# US 2026/0117425 A1 · Method for carbonizing a polymeric object in a molten medium

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0117425 A1
- Document ID: US20260117425A1
- Status: Published application
- Kind: A1
- Application number: 19/369,505
- Filed: 2025-10-27
- Published: 2026-04-30
- Earliest claimed: 2024-10-28
- Applicants: UT-Battelle, LLC; 4XIntellectual Property Holdings, LLC
- Inventors: Felix L. Paulauskas; Hippolyte Grappe; Joshua Nowak
- Web page: https://patentgrep.com/patent/US20260117425A1

## CPC

- D01F 9/22: from polyacrylonitriles
- D01F 11/121: {Halogen, halogenic acids or their salts}
- D10B 2101/12: Carbon; Pitch
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- D10B: INDEXING SCHEME ASSOCIATED WITH SUBLASSES OF SECTION D, RELATING TO TEXTILES

## Abstract

A method for producing a carbonized object, the method comprising immersing a partially carbonized polymeric object into a molten anhydrous medium maintained within a temperature range of 300° C.-1800° C. for a period of time of 0.25-30 minutes under an inert atmosphere to result in conversion of the partially carbonized object into the carbonized object, wherein said partially carbonized polymeric object is 30-70 wt % carbon and the carbonized object is at least 90 wt % carbon. Also described herein is an apparatus useful in practicing the above described method, wherein the apparatus includes a vessel (crucible) constructed of a thermally refractory material for holding the molten medium, and a lid that contains one or more protruding elements (i.e., prongs or projections) or rollers useful for maintaining a polymeric fiber or ribbon immersed in the molten medium.

## Claims

### Claim 1

A method for producing a carbonized object, the method comprising immersing a partially carbonized polymeric object into a molten anhydrous medium maintained within a temperature range of 300° C.-1800° C. for a period of time of 0.25-30 minutes under an inert atmosphere to result in conversion of the partially carbonized object into the carbonized object, wherein said partially carbonized polymeric object is 30-70 wt % carbon and the carbonized object is at least 90 wt % carbon.

### Claim 2 (depends on 1)

The method of claim 1, wherein said carbonized object is at least 92 wt % carbon.

### Claim 3 (depends on 1)

The method of claim 1, further comprising initial steps of producing the partially carbonized polymeric object by a) subjecting a polymeric object to an oxidation/stabilization step in which the polymeric object is heated to a temperature of 200-300° C. under an oxidative atmosphere, and b) subjecting the oxidized/stabilized polymeric object to a low temperature carbonization step in which the oxidized/stabilized polymeric object is heated to a temperature of 300° C.-1200° C. under an inert atmosphere to result in conversion of the oxidized/stabilized polymeric object into the partially carbonized object.

### Claim 4 (depends on 1)

The method of claim 1, further comprising a subsequent step of subjecting the carbonized object to a graphitization step by immersing the carbonized object into a molten anhydrous medium maintained at a graphitization temperature above 1800° C. for a period of time of 0.25-10 minutes under an inert atmosphere to result in conversion of the carbonized object into the graphitized object.

### Claim 5 (depends on 4)

The method of claim 4, wherein the graphitization temperature is at least 2000° C.

### Claim 6 (depends on 1)

The method of claim 1, wherein said partially carbonized polymeric object has a partially carbonized polyacrylonitrile (PAN) composition.

### Claim 7 (depends on 1)

The method of claim 1, wherein said molten anhydrous medium comprises a metal or metal alloy having a melting point below 1800° C.

### Claim 8 (depends on 7)

The method of claim 7, wherein said metal or metal alloy has a melting point below 1000° C.

### Claim 9 (depends on 7)

The method of claim 7, wherein said molten anhydrous medium is selected from the group consisting of tin, aluminum, and Ni—P alloy.

### Claim 10 (depends on 1)

The method of claim 1, wherein said molten anhydrous medium comprises a molten salt.

### Claim 11 (depends on 10)

The method of claim 10, wherein said molten salt is a metal salt.

### Claim 12 (depends on 11)

The method of claim 11, wherein said metal salt is selected from halides and oxides of alkali, alkaline earth, and metalloid elements.

### Claim 13 (depends on 1)

The method of claim 1, wherein said partially carbonized polymeric object is a continuous fiber, fiber tow, or ribbon.

### Claim 14 (depends on 1)

The method of claim 1, wherein said partially carbonized polymeric object is subjected to tension during the immersion step.

### Claim 15 (depends on 1)

The method of claim 1, wherein said partially carbonized polymeric object is subjected to said temperature range of 300° C.-1800° C. in a single heating zone.

### Claim 16 (depends on 1)

The method of claim 1, wherein said partially carbonized polymeric object is subjected to said temperature range of 300° C.-1800° C. in at least first and second heating zones, with each zone containing the molten anhydrous medium, and wherein the molten anhydrous medium in each zone is independently temperature controlled to be within a separate temperature sub-range within the range of 300° C.-1800° C.

### Claim 17

An apparatus useful in immersing a carbonizable continuous fiber or ribbon in a high temperature molten medium, the apparatus comprising:
(i) a vessel portion useful in holding the high temperature molten medium and constructed of a thermally refractory material capable of heating to 3000° C. without deformation, wherein the vessel portion has an open portion; and
(ii) a lid that conforms to the shape of the opening of the vessel and which contains an outer side and an inner side, wherein the inner side faces the open portion of the vessel and contains at least one protruding element also constructed of a thermally refractory material, wherein the protruding element protrudes into the open portion and functions to maintain the carbonizable continuous fiber or ribbon immersed in the high temperature molten medium;
wherein at least one of the vessel and lid includes an indentation that positions and guides the carbonizable continuous fiber or ribbon over the protruding element and into the high temperature molten medium during operation.

### Claim 18 (depends on 17)

The apparatus of claim 17, further comprising a heating device connected to the vessel.

### Claim 19 (depends on 17)

The apparatus of claim 17, further comprising the high temperature molten medium in the vessel portion.

### Claim 20 (depends on 19)

The apparatus of claim 19, wherein said high temperature molten medium is selected from the group consisting of tin, aluminum, and Ni—P alloy.