# US 2026/0120997 A1 · Plasma assisted remediation of single crystal diamond surfaces

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0120997 A1
- Document ID: US20260120997A1
- Status: Published application
- Kind: A1
- Application number: 19/376,286
- Filed: 2025-10-31
- Published: 2026-04-30
- Earliest claimed: 2024-10-31
- Assignees: The Government of the United States of America, as represented by the Secretary of the Navy
- Applicants: The Government of the United States of America, as represented by the Secretary of the Navy
- Inventors: Bradford B. Pate; Michael A. Mathews, JR.; Jonathan B. Levine-Miles
- Web page: https://patentgrep.com/patent/US20260120997A1

## CPC

- C30B 29/04: Diamond
- H01J 37/321: {the radio frequency energy being inductively coupled to the plasma}
- C30B 25/186: {being specially pre-treated by, e.g. chemical or physical means}
- C30B 33/12: in gas atmosphere or plasma
- H01J 2237/3341: Reactive etching
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

A method of remediation of single crystal diamond surfaces by: mounting a single crystal diamond seed to a quartz or sapphire substrate, performing a first reactive ion etch from an inductively coupled first plasma on the seed, optionally performing a first rapid thermal anneal on the seed under hydrogen and a first inert gas, performing a second reactive ion etch from an inductively coupled second plasma on the seed, and optionally performing a second rapid thermal anneal on the seed under hydrogen and a second inert gas. The first plasma is an SF6 plasma and has first ion energies from 200 to 300 eV. The second plasma is an SF6 plasma or a hydrogen/inert gas plasma and has second ion energies below 40 eV.

## Claims

### Claim 1

A method comprising:
mounting a single crystal diamond seed to a quartz or sapphire substrate;
performing a first reactive ion etch from an inductively coupled first plasma on the seed;
wherein the first plasma is an SF6 plasma; and
wherein the first plasma has first ion energies from 200 to 300 eV;
optionally, performing a first rapid thermal anneal on the seed under hydrogen and a first inert gas;
performing a second reactive ion etch from an inductively coupled second plasma on the seed;
wherein the second plasma is an SF6 plasma or a hydrogen/inert gas plasma; and
wherein the second plasma has second ion energies below 40 eV; and
optionally, performing a second rapid thermal anneal on the seed under hydrogen and a second inert gas.

### Claim 2 (depends on 1)

The method of claim 1, wherein the first etch reduces a thickness of the seed by at least 0.5 μm.

### Claim 3 (depends on 1)

The method of claim 1, wherein the first anneal has a maximum temperature of 900° C.

### Claim 4 (depends on 1)

The method of claim 1, wherein the first inert gas is argon.

### Claim 5 (depends on 1)

The method of claim 1, wherein the second etch reduces a thickness of the seed by at least 100 nm.

### Claim 6 (depends on 1)

The method of claim 1, wherein the hydrogen/inert gas plasma is a hydrogen/argon plasma.

### Claim 7 (depends on 1)

The method of claim 1, wherein the second anneal has a maximum temperature of 900° C.

### Claim 8 (depends on 1)

The method of claim 1, wherein the second inert gas is argon.

### Claim 9 (depends on 1)

The method of claim 1, further comprising:
performing chemical vapor deposition of diamond onto the seed after the second etch or the second rapid thermal anneal.