# US 2026/0132543 A1 · Method for growing single crystal, method for producing semiconductor substrate, and semiconductor substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0132543 A1
- Document ID: US20260132543A1
- Status: Published application
- Kind: A1
- Application number: 19/115,498
- Filed: 2023-08-07
- Published: 2026-05-14
- Earliest claimed: 2022-09-29
- Assignees: Novel Crystal Technology, Inc.
- Applicants: Novel Crystal Technology, Inc.
- Inventors: Yuki UEDA; Takuya IGARASHI; Kimiyoshi KOSHI
- Web page: https://patentgrep.com/patent/US20260132543A1

## CPC

- C30B 29/16: Oxides
- C01G 15/00: Compounds of gallium, indium or thallium
- C30B 11/00: Single-crystal growth by normal freezing or freezing under temperature gradient, e.g. Bridgman-Stockbarger method (C30B13/00, C30B15/00, C30B17/00, C30B19/00 take precedence; under a protective fluid C30B27/00)
- C30B 11/006: {Controlling or regulating}
- C30B 11/02: without using solvents (C30B11/06 takes precedence)
- H10D 62/875: {being semiconductor metal oxide, e.g. InGaZnO (Group II-VI materials H10D62/86; Group I-VI materials H10D62/871; Pb compounds or alloys H10D62/874)}
- C01P 2002/52: containing elements as dopants
- C01P 2004/02: obtained by optical microscopy
- C01P 2006/40: Electric properties
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

A single crystal growth method for growing a single crystal of a gallium oxide-based semiconductor, the method including growing the single crystal from a melt of a raw material of the single crystal in an oxidizing atmosphere. Density and average length of voids in the single crystal are controlled by a relative value of an Si concentration and an Sn concentration in the single crystal.

## Claims

### Claim 1

A single crystal growth method for growing a single crystal of a gallium oxide-based semiconductor, the method comprising:
growing the single crystal from a melt of a raw material of the single crystal in an oxidizing atmosphere,
wherein density and average length of voids in the single crystal are controlled by a relative value of an Si concentration and an Sn concentration in the single crystal.

### Claim 2 (depends on 1)

The single crystal growth method according to claim 1, wherein the density and average length of the voids are controlled respectively within ranges of 56 to 57000 cm−2 and 14 to 85 μm by adjusting a value obtained by subtracting the Sn concentration from the Si concentration within a range of −2.8×1018 to 3.0×1018 cm−3.

### Claim 3 (depends on 1)

The single crystal growth method according to claim 1, wherein the density and average length of the voids are controlled respectively within ranges of 56 to 57000 cm−2 and 14 to 85 μm by adjusting the Si concentration to less than 4.0×1018 cm−3 and a value obtained by subtracting the Sn concentration from the Si concentration within a range of −2.8×1018 to 3.0×1018 cm−3.

### Claim 4

A semiconductor substrate producing method for producing a semiconductor substrate comprising a single crystal of a gallium oxide-based semiconductor, the method comprising:
growing the single crystal from a melt of a raw material of the single crystal in an oxidizing atmosphere; and
cutting the semiconductor substrate out of the single crystal,
wherein density and average length of voids in the single crystal are controlled by a relative value of an Si concentration and an Sn concentration in the single crystal.

### Claim 5 (depends on 4)

The semiconductor substrate producing method according to claim 4, wherein the average length of the voids is controlled according to thickness and plane orientation of the semiconductor substrate to suppress that the voids penetrate through between two main surfaces of the semiconductor substrate.

### Claim 6 (depends on 4)

The semiconductor substrate producing method according to claim 4, wherein the density and average length of the voids are controlled respectively within ranges of 56 to 57000 cm−2 and 14 to 85 μm by adjusting a value obtained by subtracting the Sn concentration from the Si concentration within a range of −2.8×1018 to 3.0×1018 cm−3.

### Claim 7 (depends on 4)

The semiconductor substrate producing method according to claim 4, wherein the density and average length of the voids are controlled respectively within ranges of 56 to 57000 cm−2 and 14 to 85 μm by adjusting the Si concentration to less than 4.0×1018 cm−3 and a value obtained by subtracting the Sn concentration from the Si concentration within a range of −2.8×1018 to 3.0×1018 cm−3.

### Claim 8

A semiconductor substrate, comprising:
a single crystal of a gallium oxide-based semiconductor,
wherein the semiconductor substrate comprises voids with density and average length respectively within ranges of 56 to 57000 cm−2 and 14 to 85 μm.

### Claim 9 (depends on 8)

The semiconductor substrate according to claim 8, wherein a value obtained by subtracting an Sn concentration from an Si concentration is in a range of −2.8×1018 to 3.0×1018 cm−3.

### Claim 10 (depends on 8)

The semiconductor substrate according to claim 8, wherein an Si concentration is less than 4.0×1018 cm−3 and a ratio of an Si concentration to an Sn concentration is in a range of 2×1017/3×1018 to 3×1018/2×1016.

### Claim 11 (depends on 8)

The semiconductor substrate according to claim 8, wherein the voids do not penetrate through between two main surfaces.

### Claim 12 (depends on 9)

The semiconductor substrate according to claim 9, wherein the voids do not penetrate through between two main surfaces.

### Claim 13 (depends on 10)

The semiconductor substrate according to claim 10, wherein the voids do not penetrate through between two main surfaces.

### Claim 14 (depends on 8)

The semiconductor substrate according to claim 8, wherein an Si concentration is higher than 2×1017 cm−3 and an Sn concentration is higher than 2×1016 cm−3.

### Claim 15 (depends on 9)

The semiconductor substrate according to claim 9, wherein an Si concentration is higher than 2×1017 cm−3 and an Sn concentration is higher than 2×1016 cm−3.

### Claim 16 (depends on 10)

The semiconductor substrate according to claim 10, wherein an Si concentration is higher than 2×1017 cm−3 and an Sn concentration is higher than 2×1016 cm−3.

### Claim 17 (depends on 5)

The semiconductor substrate producing method according to claim 5, wherein the density and average length of the voids are controlled respectively within ranges of 56 to 57000 cm−2 and 14 to 85 μm by adjusting a value obtained by subtracting the Sn concentration from the Si concentration within a range of −2.8×1018 to 3.0×1018 cm−3.

### Claim 18 (depends on 5)

The semiconductor substrate producing method according to claim 5, wherein the density and average length of the voids are controlled respectively within ranges of 56 to 57000 cm−2 and 14 to 85 μm by adjusting the Si concentration to less than 4.0×1018 cm−3 and a value obtained by subtracting the Sn concentration from the Si concentration within a range of −2.8×1018 to 3.0×1018 cm−3.