# US 2026/0126674 A1 · Electro-opto-acoustic composition and electro-opto-acoustic device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0126674 A1
- Document ID: US20260126674A1
- Status: Published application
- Kind: A1
- Application number: 19/275,997
- Filed: 2025-07-22
- Published: 2026-05-07
- Earliest claimed: 2024-11-04
- Assignees: Korea University of Technology and Education Industry-University Cooperation Foundation
- Applicants: Korea University Of Technology And Education Industry-University Cooperation Foundation
- Inventors: Jin Woo BAE; Seung Ju OH; Seungeun Choi
- Web page: https://patentgrep.com/patent/US20260126674A1

## CPC

- G02F 1/0072: {Mechanical, acoustic, electro-elastic, magneto-elastic properties}
- C09K 11/025: {non-luminescent particle coatings or suspension media}
- C09K 11/584: {with zinc or cadmium}
- G02F 1/0102: {Constructional details, not otherwise provided for in this subclass}
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

The present disclosure relates to an electro-opto-acoustic composition and an electro-opto-acoustic device, wherein, by adding a non-ionic surfactant, it is possible to improve a dielectric constant while simultaneously improving electroluminescence performance, and the electro-opto-acoustic composition according to an embodiment of the present disclosure includes a stretchable silicone rubber, a non-ionic surfactant, and copper-doped zinc sulfide (ZnS:Cu).

## Claims

### Claim 1

An electro-opto-acoustic composition comprising:
a stretchable silicone rubber;
a non-ionic surfactant; and
copper-doped zinc sulfide.

### Claim 2 (depends on 1)

The electro-opto-acoustic composition of claim 1, wherein the stretchable silicone rubber is Ecoflex silicone rubber.

### Claim 3 (depends on 1)

The electro-opto-acoustic composition of claim 1, wherein the non-ionic surfactant comprises octylphenol ethoxylate.

### Claim 4 (depends on 1)

The electro-opto-acoustic composition of claim 1, wherein the content of the non-ionic surfactant is 0.5 parts by weight to 1.5 parts by weight based on 100 parts by weight of the stretchable silicone rubber.

### Claim 5 (depends on 1)

The electro-opto-acoustic composition of claim 1, wherein the content of the copper-doped zinc sulfide is 150 parts by weight to 250 parts by weight based on 100 parts by weight of the stretchable silicone rubber.

### Claim 6

A method for manufacturing an electro-opto-acoustic layer, the method comprising:
mixing a stretchable silicone rubber (Ecoflex), a non-ionic surfactant (Triton X), and copper-doped zinc sulfide (ZnS:Cu) to prepare a mixture;
coating the mixture to form a coating layer; and
drying the coating layer.

### Claim 7 (depends on 6)

The method of claim 6, wherein in the mixture, the content of the non-ionic surfactant is 0.5 parts by weight to 1.5 parts by weight based on 100 parts by weight of the stretchable silicone rubber.

### Claim 8 (depends on 6)

The method of claim 6, wherein in the mixture, the content of the copper-doped zinc sulfide is 150 parts by weight to 250 parts by weight based on 100 parts by weight of the stretchable silicone rubber.

### Claim 9 (depends on 6)

An electro-opto-acoustic device comprising:
a first electro-opto-acoustic layer disposed in one direction;
a second electro-opto-acoustic layer disposed in the other direction perpendicular to the one direction and disposed to be woven with the first electro-opto-acoustic layer;
first electrodes respectively disposed at one end and the other end of the first electro-opto-acoustic layer; and
second electrodes respectively disposed at one end and the other end of the second electro-opto-acoustic layer,
wherein the first and second electro-opto-acoustic layers are as described in claim 6.

### Claim 10 (depends on 1)

A method for manufacturing an electro-opto-acoustic device, the method comprising:
preparing a first electrode;
coating an electro-opto-acoustic composition on the first electrode to form a coating layer;
disposing a second electrode on the coating layer; and
curing the structure in which the first electrode, the coating layer, and the second electrode are stacked,
wherein the electro-opto-acoustic composition is as described in claim 1.

### Claim 11 (depends on 10)

The method of claim 10, wherein in the electro-opto-acoustic composition, the content of the non-ionic surfactant is 0.5 parts by weight to 1.5 parts by weight based on 100 parts by weight of the stretchable silicone rubber.

### Claim 12 (depends on 10)

The method of claim 10, wherein in the electro-opto-acoustic composition, the content of the copper-doped zinc sulfide is 150 parts by weight to 250 parts by weight based on 100 parts by weight of the stretchable silicone rubber.