# US 2026/0125774 A1 · Cold-rolled steel sheet and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0125774 A1
- Document ID: US20260125774A1
- Status: Published application
- Kind: A1
- Application number: 18/934,485
- Filed: 2024-11-01
- Published: 2026-05-07
- Earliest claimed: 2022-05-03
- Assignees: Hyundai Steel Company
- Applicants: Hyundai Steel Company
- Inventors: Kyeong Min Kim; Hyun Seong Noh; Han Sol Maeng; Nam Hoon Goo; Seong Kyung Han
- Web page: https://patentgrep.com/patent/US20260125774A1

## CPC

- C21D 9/46: for sheet metals
- C22C 38/02: containing silicon
- C21D 1/22: Martempering
- C21D 1/78: Combined heat-treatments not provided for above
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0226: {Hot rolling}
- C21D 8/0236: {Cold rolling}
- C21D 8/0247: characterised by the heat treatment
- C21D 8/0263: {following hot rolling}
- C21D 8/0273: {Final recrystallisation annealing}
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/14: containing titanium or zirconium
- C21D 2211/001: Austenite
- C21D 2211/005: Ferrite
- C21D 2211/008: Martensite
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

The present invention provides a cold-rolled steel sheet including 0.15 to 0.20% by weight of carbon (C), 1.0 to 2.0% by weight of silicon (Si), 1.5 to 3.0% by weight of manganese (Mn), greater than 0% by weight and 0.02% by weight or less of phosphorus (P), greater than 0% by weight and 0.003% by weight or less of sulfur (S), 0.01 to 0.3% by weight of aluminum (Al), greater than 0% by weight and 0.01% by weight or less of nitrogen (N), 48/14·[N] to 0.1% by weight of titanium (Ti) ([N] is a content (% by weight) of nitrogen), remaining iron (Fe), and other unavoidable impurities, wherein a final microstructure of the cold-rolled steel sheet consists of ferrite, needle-shaped residual austenite, a martensite/austenite composite structure, and block-shaped martensite; the area fraction of the ferrite may be 30 to 60%, the area fraction of the needle-shaped residual austenite may be 5 to 12%, the area fraction of the martensite/austenite composite structure may be 25 to 50%, and the area fraction of the block-shaped martensite may be 5 to 12%; and an amount of carbon concentrated in residual austenite may be 1.1% by weight or more.

## Claims

### Claim 1

A cold-rolled steel sheet comprising:
0.15 to 0.20% by weight of carbon (C),
1.0 to 2.0% by weight of silicon (Si),
1.5 to 3.0% by weight of manganese (Mn),
greater than 0% by weight and 0.02% by weight or less of phosphorus (P),
greater than 0% by weight and 0.003% by weight or less of sulfur (S),
0.01 to 0.3% by weight of aluminum (Al),
greater than 0% by weight and 0.01% by weight or less of nitrogen (N),
48/14·[N] to 0.1% by weight of titanium (Ti) ([N] is a content (% by weight) of nitrogen), and with balance being iron (Fe),
wherein a final microstructure of the cold-rolled steel sheet consists of ferrite, needle-shaped residual austenite, a martensite/austenite composite structure, and block-shaped martensite;
wherein an area fraction of the ferrite is 30 to 60%, an area fraction of the needle-shaped residual austenite is 5 to 12%, an area fraction of the martensite/austenite composite structure is 25 to 50%, and an area fraction of the block-shaped martensite is 5 to 12%; and
wherein an amount of carbon concentrated in residual austenite is 1.1% by weight or more.

### Claim 2 (depends on 1)

The cold-rolled steel sheet according to claim 1, wherein the ferrite is composed of polygonal ferrite and needle-shaped ferrite, and an area fraction of the needle-shaped ferrite in the ferrite is 40% or more.

### Claim 3 (depends on 1)

The cold-rolled steel sheet according to claim 1, wherein the cold-rolled steel sheet has a tensile strength (TS) of 980 MPa or more and an elongation (El) of 23% or more.

### Claim 4 (depends on 3)

The cold-rolled steel sheet according to claim 3, wherein the cold-rolled steel sheet has a tensile strength (TS) of 980 to 1180 MPa and an elongation (El) of 23 to 25%.

### Claim 5

A method of manufacturing a cold-rolled steel sheet, comprising:
a step (a) of reheating steel comprising 0.15 to 0.20% by weight of carbon (C), 1.0 to 2.0% by weight of silicon (Si), 1.5 to 3.0% by weight of manganese (Mn), greater than 0% by weight and 0.02% by weight or less of phosphorus (P), greater than 0% by weight and 0.003% by weight or less of sulfur (S), 0.01 to 0.3% by weight of aluminum (Al), greater than 0% by weight and 0.01% by weight or less of nitrogen (N), 48/14·[N] to 0.1% by weight of titanium (Ti) ([N] is a content (% by weight) of nitrogen), and with balance being iron (Fe);
a step (b) of hot-rolling the reheated steel;
a step (c) of cold-rolling the hot-rolled steel;
a first annealing step (d) of maintaining the cold-rolled steel at a first annealing temperature of (Ac1+30° C.) or more and (Ac3−30° C.) or less and cooling the cold-rolled steel to a cooling end point temperature of 340° C. or less; and
a second annealing step (e) of maintaining the steel at a second annealing temperature of Ac or more and (Ac3−30° C.) or less, cooling the steel to a cooling end point temperature of a martensite transformation onset temperature (Ms) or more and (bainite transformation onset temperature (Bs)−15° C.) or less, and performing over-aging,
wherein the second annealing temperature is lower than the first annealing temperature.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the step (a) comprises a step of reheating the steel at 1180 to 1300° C.,
wherein the step (b) comprises a step of performing hot-rolling at a finishing rolling temperature of 850 to 950° C. and a coiling temperature of 450 to 650° C., and
wherein the step (c) comprises a step of performing cold-rolling at a reduction ratio of 40 to 70%.

### Claim 7 (depends on 5)

The method according to claim 5, wherein the first annealing step (d) comprises a process of maintaining the cold-rolled steel at the first annealing temperature for 30 to 120 seconds and cooling the cold-rolled steel to a cooling end point temperature of 340° C. or less at a cooling rate of 15° C./s or more.

### Claim 8 (depends on 7)

The method according to claim 7, wherein, after performing the first annealing step (d), an area fraction of ferrite in a microstructure of the steel is 30 to 50%.

### Claim 9 (depends on 5)

The method according to claim 5, wherein the second annealing step (e) comprises a process of maintaining the steel at the second annealing temperature for 30 to 120 seconds, cooling the steel to a cooling end point temperature of a martensite transformation onset temperature (Ms) or more and (bainite transformation onset temperature (Bs)−15° C.) or less at a cooling rate of 15° C./s or more, and performing over-aging for 30 to 300 seconds.

### Claim 10 (depends on 9)

The method according to claim 9, wherein, after performing the second annealing step (e), a microstructure of the steel is composed of ferrite, needle-shaped residual austenite, a martensite/austenite composite structure, and block-shaped martensite;
wherein an area fraction of the ferrite is 30 to 60%, an area fraction of the needle-shaped residual austenite is 5 to 12%; and
wherein an area fraction of the martensite/austenite composite structure is 25 to 50%, and an area fraction of the block-shaped martensite is 5 to 12%.

### Claim 11 (depends on 5)

The method according to claim 5, wherein the cold-rolled steel sheet has a tensile strength (TS) of 980 MPa or more and an elongation (El) of 23% or more.

### Claim 12 (depends on 5)

The method according to claim 5, wherein the cold-rolled steel sheet has a tensile strength (TS) of 980 to 1180 MPa and an elongation (El) of 23 to 25%.

### Claim 13

A cold-rolled steel sheet comprising:
0.15 to 0.20% by weight of carbon (C),
1.0 to 2.0% by weight of silicon (Si),
1.5 to 3.0% by weight of manganese (Mn),
greater than 0% by weight and 0.02% by weight or less of phosphorus (P),
greater than 0% by weight and 0.003% by weight or less of sulfur (S),
0.01 to 0.3% by weight of aluminum (Al),
greater than 0% by weight and 0.01% by weight or less of nitrogen (N),
48/14·[N] to 0.1% by weight of titanium (Ti) ([N] is a content (% by weight) of nitrogen), with the balance being iron (Fe),
wherein a final microstructure of the cold-rolled steel sheet consists of ferrite, needle-shaped residual austenite, a martensite/austenite composite structure, and block-shaped martensite.

### Claim 14 (depends on 13)

The cold-rolled steel sheet according to claim 13, wherein an area fraction of the ferrite is 30 to 60%, an area fraction of the needle-shaped residual austenite is 5 to 12%, an area fraction of the martensite/austenite composite structure is 25 to 50%, and an area fraction of the block-shaped martensite is 5 to 12%.

### Claim 15 (depends on 13)

The cold-rolled steel sheet according to claim 13, wherein the ferrite is composed of polygonal ferrite and needle-shaped ferrite, and an area fraction of the needle-shaped ferrite in the ferrite is 40% or more.

### Claim 16 (depends on 13)

The cold-rolled steel sheet according to claim 13, wherein an amount of carbon concentrated in residual austenite is 1.1% by weight or more.

### Claim 17 (depends on 13)

The cold-rolled steel sheet according to claim 13, wherein the cold-rolled steel sheet has a tensile strength (TS) of 980 or more and an elongation (El) of 23% or more

### Claim 18 (depends on 17)

The cold-rolled steel sheet according to claim 17, wherein the cold-rolled steel sheet has a tensile strength (TS) of 980 to 1180 MPa and an elongation (El) of 23 to 25%.