# US 2026/0138925 A1 · Lead-zinc tailings-based ceramsite

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0138925 A1
- Document ID: US20260138925A1
- Status: Published application
- Kind: A1
- Application number: 19/390,419
- Filed: 2025-11-14
- Published: 2026-05-21
- Earliest claimed: 2024-11-18
- Assignees: Henan Building Materials Research and Design Institute Co., Ltd.
- Applicants: Henan Building Materials Research and Design Institute Co., Ltd
- Inventors: Maoliang Zhang; Xindi Wan; Yan Ma; Jianwei Li; Jinhua Wang; Lu Zhang; Huanhuan Zhang; Huiling Yin
- Web page: https://patentgrep.com/patent/US20260138925A1

## CPC

- C04B 33/1327: {containing heavy metals}
- C04B 33/138: from metallurgical processes, e.g. slag, furnace dust, galvanic waste
- C04B 33/1321: {Waste slurries, e.g. harbour sludge, industrial muds}
- C04B 33/32: Burning methods
- C04B 2235/3463: Alumino-silicates other than clay, e.g. mullite
- C04B 2235/36: Glass starting materials for making ceramics, e.g. silica glass
- C04B 2235/5409: expressed by specific surface values
- C04B 2235/5454: nanometer sized, i.e. below 100 nm
- C04B 2235/6562: Heating rate
- C04B 2235/6565: Cooling rate
- C04B 2235/661: Multi-step sintering
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

A lead-zinc tailings-based ceramsite includes the following raw materials in parts by mass: 100 parts of lead-zinc tailings; 20-30 parts of limestone tailings; 6-8 parts of activated mullite nanopowder, 1-3 parts of glass powder, and 8-12 parts of dried sludge powder. A preparation method for the lead-zinc tailings-based ceramsite is further provided.

## Claims

### Claim 1

A lead-zinc tailings-based ceramsite, comprising the following raw materials in parts by mass:
100 parts of lead-zinc tailings;
20-30 parts of limestone tailings;
6-8 parts of activated mullite nanopowder;
1-3 parts of glass powder; and
8-12 parts of dried sludge powder;
wherein the activated mullite nanopowder is produced by uniformly dispersing mullite particles in a mixed solution of sodium silicate and potassium silicate, followed by heating and grinding, with a target temperature of 300-600° C.; and
the lead-zinc tailings-based ceramsite is prepared according to following preparation method:
(1) uniformly mixing the raw materials comprising the lead-zinc tailings, the limestone tailings, the activated mullite nanopowder, the glass powder, and the dried sludge powder in parts by mass, and adding water to prepare a ceramsite green body;
(2) heating the ceramsite green body to temperature of 900-980° C. and maintaining the temperature for 5-8 min; and heating the ceramsite green body to temperature of 1200-1300° C. and maintaining the temperature for 8-10 min; and
(3) cooling the ceramsite green body to temperature of 1150-1100° C. and maintaining the temperature for 5-10 min; cooling the ceramsite green body to temperature of 1080-1000° C. and maintaining the temperature for 5-10 min; cooling the ceramsite green body to temperature of 950-900° C. and maintaining the temperature for 5-10 min; and slowly cooling the ceramsite green body to standard ambient temperature to obtain the lead-zinc tailings-based ceramsite.

### Claim 2 (depends on 1)

The lead-zinc tailings-based ceramsite according to claim 1, wherein a mass ratio of the mullite particles to the sodium silicate and the potassium silicate is 1:(1-2):(3-5);
the mullite particles have a particle size of 50-100 nm; the mixed solution of sodium silicate and potassium silicate has a concentration of 5-15 wt %; and both sodium silicate and potassium silicate have a modulus not exceeding 2; and
the activated mullite nanopowder has a particle size of 200-400 nm.

### Claim 3 (depends on 1)

The lead-zinc tailings-based ceramsite according to claim 1, wherein a specific surface area of the lead-zinc tailings is 800-1000 m2/kg.

### Claim 4 (depends on 1)

The lead-zinc tailings-based ceramsite according to claim 1, wherein a specific surface area of the limestone tailings is not less than 200 m2/kg.

### Claim 5 (depends on 1)

The lead-zinc tailings-based ceramsite according to claim 1, wherein a specific surface area of the glass powder is not less than 300 m2/kg.

### Claim 6 (depends on 1)

The lead-zinc tailings-based ceramsite according to claim 1, wherein a specific surface area of the dried sludge powder is not less than 200 m2/kg.

### Claim 7 (depends on 1)

The lead-zinc tailings-based ceramsite according to claim 1, wherein the activated mullite nanopowder is prepared according to following preparation method: uniformly dispersing the mullite particles in the mixed solution of sodium silicate and potassium silicate; heating and drying the mixture until dried mixture reaches a constant mass; and grinding the dried mixture under completely dry conditions to a particle size of 200-400 nm to obtain the activated mullite nanopowder.

### Claim 8 (depends on 1)

The lead-zinc tailings-based ceramsite according to claim 1, wherein during slowly cooling the ceramsite green body to standard ambient temperature in step (3), a cooling rate is not exceed 10° C./min.