# US 2026/0132535 A1 · Superamphiphobic coating with durable wear resistance and corrosion resistance for aluminum alloy surface and preparation method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0132535 A1
- Document ID: US20260132535A1
- Status: Published application
- Kind: A1
- Application number: 19/378,807
- Filed: 2025-11-04
- Published: 2026-05-14
- Earliest claimed: 2024-11-13
- Assignees: China Academy of Machinery Wuhan Research Institute of Materials Protection Co. Ltd.
- Applicants: China Academy of Machinery Wuhan Research Institute of Materials Protection Co., Ltd.
- Inventors: Dan Jia; Ao Chen; Yijie Jin; Haitao Duan; Shengpeng Zhan; Tian Yang; Yu Cheng; Xiaoshuang Luo; Jinming Ma
- Web page: https://patentgrep.com/patent/US20260132535A1

## CPC

- C25D 13/02: with inorganic material
- C09D 5/1681: {Antifouling coatings characterised by surface structure, e.g. for roughness effect giving superhydrophobic coatings or Lotus effect}
- C09D 5/448: {characterised by the additives used (C09D5/4403 - C09D5/4476, C09D5/4492 take precedence)}
- C09D 7/61: inorganic
- C09D 7/62: modified by treatment with other compounds
- C25D 13/06: with polymers {(not used, see C09D5/44)}
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

A superamphiphobic coating with durable wear resistance and corrosion resistance for an aluminum alloy surface and a preparation method therefor are provided. A superamphiphobic paint includes, in parts by weight: 10-15 parts of modified SiO2 particles, 10-15 parts of modified TiO2 particles, 5-10 parts of PTFE, and epoxy resin matrix. The preparation method for the superamphiphobic coating includes: pre-mixing raw materials, uniformly depositing components in a pre-mixed solution on the aluminum alloy surface by electrophoresis, followed by baking to obtain the superamphiphobic coating. A superamphiphobic paint is pollution-free during production and use, and the superamphiphobic coating has high cross-linking density, low curing shrinkage rate, high wear resistance, high hardness, superhydrophobicity, and oleophobiccity. Meanwhile, by pre-treating the aluminum alloy surface, a stable and dense coating is formed to isolate oxygen, thereby improving corrosion resistance of a coated surface and providing sustainable and long-term protection for the coated surface.

## Claims

### Claim 1

A superamphiphobic coating with durable wear resistance and corrosion resistance for an aluminum alloy surface, made from the following raw materials in parts by weight: 10 parts of modified silicon dioxide (SiO2) particles, 15 parts of modified titanium dioxide (TiO2) particles, 10 parts of polytetrafluoroethylene (PTFE), and 75 parts of epoxy resin matrix as a carrier;
wherein an average particle size of the modified SiO2 particles is in a range of 20 nanometers (nm) to 22 nm; and an average particle size of the modified TiO2 particles is in a range of 25 nm to 28 nm;
wherein an average particle size of PTFE powder is in a range of 200 nm to 220 nm;
wherein a preparation method for the superamphiphobic coating for the aluminum alloy surface comprises the following steps:
S1) mixing SiO2 nanoparticles and TiO2 nanoparticles with a modifier individually, followed by stirring or ultrasonically dispersing to make the modifier evenly coated on surfaces of the SiO2 nanoparticles and the TiO2 nanoparticles individually to thereby obtain a SiO2 nanoparticle-modifier mixture and a TiO2 nanoparticle-modifier mixture, and washing the SiO2 nanoparticle-modifier mixture and the TiO2 nanoparticle-modifier mixture to remove unreacted residues to thereby obtain charged SiO2 nanoparticles and charged TiO2 nanoparticles, namely the modified SiO2 particles and the modified TiO2 particles;
S2) mixing the modified SiO2 particles in a nano-sized form, the modified TiO2 particles in the nano-sized form, and the PTFE powder with the epoxy resin matrix to form a pre-mixed solution;
S3) treating the pre-mixed solution by ultrasonic dispersion to ensure that the modified SiO2 particles in the nano-sized form, the modified TiO2 particles in the nano-sized form, and the PTFE powder are evenly dispersed in the epoxy resin matrix to form a stable suspension system;
S4) uniformly depositing components in the pre-mixed solution on the aluminum alloy surface by electrophoresis: putting an aluminum alloy material performed with pre-treatment into an electrophoresis tank, adjusting appropriate electric field parameters, and uniformly depositing the charged SiO2 nanoparticles and the charged TiO2 nanoparticles in the pre-mixed solution on the aluminum alloy surface to form a uniform coating, to thereby obtain a coated-aluminum alloy material;
S5) removing the coated-aluminum alloy material from the electrophoresis tank, and rinsing the coated-aluminum alloy material with deionized water to remove excess sediment, to thereby obtain a prepared aluminum alloy plate; and
S6) baking the prepared aluminum alloy plate at 80 degrees Celsius (° C.) to 120° C. to cure the uniform coating, to thereby obtain the superamphiphobic coating; and
wherein in the step S1), the modifier is an amino silane coupling agent or a positively charged polymer.

### Claim 2 (depends on 1)

The superamphiphobic coating for the aluminum alloy surface as claimed in claim 1, wherein the amino silane coupling agent is one or more selected from the group consisting of 3-aminopropyltriethoxysilane, 3-aminopropyltrimethoxysilane, and N-(2-aminoethyl)-3-aminopropyltrimethoxysilane; and the positively charged polymer is one or more selected from the group consisting of polyethyleneimine, polydimethyldiallylammonium chloride, and chitosan.

### Claim 3 (depends on 2)

The superamphiphobic coating for the aluminum alloy surface as claimed in claim 2, wherein in the step S2), the ultrasonic dispersion is performed for 30 minutes (min) to 35 min under a power in a range of 200 watts (W) to 220 W to ensure that the modified SiO2 particles in the nano-sized form and the modified TiO2 particles in the nano-sized form in the pre-mixed solution are uniformly dispersed.

### Claim 4 (depends on 3)

The superamphiphobic coating for the aluminum alloy surface as claimed in claim 3, wherein in the step S3), the pre-treatment for the aluminum alloy material comprises surface cleaning and micro roughness treatment to increase an adhesion strength between the superamphiphobic coating and the aluminum alloy surface; a conductivity of the pre-mixed solution in the electrophoresis tank is in a range of 100 micro siemens per centimeter (μS/cm) to 110 μS/cm, an electrophoresis voltage is in a range of 50 volts (V) to 55 V, and an electrophoresis duration is in a range of 10 min to 12 min.

### Claim 5 (depends on 4)

The superamphiphobic coating for the aluminum alloy surface as claimed in claim 4, wherein in the step S5), a temperature during baking the prepared aluminum alloy plate is increased gradually to avoid aggregation of the modified SiO2 particles in the nano-sized form and the modified TiO2 particles in the nano-sized form in the pre-mixed solution due to rapid heating, thereby ensuring uniformity and performance stability of the superamphiphobic coating.