# US 2026/0121010 A1 · Crystalline graphite substrate and measuring device using crystalline graphite substrate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0121010 A1
- Document ID: US20260121010A1
- Status: Published application
- Kind: A1
- Application number: 19/422,526
- Filed: 2025-12-17
- Published: 2026-04-30
- Earliest claimed: 2023-06-26
- Assignees: Panasonic Holdings Corporation
- Applicants: Panasonic Holdings Corporation
- Inventors: NAOMI NISHIKI; RYOU KUWABARA; TAKASHI TSURUTA; KOSO MATSUNO; TOSHIRO MATSUI; MITSURU TANAKA; KEISHIRO ARIMA
- Web page: https://patentgrep.com/patent/US20260121010A1

## CPC

- H01J 49/164: {Laser desorption/ionisation, e.g. matrix-assisted laser desorption/ionisation [MALDI] (sample holders H01J49/0418)}
- C01B 32/20: Graphite
- C01B 32/205: Preparation
- G01N 27/62: by investigating the ionisation of gases, e.g. aerosols; by investigating electric discharges, e.g. emission of cathode
- H01J 49/04: Arrangements for introducing or extracting samples to be analysed, e.g. vacuum locks; Arrangements for external adjustment of electron- or ion-optical components
- H01J 49/0418: {for laser desorption, e.g. matrix-assisted laser desorption/ionisation [MALDI] plates or surface enhanced laser desorption/ionisation [SELDI] plates}
- H01J 49/16: using surface ionisation, e.g. field-, thermionic- or photo-emission
- H01J 49/40: Time-of-flight spectrometers (H01J49/36 takes precedence)
- C01P 2002/76: by a space-group or by other symmetry indications
- C01P 2004/03: obtained by SEM
- C01P 2006/80: Compositional purity
- C01P 2006/90: Other properties not specified above
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

A crystalline graphite substrate having a carbon purity of 95% or more, in which a surface roughness Ra is from 1 μm to 8 μm inclusive, and a FWHM for a peak in X-ray diffraction corresponding to a layer interval at which hexagonal mesh structures in which six-membered rings of carbon atoms are continuous are stacked is from 3.5 degrees to 9 degrees inclusive.

## Claims

### Claim 1

A crystalline graphite substrate having a carbon purity of 95% or more, in which
a surface roughness Ra is from 1 μm to 8 μm inclusive, and
a full width at half maximum (FWHM) for a peak in X-ray diffraction corresponding to a layer interval at which hexagonal mesh structures in which six-membered rings of carbon atoms are continuous are stacked is from 3.5 degrees to 9 degrees inclusive.

### Claim 2 (depends on 1)

The crystalline graphite substrate according to claim 1, wherein a thickness of the crystalline graphite substrate is from 0.05 mm to 3 mm inclusive.

### Claim 3 (depends on 1)

The crystalline graphite substrate according to claim 1, wherein an apparent density of the crystalline graphite substrate is from 0.5 to 1.5 inclusive.

### Claim 4 (depends on 1)

A measuring device that mounts a measurement object in laser desorption ionization, the measuring device comprising:
the crystalline graphite substrate according to claim 1 for a portion on which a measurement object to be ionized is mounted, wherein
the crystalline graphite substrate is held by applying a tensile force from surroundings in a case where the crystalline graphite substrate has a thickness of 0.5 mm or less.

### Claim 5

A method for manufacturing a crystalline graphite substrate, the method comprising:
heating a polyimide film to 2500° C. or higher in an oxygen-free state to release hydrogen, oxygen, and nitrogen, and then recrystallizing remaining carbon atoms to provide a crystalline graphite substrate having a layered shape in which hexagonal mesh structures in which six-membered rings of carbon atoms are continuous are stacked; and
applying a pressing pressure of 0.5 MPa to 10 MPa to the crystalline graphite substrate.

### Claim 6 (depends on 5)

The method according to claim 5, wherein, in the heating of the polyimide film, a temperature raising rate to 1300° C. is set to 7° C./min to 13° C./min, a temperature raising rate from 1300° C. to 2200° C. is set to 4.9° C./min to 9.1° C./min, and a temperature raising rate at 2200° C. or higher is set to 3.5° C./min to 6.5° C./min.