# US 2026/0138182 A1 · Method to increase the surface area of lithium metal

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0138182 A1
- Document ID: US20260138182A1
- Status: Published application
- Kind: A1
- Application number: 18/953,350
- Filed: 2024-11-20
- Published: 2026-05-21
- Earliest claimed: 2024-11-20
- Assignees: Enpower Greentech, Inc.
- Applicants: Enpower Greentech, Inc.
- Inventors: Yang Wang; Brendan T. Skelly; Zhendong Hu; Yong Che
- Web page: https://patentgrep.com/patent/US20260138182A1

## CPC

- B22F 9/06: starting from liquid material
- B22F 1/05: Metallic powder characterised by the size or surface area of the particles
- C22C 1/0408: {Light metal alloys}
- C22C 1/0483: {Alloys based on the low melting point metals Zn, Pb, Sn, Cd, In or Ga}
- H01M 4/382: {Lithium (H01M4/405 takes precedence)}
- H01M 4/628: {Inhibitors, e.g. gassing inhibitors, corrosion inhibitors}
- B22F 2201/11: Argon
- B22F 2301/054: Alkali metals, i.e. Li, Na, K, Rb, Cs, Fr
- B22F 2304/10: Micron size particles, i.e. above 1 micrometer up to 500 micrometer
- B22F 2304/15: Millimeter size particles, i.e. above 500 micrometer
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY

## Abstract

Disclosed is a method to increase the surface area of lithium metal. The method includes at least four steps. The first step is melting bulk lithium metal. The second step is adding a particle stabilizing agent to the molten lithium. Alternatively, the particle stabilizing agent can be heated to a temperature above the melting point of the lithium metal and then the bulk lithium material is added to the heated particle stabilizing agent. The third step is agitating the mixture until the lithium particles that form are the desired size. The final step involves cooling the lithium particles to form stabilized lithium particles thereby increasing the surface area of the lithium metal.

## Claims

### Claim 1

A method to increase the surface area of lithium metal comprising the steps of:
a. melting bulk lithium metal at a temperature above the melting point of the lithium metal to form molten lithium metal;
b. mixing the molten lithium metal with one or more particle stabilizing agents;
c. agitating the mixture of molten lithium and one or more particle stabilizing agents to form a plurality of lithium metal particles;
d. cooling the lithium metal particles.

### Claim 2 (depends on 1)

The method to increase the surface area of lithium metal according to claim 1, wherein the steps of the method are conducted under standard temperature and atmospheric pressure in a dry room, in a glove box filled with an inert gas, in a vacuum chamber, or in a combination thereof.

### Claim 3 (depends on 1)

The method to increase the surface area of lithium metal according to claim 1, wherein the viscosity of the one or more particle stabilizing agents is between 1 and 100,000 mPa·s at a temperature of 25° C.

### Claim 4 (depends on 1)

The method to increase the surface area of lithium metal according to claim 1, wherein the volume ratio of the one or more particle stabilizing agents to the molten lithium each ranges from 0.001 to 1.0 to 10000 to 1.0.

### Claim 5 (depends on 1)

The method to increase the surface area of lithium metal according to claim 1, wherein the one or more particle stabilizing agents is selected from the group consisting of a polyester polymer, a polyurethane polymer, a styrene-maleic anhydride copolymer, a modified siloxane, a siloxane polymer, a mineral oil, and combinations thereof.

### Claim 6 (depends on 2)

The method to increase the surface area of lithium metal according to claim 2, wherein the one or more particle stabilizing agents are dissolved in a solvent that has a boiling point above the melting point temperature of the lithium metal.

### Claim 7 (depends on 1)

The method to increase the surface area of lithium metal according to claim 1, wherein the agitation of the mixture of lithium metal and the one or more particle stabilizing agents is conducted manually, magnetically, or mechanically.

### Claim 8 (depends on 1)

The method to increase the surface area of lithium metal according to claim 1, wherein the size of the lithium particles after step d. ranges from 20 microns (μm) to 20 mm.