum electrolysis metal anode shell and electric connection according to claim 1, wherein the protective atmosphere is argon gas; and
a process of the cooling includes: first decreasing the temperature to 400-500° C. at a cooling rate of less than 5° C./min, and then performing furnace cooling to the room temperature.