# US 2026/0121375 A1 · Method of manufacturing aluminum-copper integrated die-casting composite radiator for laser chip and radiator

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0121375 A1
- Document ID: US20260121375A1
- Status: Published application
- Kind: A1
- Application number: 18/859,284
- Filed: 2024-08-07
- Published: 2026-04-30
- Earliest claimed: 2024-07-03
- Assignees: Trio Metal (Gz) Co., Ltd
- Applicants: Trio Metal (Gz) Co., Ltd
- Inventors: Xinyun WANG; Binbin HAI; Yuhuan WANG; Yajun HUANG
- Web page: https://patentgrep.com/patent/US20260121375A1

## CPC

- B22D 19/0072: {for making objects with integrated channels}
- H01S 5/02469: {Passive cooling, e.g. where heat is removed by the housing as a whole or by a heat pipe without any active cooling element like a TEC}
- B22D 19/00: Casting in, on, or around objects which form part of the product (B22D23/04 takes precedence; alumino-thermic welding B23K23/00; coating by casting molten material on the substrate C23C6/00)
- B22D 19/0081: {pretreatment of the insert, e.g. for enhancing the bonding between insert and surrounding cast metal}
- B22D 21/007: {with low melting point, e.g. Al 659 degrees C, Mg 650 degrees C}
- B22D 30/00: Cooling castings, not restricted to casting processes covered by a single main group (accessories for cooling cast stock in continuous casting of metals B22D11/124; controlling or regulating processes or operations for cooling cast stock or mould in continuous casting of metals B22D11/22; chill casting B22D15/00)
- C22F 1/002: {by rapid cooling or quenching; cooling agents used therefor}
- C22F 1/04: of aluminium or alloys based thereon
- C22F 1/08: of copper or alloys based thereon
- H01S 5/02423: {Liquid cooling, e.g. a liquid cools a mount of the laser}
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- H01S: DEVICES USING THE PROCESS OF LIGHT AMPLIFICATION BY STIMULATED EMISSION OF RADIATION [LASER] TO AMPLIFY OR GENERATE LIGHT; DEVICES USING STIMULATED EMISSION OF ELECTROMAGNETIC RADIATION IN WAVE RANGES OTHER THAN OPTICAL
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)

## Abstract

The present disclosure discloses a composite radiator manufactured by an aluminum-copper integrated die-casting process for a laser chip. In the process, a copper heat dissipation assembly, after being completely manufactured, is stably provided in an anti-gravity cavity mold, and is die-cast with an aluminum material to form a copper-aluminum composite, which is subjected to (T4+T6) heat treatments to be prepared into a composite blank; single T2 copper heat dissipation and heat exchange flow paths are formed, an advanced coolant is used, and in combination with a structure design of a cooling module, an totally-enclosed cooling circulation system is formed; and an integrated laser pump source structure with a concise structure, efficient cooling, stable dimension, and easy post processing is manufactured.

## Claims

### Claim 1

A method of manufacturing an aluminum-copper integrated die-casting composite radiator for a laser chip, comprising following steps:
in S1, manufacturing an inner core of a radiator comprising inner-core bodies and inner-core fittings, comprising:
in S11, placing a copper rod into a mold of the inner-core bodies, applying a pulling force to form several inner-core bodies matching a shape of the mold of the inner-core bodies, further milling the inner-core bodies, thus completing manufacturing of the inner-core bodies made of pure copper;
in S12, welding the several inner-core bodies that have been manufactured and the inner-core fittings into one piece;
in S13, subjecting the inner-core bodies and the inner-core fittings welded into one piece to copper polishing, cleaning, nickel plating, and drying treatments, thus completing manufacturing of the inner core of the radiator comprising the inner-core bodies and the inner-core fittings; and
in S14, filling foundry sand into the inner core; and
in S2, manufacturing an outer shell of the radiator, and forming a copper-aluminum composite blank with the inner core and the outer shell being integrated, comprising:
in S21, preparing an aluminum liquid;
in S22, placing the manufactured inner core into an anti-gravity cavity mold, filling the prepared aluminum liquid into the cavity mold, performing a die casting treatment to form a copper-aluminum-part composite blank with the aluminum-made outer shell wrapping the copper-made inner-core bodies and the inner-core fittings, and demolding and naturally cooling to 20-35° C.;
in S23, trimming the outer shell, to remove a material strip and a slag package, and purging and removing the foundry sand in the inner core of the radiator;
in S24, performing T4+T6 heat treatments on the outer shell having undergone the die casting treatment;
in S25, subjecting the outer shell having undergone the heat treatments to CNC roughing; and
in S26, cleaning and drying the integrated copper-aluminum composite blank having been roughed.

### Claim 2 (depends on 1)

The method of manufacturing an aluminum-copper integrated die-casting composite radiator for a laser chip according to claim 1, wherein performing T4+T6 heat treatments on the outer shell having undergone the die casting treatment in the step S24 comprises following substeps:
S241, solutionizing treatment: heating the outer shell to a solutionizing temperature to make solute atoms in the outer shell to be fused into solvent lattice, wherein the solutionizing treatment is performed at a temperature of 470° C.-540 ° C. for a time of 2 h-3 h;
S242, rapid cooling treatment: subjecting the outer shell having undergone the solutionizing treatment to a water-quenching treatment, to rapidly cool the outer shell to 20° C.-35° C.;
S243, aging treatment: continuously heating the rapidly cooled outer shell at a temperature of 120° C.-200° C. for a time of 2 h-3 h; and
S244, natural cooling treatment: leaving the outer shell having undergone the aging treatment to stand at 20° C.-35°C.

### Claim 3 (depends on 1)

The method of manufacturing an aluminum-copper integrated die-casting composite radiator for a laser chip according to claim 1, wherein preparing an aluminum liquid in the step S21 comprises following substeps:
S211, heating and stirring an aluminum material, and adding a grain refiner into the aluminum material in a solution state to form molten aluminum; and
S212, further performing a degassing treatment on the molten aluminum added with the grain refiner to render the prepared aluminum liquid.

### Claim 4 (depends on 1)

The method of manufacturing an aluminum-copper integrated die-casting composite radiator for a laser chip according to claim 1, wherein subjecting the inner-core bodies and the inner-core fittings welded into one piece to copper polishing, cleaning, nickel plating, and drying treatments in the step S13 comprises:
performing the copper polishing to remove an oxide layer, cleaning with an ultrasonic degreasing agent, rinsing with pure water, then performing surface nickel plating treatment, next performing wind-shear dewatering, and then performing tunnel drying, wherein a drying temperature is 100° C. at the highest; and the cleaning and drying the integrated copper-aluminum composite blank in the step S26 comprises: cleaning with an ultrasonic degreasing agent, then rinsing with pure water, next performing wind-shear dewatering, and then performing tunnel drying, wherein a drying temperature is 100° C. at the highest.

### Claim 5 (depends on 1)

The method of manufacturing an aluminum-copper integrated die-casting composite radiator for a laser chip according to claim 1, wherein for milling the inner-core bodies in the step S11, the inner-core bodies are milled using a CNC machining process; and subjecting the outer shell having undergone the heat treatments to CNC roughing in the step S25 is cutting the outer shell.

### Claim 6 (depends on 3)

The method of manufacturing an aluminum-copper integrated die-casting composite radiator for a laser chip according to claim 3, wherein in preparing the aluminum liquid in the step S21, a weight ratio of the grain refiner to the aluminum liquid is 0.2:100.

### Claim 7 (depends on 1)

The method of manufacturing an aluminum-copper integrated die-casting composite radiator for a laser chip according to claim 1, wherein in die-casting solidification shrinkage in the step S22, the die casting treatment is performed at a temperature of 500° C.-800° C. and a pressure of 80 MPa-120 MPa for a time of 150 s-220 s.

### Claim 8 (depends on 1)

The method of manufacturing an aluminum-copper integrated die-casting composite radiator for a laser chip according to claim 1, wherein for the pulling force applied in the step S11, a value of the pulling force is 15000 N-22000 N.

### Claim 9 (depends on 1)

An aluminum-copper integrated die-casting composite radiator for a laser chip, wherein the aluminum-copper integrated die-casting composite radiator for a laser chip is manufactured by the method of manufacturing an aluminum-copper integrated die-casting composite radiator for a laser chip according to a claim 1, and comprises: several inner-core bodies, inner-core fittings and an outer shell, wherein the inner core fittings comprise several connectors and several pipelines, one of the connectors is fixed to an end of a first one of the inner-core bodies by welding, another one of the connectors is fixed to an end of a last one of the inner-core bodies by welding, the pipelines connect the several inner-core bodies end to end, and the outer shell wraps the inner-core bodies and the inner-core fittings that are welded into one piece.

### Claim 10 (depends on 9)

The aluminum-copper integrated die-casting composite radiator for a laser chip according to claim 9, wherein the inner-core bodies each comprise an inner tube provided with several heat dissipation slots on an inner wall; and an outer wall provided with several slot strips, wherein a diameter of the inner tube is the same as an internal diameter of the connectors and a diameter of the pipelines, and a cross section of the heat dissipation slots is in a peak-tooth shape.

### Claim 11

A radiator, comprising several inner-core bodies, inner-core fittings and an outer shell, wherein the inner-core fittings comprise several connectors and several pipelines, one of the connectors is fixed to an end of a first one of the inner-core bodies by welding, another one of the connectors is fixed to an end of a last one of the inner-core bodies by welding, the pipelines connect the plurality of inner-core bodies end to end, and the outer shell wraps the inner-core bodies and the inner-core fittings that are welded into one piece; and the inner-core bodies are bonded by any one of welding bonding, mechanical bonding, metallurgical bonding or other types of bonding.

### Claim 12 (depends on 11)

The radiator according to claim 11, wherein the inner-core bodies each comprise an inner tube provided with several heat dissipation slots on an inner wall; and an outer wall provided with several slot strips; a diameter of the inner tube is the same as an internal diameter of the connectors and a diameter of the pipelines; and a cross section of the heat dissipation slots is any one of following through-hole structures: a peak-tooth shape, a round hole shape, a mesh shape, and a sponge shape.

### Claim 13 (depends on 11)

The radiator according to claim 11, wherein the inner-core bodies are made of a first material, and the outer shell is made of a second material.

### Claim 14 (depends on 13)

The radiator according to claim 13, wherein the first material is any one of following high heat conduction materials: copper, silver, diamond, and boron nitride; and the second material is any one of following die-casting materials: aluminum alloy, zinc alloy, and magnesium alloy.

### Claim 15 (depends on 11)

The radiator according to claim 11, wherein the radiator is at least applied to following fields: laser chips, data centers, high-performance computers, artificial intelligence, and energy storage.

### Claim 16

A method of manufacturing a radiator, comprising steps of:
manufacturing an inner core of a radiator comprising inner-core bodies and inner-core fittings; and
manufacturing an outer shell of the radiator, and forming a metal composite blank with the inner core and the outer shell being integrated.

### Claim 17 (depends on 16)

The method of manufacturing a radiator according to claim 16, wherein the step of manufacturing an inner core of a radiator comprising inner-core bodies and inner-core fittings comprises:
placing a first material into a mold of the inner-core bodies; applying a pulling force, to form several inner-core bodies matching a shape of the mold of the inner-core bodies; and milling the inner-core bodies, so as to manufacture the inner-core bodies;
welding the several inner-core bodies that have been manufactured and the inner-core fittings into one piece;
subjecting the inner-core bodies and the inner-core fittings that are welded into one piece to polishing, cleaning, nickel plating, and drying treatments, so as to manufacture the inner core; and
filling foundry sand into the inner core; and
the step of manufacturing an outer shell of the radiator, and forming a metal composite blank with the inner core and the outer shell being integrated comprises:
preparing a second material liquid;
placing the manufactured inner core into an anti-gravity cavity mold, filling the prepared second material liquid into the anti-gravity cavity mold, and performing a die casting treatment to form a metal composite blank with the first-material outer shell wrapping the second-material inner-core bodies and the inner-core fittings, and demolding and naturally cooling to a first temperature;
trimming the first-material outer shell, to remove a material strip and a slag package, and purging and removing the foundry sand in the inner core;
performing a heat treatment on the first-material outer shell having undergone the die casting treatment;
subjecting the first-material outer shell having undergone the heat treatments to roughing; and
cleaning and drying the integrated metal composite blank having undergone the roughing.

### Claim 18 (depends on 17)

The method of manufacturing a radiator according to claim 17, wherein the step of performing a heat treatment on the first-material outer shell having undergone the die casting treatment comprises:
heating the first-material outer shell to a solutionizing temperature to make solute atoms in the first-material outer shell to be fused into solvent lattice;
subjecting the first-material outer shell having undergone the solutionizing treatment to a water-quenching treatment;
continuously heating the first-material outer shell having undergone the water-quenching treatment at a second temperature for a preset duration; and
leaving the heated first-material outer shell to stand at a third temperature.

### Claim 19 (depends on 17)

The method of manufacturing a radiator according to claim 17, wherein the step of preparing a second material liquid comprises:
heating and stirring the second material, and adding a grain refiner into the second material in a solution state to form a molten second material; and
performing a degassing treatment on the molten second material added with the grain refiner to render the prepared second material liquid.

### Claim 20 (depends on 17)

The method of manufacturing a radiator according to claim 17, wherein the step of subjecting the inner-core bodies and the inner-core fittings that are welded into one piece to polishing, cleaning, nickel plating, and drying treatments comprises:
subjecting the inner-core bodies and the inner-core fittings that are welded into one piece to polishing, cleaning with an ultrasonic degreasing agent, rinsing with pure water, surface nickel plating treatment, wind-shear dewatering, and tunnel drying in sequence; and
the step of cleaning and drying the integrated metal composite blank having undergone the roughing comprises:
subjecting the integrated metal composite blank having undergone the roughing to cleaning with an ultrasonic degreasing agent, rinsing with pure water, wind-shear dewatering, and tunnel drying.