# US 2026/0128294 A1 · Lithium titanium composite oxide comprising aluminum-coated primary particles and manufacturing method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0128294 A1
- Document ID: US20260128294A1
- Status: Published application
- Kind: A1
- Application number: 19/426,816
- Filed: 2025-12-19
- Published: 2026-05-07
- Earliest claimed: 2018-03-12
- Assignees: Posco Chemical Co., Ltd
- Applicants: Posco Chemical Co., Ltd
- Inventors: Su Bong CHOI; Chun Gu KANG; Jeong Han KIM; Jae An LEE
- Web page: https://patentgrep.com/patent/US20260128294A1

## CPC

- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- C01G 23/005: {Alkali titanates}
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/366: {as layered products}
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 4/628: {Inhibitors, e.g. gassing inhibitors, corrosion inhibitors}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2002/54: one element only
- C01P 2004/03: obtained by SEM
- C01P 2004/50: Agglomerated particles
- C01P 2004/51: Particles with a specific particle size distribution
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2004/62: Submicrometer sized, i.e. from 0.1-1 micrometer
- C01P 2004/80: Particles consisting of a mixture of two or more inorganic phases
- C01P 2004/84: one phase coated with the other
- C01P 2006/11: Powder tap density
- C01P 2006/12: Surface area
- C01P 2006/40: Electric properties
- C01P 2006/80: Compositional purity
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A lithium titanium composite oxide including aluminum-coated primary particles and a method for manufacturing the same are disclosed. A lithium titanium composite oxide including aluminum-coated primary particles according to an embodiment is manufactured by coating lithium titanium oxide primary particles with aluminum by mixing an aluminum compound with re-pulverized particles and then by spray-drying the mixture again to prepare secondary particles. A battery including the lithium titanium composite oxide including the aluminum-coated primary particles exhibits effects of suppressing electrolyte decomposition and gas generation that may be respectively caused by titanium ions and residual lithium in conventional lithium titanium composite oxides.

## Claims

### Claim 1

A method for manufacturing a lithium titanium composite oxide including aluminum-coated primary particles, the method comprising:
i) mixing, in a solid state, a lithium-containing compound, a titanium oxide, and a dissimilar metal compound in a stoichiometric ratio;
ii) manufacturing a slurry by dispersing the solid mixture of i) in a solvent and performing wet pulverizing until particles having an average particle diameter in a range from 0.1 μm to 0.2 μm are formed;
iii) spray-drying the slurry to form particles;
iv) plasticizing the spray-dried particles;
v) pulverizing the plasticized particles;
vi) manufacturing a slurry by dispersing a mixture of the pulverized particles and an aluminum compound in a solvent and pulverizing the dispersed mixture;
vii) performing spray-drying; and
viii) performing heat treatment.

### Claim 2 (depends on 1)

The method for manufacturing a lithium titanium composite oxide including aluminum-coated primary particles of claim 1, wherein the dissimilar metal compound is a zirconium compound.

### Claim 3 (depends on 1)

The method for manufacturing a lithium titanium composite oxide including aluminum-coated primary particles of claim 1, wherein the aluminum compound is an aluminum sulfate.

### Claim 4 (depends on 1)

The method for manufacturing a lithium titanium composite oxide including aluminum-coated primary particles of claim 1, wherein in plasticizing the spray-dried particles, heat treatment is performed for 10 to 20 hours at a temperature in a range from 700 to 800° C.

### Claim 5 (depends on 1)

The method for manufacturing a lithium titanium composite oxide including aluminum-coated primary particles of claim 1, wherein in performing heat treatment, heat treatment is performed for 10 to 20 hours at a temperature in a range from 400 to 500° C.