- Number: US 2026/0125309 A1
- Document ID: US20260125309A1
- Status: Published application
- Kind: A1
- Application number: 19/440,069
- Filed: 2026-01-05
- Published: 2026-05-07
- Earliest claimed: 2023-11-30
- Assignees: Corning Incorporated
- Applicants: Corning Incorporated
- Inventors: Lars Martin Otfried Brusberg; Matthew John Dejneka
- Web page: https://patentgrep.com/patent/US20260125309A1

## CPC

- C03C 3/091: containing aluminium
- C03C 3/095: containing rare earths
- C03C 3/097: containing phosphorus, niobium or tantalum
- C03C 21/005: {to introduce in the glass such metals or metallic ions as Ag, Cu}
- G02B 6/122: Basic optical elements, e.g. light-guiding paths
- G02B 2006/12038: {Glass (SiO2 based materials)}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS

## Abstract

Disclosed herein are embodiments of a glass composition including SiO2 in an amount in a range from 53 mol % to 84 mol %, Al2O3 in an amount in a range from 0.3 mol % to 20 mol %, Na2O in an amount in a range from 3 mol % to 16 mol %, and at least one of Cs2O or Rb2O in an amount in a range from 0.05 mol % to 8 mol %. The glass composition has a first silver ion diffusivity at 110° C. of 5×10−19 m2/s or less, and the glass composition has a second silver ion diffusivity at 350° C. of at least 5×10−17 m2/s at 350° C. The glass composition is particularly suitable for use as a glass substrate of a photonic chip package.

## Claims

### Claim 1

A glass article, comprising:
a glass substrate comprising glass having a composition, in terms of mol % on a representative oxide basis, comprising:
SiO2 in an amount in a range from 61 mol % to 84 mol %;
B2O3 in an amount in a range from 0 mol % to 15 mol %;
Li2O in an amount in a range from 0 mol % to 4 mol %;
SrO in an amount in a range from 0.25 mol % to 10 mol %; and
at least one of Cs2O or Rb2O in an amount in a range from 0.05 mol % to 8 mol %;
a first major surface of the glass substrate;
a second major surface of the glass substrate opposite to the first major surface;
a waveguide comprising silver disposed in the glass substate between the first major surface and the second major surface, and closer to the first major surface than the second major surface.

### Claim 2 (depends on 1)

The glass article of claim 1, wherein the composition comprises no more than 12 mol % Al2O3.

### Claim 3 (depends on 1)

The glass article of claim 1, wherein the glass substrate has a silver ion diffusivity of at most 5×10−19 m2/s at a temperature of 110° C.

### Claim 4 (depends on 1)

The glass article of claim 1, wherein the glass substrate has a silver ion diffusivity of at least 5×10−17 m2/s at 350° C.

### Claim 5 (depends on 1)

The glass article of claim 1, further comprising a depth of layer of from at least 4 micrometers to less than 80 micrometers for the silver.

### Claim 6 (depends on 1)

The glass article of claim 1, wherein the waveguide has a width from at least 1 micrometer to no more than 50 micrometers.

### Claim 7 (depends on 1)

The glass article of claim 1, wherein the waveguide has a refractive index profile comprising a first refractive index (ns) at the first major surface, a bulk refractive index (n0) of the glass, and a maximum refractive index (n1) within the waveguide such that n0<n1 and such that n0≤ns, and (ns−n0)≥0.015.

### Claim 8 (depends on 7)

The glass article of claim 7, wherein (ns−n0)≥0.02, and the waveguide has a propagation loss of 0.1 dB/cm or less at 1310 nm.

### Claim 9

A glass article, comprising:
a glass substrate comprising glass having a composition, in terms of mol % on a representative oxide basis, comprising:
SiO2 in an amount in a range from 53 mol % to 84 mol %;
B2O3 in an amount in a range from 0 mol % to 12.8 mol %;
Li2O in an amount in a range from 0 mol % to 4 mol %;
K2O in an amount in a range from 0 mol % to 6 mol %;
Rb2O in an amount in a range from 0 mol % to 5 mol %; and
alkaline earth metal oxides of the group consisting of MgO, CaO, and SrO, wherein a sum of the alkaline earth metal oxides of the group is in a range from 1 mol % to 16 mol %;
a first major surface of the glass substrate;
a second major surface of the glass substrate opposite to the first major surface;
a waveguide disposed in the glass substate between the first major surface and the second major surface, and closer to the first major surface than the second major surface;
wherein the waveguide has a refractive index profile comprising a first refractive index (ns) at the first major surface, a bulk refractive index (n0) of the glass, and a maximum refractive index (n1) within the waveguide such that n0<n1 and such that n0≤ns.

### Claim 10 (depends on 9)

The glass article of claim 9, wherein the glass further comprises B2O3 in an amount in a range from 0 mol % to 12 mol %.

### Claim 11 (depends on 9)

The glass article of claim 9, wherein the glass substrate has a silver ion diffusivity of at most 5×10−19 m2/s at a temperature of 110° C.

### Claim 12 (depends on 9)

The glass article of claim 9, wherein the glass substrate has a silver ion diffusivity of at least 5×10−17 m2/s at 350° C.

### Claim 13 (depends on 10)

The glass article of claim 10, wherein the glass comprises no more than 0.5 mol % in total of trace metal oxides of the group consisting of oxides of iron, chromium, nickel, copper, and arsenic.

### Claim 14 (depends on 10)

The glass article of claim 10, wherein the first refractive index of the waveguide is a maximum refractive index within the waveguide such that n0<ns, and (ns−n0)≥0.015.

### Claim 15 (depends on 14)

The glass article of claim 14, wherein (ns−n0)≥0.02.

### Claim 16 (depends on 10)

The glass article of claim 10, wherein the waveguide has a propagation loss of 0.1 dB/cm or less at 1310 nm.

### Claim 17

A glass article, comprising:
a glass substrate comprising glass having a composition, in terms of mol % on a representative oxide basis, comprising:
SiO2 in an amount in a range from 61 mol % to 82 mol %;
B2O3 in an amount in a range from 0 mol % to 15 mol %;
Li2O in an amount in a range from 0 mol % to 4 mol %;
K2O in an amount in a range from 0 mol % to 8 mol %; and
Rb2O in an amount in a range from 0 mol % to 5 mol %;
a first major surface of the glass substrate;
a second major surface of the glass substrate opposite to the first major surface;
a waveguide comprising silver disposed in the glass substate between the first major surface and the second major surface,
wherein the waveguide has a refractive index profile comprising a first refractive index (ns) at the first major surface, a bulk refractive index (n0) of the glass, and a maximum refractive index (n1) within the waveguide such that n0<n1 and such that n0≤ns,
wherein the glass substrate has a silver ion diffusivity of at most 5×10−19 m2/s at a temperature of 110° C., and the glass substrate has a second silver ion diffusivity of at least 5×10−17 m2/s at 350° C., and
wherein the first refractive index of the waveguide is a maximum refractive index within the waveguide such that n0<ns and (ns−n0)≥0.02.

### Claim 18 (depends on 17)

The glass article of claim 17, wherein the waveguide has a propagation loss of 0.1 dB/cm or less at 1310 nm.

### Claim 19 (depends on 17)

The glass article of claim 17, wherein the waveguide comprises a depth of layer in a range of 4 μm to 15 μm below the first major surface.

### Claim 20 (depends on 17)

The glass article of claim 17, wherein the waveguide comprises a width in a range from 10 μm to 50 μm.