# US 2026/0128190 A1 · Rectangular wire and production method for same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0128190 A1
- Document ID: US20260128190A1
- Status: Published application
- Kind: A1
- Application number: 19/354,437
- Filed: 2025-10-09
- Published: 2026-05-07
- Earliest claimed: 2023-04-12
- Assignees: AGC Inc.
- Applicants: AGC Inc.
- Inventors: Masatoshi ABE; Toru SASAKI; Tsuyoshi KAWAI
- Web page: https://patentgrep.com/patent/US20260128190A1

## CPC

- H01B 3/307: {Other macromolecular compounds}
- B29C 48/34: Cross-head annular extrusion nozzles, i.e. for simultaneously receiving moulding material and the preform to be coated
- C08L 71/00: Compositions of polyethers obtained by reactions forming an ether link in the main chain (of polyacetals C08L59/00; of epoxy resins C08L63/00; of polythioether-ethers C08L81/02; of polyether-sulfones C08L81/06); Compositions of derivatives of such polymers
- H01B 3/427: {Polyethers}
- H01B 3/445: {from vinylfluorides or other fluoroethylenic compounds}
- H01B 7/0009: {Details relating to the conductive cores}
- H01B 13/14: by extrusion {(extrusion in general B29C48/00)}
- B29C 48/154: Coating solid articles, i.e. non-hollow articles
- B29K 2027/18: PTFE, i.e. polytetrafluoroethylene {, e.g. ePTFE, i.e. expanded polytetrafluoroethylene}
- B29K 2071/00: Use of polyethers {, e.g. PEEK, i.e. polyether-etherketone or PEK, i.e. polyetherketone or derivatives thereof}, as moulding material
- B29K 2105/0085: {Copolymers}
- B29K 2105/0094: {having particular viscosity}
- B29K 2705/10: Copper
- C08L 2203/202: use in electrical wires or wirecoating
- H01F 5/06: Insulation of windings
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES

## Abstract

The present invention pertains to a rectangular wire including: a rectangular conductor; and a film of an insulating coating material that directly covers the entire circumferential direction of the rectangular conductor, wherein: a melt flow rate of the insulating coating material at a temperature of 372° C. and a load of 49 N is from 20.0 to 300.0 g/10 min; the insulating coating material contains polyaryletherketone (A) and a fluorine-containing copolymer (B) having a unit based on tetrafluoroethylene; an amount of the fluorine-containing copolymer (B) with respect to a total mass of the polyaryletherketone (A) and the fluorine-containing copolymer (B) in the insulating coating material is 5% by mass or more; and the rectangular wire is such that the film of the insulating coating material does not peel off from the rectangular conductor in a winding test conforming to “JIS3216-3:2011 5.1.2 Rectangular Wire”.

## Claims

### Claim 1

A rectangular wire comprising:
a rectangular conductor having a rectangular cross section in a direction perpendicular to the axial direction; and
a film of an insulating coating material formed by extrusion molding that directly covers the entire circumferential direction of said rectangular conductor,
wherein: a melt flow rate of said insulating coating material at a temperature of 372° C. and a load of 49 N is from 20.0 to 300.0 g/10 min;
an average thickness of the film of said insulating coating material is from 10 to 1,000 μm;
an unbiased standard deviation of a thickness of the film of said insulating coating material in the axial direction of said rectangular wire is less than 0.06 mm;
said insulating coating material comprises polyaryletherketone (A) and a fluorine-containing copolymer (B) having a unit based on tetrafluoroethylene;
said fluorine-containing copolymer (B) comprises one or more selected from the group consisting of a fluorine-containing resin (B1) having a melting point of 260° C. or higher and a fluorine-containing elastomer (B2);
an amount of said fluorine-containing copolymer (B) with respect to a total mass of said polyaryletherketone (A) and said fluorine-containing copolymer (B) in said insulating coating material is 5% by mass or more; and
said rectangular wire is such that the film of said insulating coating material does not peel off from said rectangular conductor in a winding test conforming to “JIS3216-3:2011 5.1.2 Rectangular Wire”.

### Claim 2 (depends on 1)

The rectangular wire according to claim 1, wherein a cross sectional area of said rectangular conductor is 2.6 mm2 or more.

### Claim 3 (depends on 1)

The rectangular wire according to claim 1,
wherein said fluorine-containing resin (B1) has a —CH2OH group, and
an amount of said —CH2OH group is more than 30 with respect to 1×106 main chain carbon atoms of said fluorine-containing resin (B1).

### Claim 4 (depends on 1)

The rectangular wire according to claim 1,
wherein said fluorine-containing elastomer (B2) has an iodine atom, and
an amount of said iodine atom is 0.05% by mass or more with respect to a total mass of said fluorine-containing elastomer (B2).

### Claim 5 (depends on 1)

The rectangular wire according to claim 1, wherein a partial discharge inception voltage of said insulating coating material is 600 Vrms or more.

### Claim 6

A method for producing a rectangular wire including a rectangular conductor having a rectangular cross section in a direction perpendicular to the axial direction, and a film of an insulating coating material formed by extrusion molding that directly covers the entire circumferential direction of said rectangular conductor,
the method comprising:
melting a composition containing polyaryletherketone (A) and a fluorine-containing copolymer (B) having a unit based on tetrafluoroethylene using an extruder equipped with a die; and
extruding said composition that has been melted from said die around said rectangular conductor;
thereby coating around said rectangular conductor with said melted composition and forming said insulating coating material,
wherein: a melt flow rate of said insulating coating material at a temperature of 372° C. and a load of 49 N is from 20.0 to 300.0 g/10 min;
an average thickness of the film of said insulating coating material is from 10 to 1,000 μm;
an unbiased standard deviation of a thickness of the film of said insulating coating material in the axial direction of said rectangular wire is less than 0.06 mm;
said fluorine-containing copolymer (B) comprises one or more selected from the group consisting of a fluorine-containing resin (B1) having a melting point of 260° C. or higher and a fluorine-containing elastomer (B2);
an amount of said fluorine-containing copolymer (B) with respect to a total mass of said polyaryletherketone (A) and said fluorine-containing copolymer (B) in said composition is 5% by mass or more; and
said rectangular wire is such that the film of said insulating coating material does not peel off from said rectangular conductor in a winding test conforming to “JIS3216-3:2011 5.1.2 Rectangular Wire”.

### Claim 7 (depends on 6)

The method for producing a rectangular wire according to claim 6, wherein a drawdown ratio DDR calculated by the following Formula 1 is 0.5 or more and less than 10.0,
DDR
=
(
D
A
-
C
A
)
/
(
F
A
-
C
A
)
Formula
⁢
1
wherein DA is an opening area (mm2) of said die, CA is a cross sectional area (mm2) of said rectangular conductor in a direction perpendicular to the axial direction, and FA is a cross sectional area (mm2) of said rectangular wire in a direction perpendicular to the axial direction.

### Claim 8 (depends on 6)

The method for producing a rectangular wire according to claim 6, wherein a cross sectional area of said rectangular conductor is 2.6 mm2 or more.

### Claim 9 (depends on 6)

The method for producing a rectangular wire according to claim 6,
wherein said fluorine-containing resin (B1) has a —CH2OH group, and
an amount of said —CH2OH group is more than 30 with respect to 1×106 main chain carbon atoms of said fluorine-containing resin (B1).

### Claim 10 (depends on 6)

The method for producing a rectangular wire according to claim 6,
wherein said fluorine-containing elastomer (B2) has an iodine atom, and
an amount of said iodine atom is 0.05% by mass or more with respect to a total mass of said fluorine-containing elastomer (B2).

### Claim 11 (depends on 6)

The method for producing a rectangular wire according to claim 6, wherein a partial discharge inception voltage of said insulating coating material is 600 Vrms or more.