# US 2026/0121016 A1 · Positive electrode material, and preparation method therefor and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0121016 A1
- Document ID: US20260121016A1
- Status: Published application
- Kind: A1
- Application number: 19/489,246
- Filed: 2023-07-27
- Published: 2026-04-30
- Earliest claimed: 2023-07-27
- Assignees: Gem Co., Ltd.; Pt Qmb New Energy Materials; Pt Green Eco Nickel; Pt Esg New Energy Material
- Applicants: Gem Co., Ltd.; Pt Qmb New Energy Materials; Pt Green Eco Nickel; Pt Esg New Energy Material
- Inventors: Kaihua XU; Rizky WANALDI; Andi Syaputra HASIBUAN; Tegar Mukti AJI
- Web page: https://patentgrep.com/patent/US20260121016A1

## CPC

- C01G 45/1221: Manganates or manganites with trivalent manganese, tetravalent manganese or mixtures thereof
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- C01G 45/20: Compounds containing manganese, with or without oxygen or hydrogen, and containing one or more other elements (C01G45/04 - C01G45/12 take precedence)
- C01G 53/44: containing manganese
- C01G 53/82: Compounds containing nickel, with or without oxygen or hydrogen, and containing two or more other elements
- H01M 4/0419: {involving spraying}
- H01M 4/13: Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 4/604: {containing aliphatic main chain polymers}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2004/80: Particles consisting of a mixture of two or more inorganic phases
- C01P 2006/40: Electric properties
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A cathode material, and a preparation method therefor and the use thereof. The preparation method comprises the following steps: (1) mixing a vanadium source, a complexing agent and a high-molecular polymer with an organic solvent to obtain a mixed solution; (2) respectively performing an atomization treatment on the mixed solution and a metal salt solution, and respectively conveying the mixed solution and the metal salt solution with a gas into a spray pyrolysis furnace to perform mixed pyrolysis, so as to obtain a coated precursor; and (3) mixing the coated precursor with a lithium source or a sodium source, and sintering same to obtain a cathode material. By using a spray pyrolysis method, the tap density and uniformity of the precursor are improved while the precursor is coated, such that a cathode material having good performance can be prepared.

## Claims

### Claim at position 1

1-13. (canceled)

### Claim 14

A preparation method for a cathode material, which comprises the following steps:
(1) mixing a vanadium source, a complexant, and a polymer with an organic solvent to obtain a mixed solution;
(2) subjecting the mixed solution and a metal salt solution to an atomization treatment separately and then separately transporting to a spray pyrolysis furnace by gas and performing mixed pyrolysis to obtain a coated precursor; and
(3) mixing and sintering the coated precursor with a lithium source or a sodium source to obtain the cathode material.

### Claim 15 (depends on 14)

The preparation method according to claim 14, wherein the vanadium source in step (1) comprises ammonium metavanadate.

### Claim 16 (depends on 14)

The preparation method according to claim 14, wherein the complexant comprises oxalic acid.

### Claim 17 (depends on 14)

The preparation method according to claim 14, wherein the polymer comprises polyvinylpyrrolidone.

### Claim 18 (depends on 14)

The preparation method according to claim 14, wherein the organic solvent comprises N,N-dimethylformamide.

### Claim 19 (depends on 14)

The preparation method according to claim 14, wherein in step (1), the vanadium source in the mixed solution has a molar concentration of 0.001-0.1 mol/L;
the complexant in the mixed solution has a molar concentration of 0.002-0.2 mol/L.

### Claim 20 (depends on 14)

The preparation method according to claim 14, wherein in step (1), the polymer in the mixed solution has a mass concentration of 10-30 g/L.

### Claim 21 (depends on 14)

The preparation method according to claim 14, wherein in step (2), a solute of the metal salt solution comprises any one or a combination of at least two of a nickel salt, a cobalt salt, a manganese salt, a copper salt, or an iron salt.

### Claim 22 (depends on 14)

The preparation method according to claim 14, wherein in step (2), metal ions in the metal salt solution have a total mass concentration of 80-150 g/L.

### Claim 23 (depends on 14)

The preparation method according to claim 14, wherein in step (2), the atomization treatment comprises an ultrasonic atomization treatment.

### Claim 24 (depends on 14)

The preparation method according to claim 14, wherein in step (2), the mixed pyrolysis is performed at a temperature of 700-950° C.

### Claim 25 (depends on 14)

The preparation method according to claim 14, wherein in step (2), the gas comprises nitrogen and/or oxygen;
the gas has a flow rate of 3-8 L/min.

### Claim 26 (depends on 14)

The preparation method according to claim 14, wherein the lithium source in step (3) comprises any one or a combination of at least two of lithium hydroxide, lithium carbonate, or lithium nitrate;
the sodium source comprises any one or a combination of at least two of sodium carbonate, sodium bicarbonate, sodium sulfate, sodium bisulfate, sodium oxalate, sodium hydroxide, sodium nitrate, or sodium acetate.

### Claim 27 (depends on 14)

The preparation method according to claim 14, wherein a ratio of a molar amount of lithium element in the lithium source or sodium element in the sodium source to a total molar amount of main metal element in the coated precursor is 1-1.15:1.

### Claim 28 (depends on 14)

The preparation method according to claim 14, wherein in step (3), the sintering comprises a primary sintering and a secondary sintering.

### Claim 29 (depends on 28)

The preparation method according to claim 28, wherein the primary sintering is performed at a temperature of 550-600° C.;
the primary sintering is performed for a period of 8-12 h.

### Claim 30 (depends on 28)

The preparation method according to claim 28, wherein the secondary sintering is performed at a temperature of 800-900° C.;
the secondary sintering is performed for a period of 20-30 h.

### Claim 31 (depends on 14)

A cathode material, which is prepared by the method according to claim 14.

### Claim 32 (depends on 31)

A cathode plate, which comprises the cathode material according to claim 31.

### Claim 33 (depends on 32)

A battery, which comprises the cathode plate according to claim 32.