# US 2026/0125278 A1 · Method for recovering nickel hydroxide and nickel sulfate from nickel-containing materials

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0125278 A1
- Document ID: US20260125278A1
- Status: Published application
- Kind: A1
- Application number: 19/116,540
- Filed: 2023-09-27
- Published: 2026-05-07
- Earliest claimed: 2022-10-06
- Assignees: Korea Institute of Geoscience and Mineral Resources
- Applicants: Korea Institute Of Geoscience And Mineral Resources
- Inventors: Tae-Gong RYU; Jun-Ho SHIN; Jae-Min JEONG
- Web page: https://patentgrep.com/patent/US20260125278A1

## CPC

- C01G 53/10: Sulfates
- C01G 53/05: Hydroxides; Oxyhydroxides
- C22B 1/24: Binding; Briquetting {; Granulating}
- C22B 3/00: Extraction of metal compounds from ores or concentrates by wet processes
- C22B 3/06: in inorganic acid solutions {, e.g. with acids generated in situ; in inorganic salt solutions other than ammonium salt solutions}
- C22B 3/08: Sulfuric acid {, other sulfurated acids or salts thereof}
- C22B 3/22: by physical processes, e.g. by filtration, by magnetic means {, or by thermal decomposition} (treatment or purification of solutions by liquid-liquid extraction C22B3/26)
- C22B 3/44: by chemical processes (treatment or purification of solutions by liquid-liquid extraction C22B3/26, by ion-exchange extraction C22B3/42)
- C22B 7/00: Working up raw materials other than ores, e.g. scrap, to produce non-ferrous metals and compounds thereof; {Methods of a general interest or applied to the winning of more than two metals (briquetting of scrap C22B1/248; preliminary treatment of scrap C22B1/005)}
- C22B 7/007: {by acid leaching}
- C22B 23/00: Obtaining nickel or cobalt
- C22B 23/043: {Sulfurated acids or salts thereof}
- C22B 23/0461: {by chemical methods}
- Y02P 10/20: Recycling
- Y02W 30/84: Recycling of batteries or fuel cells
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

The present invention provides a method for recovering nickel hydroxide and nickel sulfate from nickel-containing materials, wherein the nickel-containing materials are crushed and pulverized and then leached with sulfuric acid, leached residue separation and filtrate separation are performed and then the pH is adjusted to recover nickel hydroxide, and the recovered nickel hydroxide is further subjected to a sulfation reaction to recover nickel sulfate.

## Claims

### Claim 1

A method for recovering nickel hydroxide from nickel-containing material, comprising steps of:
(a-1) crushing and pulverizing a multilayer ceramic capacitor process sludge;
(a-2) leaching the crushed and pulverized multilayer ceramic capacitor process sludge with sulfuric acid to form a first sulfuric acid leachate containing a primary filtrate;
(a-3) separating a leached residue and the primary filtrate from the first sulfuric acid leachate;
(a-4) performing a primary pH adjustment on the first sulfuric acid leachate, from which the leached residue has been separated, to form a second sulfuric acid leachate containing a primary pH-adjusted impurity precipitate and a secondary filtrate;
(a-5) separating the primary pH-adjusted impurity precipitate and the secondary filtrate from the second sulfuric acid leachate;
(a-6) performing a secondary pH adjustment on the second sulfuric acid leachate, from which the impurity precipitate has been separated, to separate nickel hydroxide; and
(a-7) washing the separated nickel hydroxide to recover nickel hydroxide, wherein in the step (a-2) of leaching the crushed and pulverized multilayer ceramic capacitor process sludge with sulfuric acid to form a first sulfuric acid leachate containing a primary filtrate,
a leaching temperature ranges from 10 to 90° C.

### Claim 2 (depends on 1)

The method of claim 1,
wherein in the step (a-1) of crushing and pulverizing a multilayer ceramic capacitor process sludge,
the nickel-containing material includes nickel-containing sludge, nickel-containing slag, nickel-containing minerals, or waste ferronickel slag, which are generated during manufacturing of electrical/electronic devices and recycling process of waste electrical/electronic devices, and
wherein a metallic component of the nickel-containing material includes at least one selected from a group consisting of Ni, Al, Fe, Mg, Si, Ba, Ca, P, Cu, Zn, Zr, B, Ba, Cr, Sr, and Mn.

### Claim 3 (depends on 1)

The method of claim 1,
wherein in the step (a-1) of crushing and pulverizing a multilayer ceramic capacitor process sludge, the crushing and pulverizing process comprises:
a primary crushing step using a jaw crusher or a cone crusher; and
a secondary pulverizing step using a rod mill, a pin mill, a ball mill, a tube mill, a pot mill, a roller mill, a turbo mill, or a tower mill,
wherein a particle size of the crushed and pulverized multilayer ceramic capacitor process sludge ranges from 0.1 μm to 5 mm.

### Claim 4 (depends on 1)

The method of claim 1,
wherein in the step (a-2) of leaching the crushed and pulverized multilayer ceramic capacitor process sludge with sulfuric acid to form a first sulfuric acid leachate containing a primary filtrate,
the sulfuric acid leaching is performed under conditions where a solid-to-liquid ratio of the crushed and pulverized nickel-containing material (g) to sulfuric acid solution (L) ranges from 50 to 200, and
a molar concentration of the sulfuric acid solution ranges from 0.2 to 5 M.

### Claim 5 (depends on 1)

The method of claim 1,
wherein in the step (a-3) of separating a leached residue and the primary filtrate from the first sulfuric acid leachate,
separation of impurity from the first sulfuric acid leachate is performed by separating the leached residue that has not leached.

### Claim 6 (depends on 1)

The method of claim 1,
wherein in the step (a-4) of performing a primary pH adjustment on the first sulfuric acid leachate, from which the leached residue has been separated, to form a second sulfuric acid leachate containing a primary pH-adjusted impurity precipitate and a secondary filtrate,
a pH of the primary pH adjustment ranges from 2 to 7.

### Claim 7 (depends on 1)

The method of claim 1,
wherein in the step (a-5) of separating the primary pH-adjusted impurity precipitate and the secondary filtrate from the second sulfuric acid leachate, the separation of the impurity precipitate from the second sulfuric acid leachate is performed by a pH titration method sequentially using metal hydroxide and metal fluoride,
wherein the metal hydroxide is at least one selected from a group consisting of NaOH, KOH, Mg(OH)2, Ca(OH)2, and Al(OH)3, and
wherein the metal fluoride is at least one selected from a group consisting of sodium fluoride (NaF), ammonium fluoride (NH4F), potassium fluoride (KF), ferrous fluoride (FeF2), ferric fluoride (FeF3), aluminum fluoride (AlF3), and hydrofluoric acid (HF).

### Claim 8 (depends on 1)

The method of claim 1,
wherein in the step (a-5) of separating the primary pH-adjusted impurity precipitate and the secondary filtrate from the second sulfuric acid leachate, the separation of the impurity precipitate from the second sulfuric acid leachate is performed by a pH titration method sequentially using metal hydroxide and metal fluoride,
wherein conditions for the separation of the impurity precipitate include:
a pH titration temperature ranging from 10 to 90° C.;
a molar ratio of nickel to metal hydroxide in the second sulfuric acid leachate ranging from 1:0.01 to 0.01:1; and
a molar ratio of nickel to metal fluoride in the second sulfuric acid leachate, after nickel and impurities in the second sulfuric acid leachate have been pH-titrated and separated as metal hydroxides, ranging from 1:0.02 to 0.02:1.

### Claim 9 (depends on 1)

The method of claim 1,
wherein in the step (a-6) of performing a secondary pH adjustment on the second sulfuric acid leachate, from which the impurity precipitate has been separated, to separate nickel hydroxide,
a pH of the secondary pH adjustment ranges from 6 to 13.

### Claim 10 (depends on 1)

The method of claim 1,
wherein in the step (a-7) of washing the separated nickel hydroxide to recover nickel hydroxide,
the washing is performed using deionized water to remove water-soluble impurity components contained in the nickel hydroxide.

### Claim 11

A method for recovering nickel sulfate from nickel-containing material, comprising steps of:
(a-1) crushing and pulverizing a multilayer ceramic capacitor process sludge;
(a-2) leaching the crushed and pulverized multilayer ceramic capacitor process sludge with sulfuric acid to form a first sulfuric acid leachate containing a primary filtrate;
(a-3) separating a leached residue and the primary filtrate from the first sulfuric acid leachate;
(a-4) performing a primary pH adjustment on the first sulfuric acid leachate, from which the leached residue has been separated, to form a second sulfuric acid leachate containing a primary pH-adjusted impurity precipitate and a secondary filtrate;
(a-5) separating the primary pH-adjusted impurity precipitate and the secondary filtrate from the second sulfuric acid leachate;
(a-6) performing a secondary pH adjustment on the second sulfuric acid leachate, from which the impurity precipitate has been separated, to separate nickel hydroxide;
(a-7) washing the separated nickel hydroxide to recover nickel hydroxide; and
(a-8) performing a sulfation reaction between the recovered nickel hydroxide and a sulfuric acid compound to recover nickel sulfate,
wherein in the step (a-2) of leaching the crushed and pulverized multilayer ceramic capacitor process sludge with sulfuric acid to form a first sulfuric acid leachate containing a primary filtrate,
a leaching temperature ranges from 10 to 90° C.

### Claim 12 (depends on 11)

The method of claim 11,
wherein in the step (a-8) of performing a sulfation reaction between the recovered nickel hydroxide and a sulfuric acid compound to recover nickel sulfate,
the sulfuric acid compound is at least one selected from a group consisting of: sulfuric acid (H2SO4), sulfurous acid (H2SO3), hyposulfurous acid (H2SO2), magnesium sulfate (MgSO4), magnesium sulfite (MgSO3), magnesium hyposulfite (MgSO2), calcium sulfate (CaSO4), calcium sulfite (CaSO3), calcium hyposulfite (CaSO2), ferrous sulfate (FeSO4), ferrous sulfite (FeSO3), ferrous hyposulfite (FeSO2), ferric sulfate (Fe2(SO4)3), ferric sulfite (Fe2(SO3)3), ferric hyposulfite (Fe2(SO2)3), ammonium sulfate ((NH4)2SO4), aluminum sulfate (Al2(SO4)3), aluminum sulfite (Al2(SO3)3), and aluminum hyposulfite (Al2(SO2)3).

### Claim 13 (depends on 11)

The method of claim 11,
wherein in the step (a-8) of performing a sulfation reaction between the recovered nickel hydroxide and a sulfuric acid compound to recover nickel sulfate,
the sulfation reaction is performed under conditions characterized by:
a molar ratio of nickel hydroxide to the sulfuric acid compound, expressed as a molar ratio of SO4/Ni, ranging from 0.5 to 5;
a reaction temperature ranging from 80° C. to 800° C.; and
a reaction time ranging from 0.5 hour to 36 hours.

### Claim 14 (depends on 1)

A nickel hydroxide recovered by the method for recovering nickel hydroxide from nickel-containing material according to claim 1.

### Claim 15 (depends on 11)

A nickel sulfate recovered from the method for recovering nickel sulfate from nickel-containing material according to claim 11.