# US 2026/0117334 A1 · Hollow wind turbine main shaft and profiling forging process and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0117334 A1
- Document ID: US20260117334A1
- Status: Published application
- Kind: A1
- Application number: 18/848,539
- Filed: 2024-03-08
- Published: 2026-04-30
- Earliest claimed: 2023-10-31
- Assignees: Zenkung Heavy Industry (Jiangsu) Co., Ltd.
- Applicants: Zenkung Heavy Industry (Jiangsu) Co., Ltd.
- Inventors: Zhijie ZHAO; Liang XU; Zhenwei YAN; Zhen YUAN
- Web page: https://patentgrep.com/patent/US20260117334A1

## CPC

- C21D 9/28: for plain shafts
- B21K 1/063: {hollow (hollow racks B21K1/768)}
- C21D 7/00: Modifying the physical properties of iron or steel by deformation (apparatus for mechanical working of metal B21, B23, B24)
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/008: {containing tin}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/42: with copper
- C22C 38/44: with molybdenum or tungsten
- C22C 38/46: with vanadium
- C22C 38/58: with more than 1.5% by weight of manganese
- C22C 38/60: containing lead, selenium, tellurium, or antimony, or more than 0.04% by weight of sulfur
- F03D 9/25: the apparatus being an electrical generator (F03D9/22 takes precedence)
- F03D 15/00: Transmission of mechanical power
- F05B 2230/25: by forging
- F05B 2240/61: hollow
- Y02E 10/72: Wind turbines with rotation axis in wind direction
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- B21K: MAKING FORGED OR PRESSED METAL PRODUCTS, e.g. HORSE-SHOES, RIVETS, BOLTS OR WHEELS (making particular articles by working sheet metal without essentially removing material B21D; processing wire B21F; making pins, needles or nails B21G; making particular articles by rolling B21H; forging machines, pressing machines, hammering machines, in general B21J; making chains B21L; plating B23K)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- F03D: WIND MOTORS
- F05B: INDEXING SCHEME RELATING TO WIND, SPRING, WEIGHT, INERTIA OR LIKE MOTORS, TO MACHINES OR ENGINES FOR LIQUIDS COVERED BY SUBCLASSES F03B, F03D AND F03G
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A hollow wind turbine main shaft and a profiling forging process and a use thereof are provided. The profiling forging process includes: step S1: smelting alloying elements according to a formula to obtain a melt, casting the melt to obtain an ingot, and hot-feeding the ingot; step S2: reheating the ingot hot-fed in the step S1, followed by primary drawing-out, primary upsetting, secondary drawing-out, and secondary upsetting to obtain a forged ingot; step S3: reheating the forged ingot, followed by punching to obtain a punched forging; step S4: reheating the punched forging, and performing drawing-out and rounding on a shaft body of the punched forging to obtain a finished forging; and step S5: placing the finished forging into a thermal insulation barrel for slow cooling, and air-cooling the finished forging to a room temperature to obtain the hollow wind turbine main shaft.

## Claims

### Claim 1

A profiling forging process of a hollow wind turbine main shaft, comprising the following steps:
step S1: billet hot-feeding: smelting alloying elements according to a formula to obtain a melt, casting the melt to obtain an ingot, and hot-feeding the ingot, wherein a mass ratio of Mn to Ni in the formula is Mn:Ni=1:(1.05-1.22);
step S2: drawing-out and upsetting: reheating the ingot hot-fed in the step S1, followed by primary drawing-out, primary upsetting, secondary drawing-out, and secondary upsetting for a forging process to obtain a forged ingot, wherein
before the forging process, the ingot hot-fed in the step S1 is reheated to 1,260° C. to 1,280° C. at a first heating rate of 70° C./hour to 80° C./hour for 5 hours to 6 hours; and
the primary drawing-out is performed at a first forging ratio of 6.1 to 6.5, the primary upsetting is performed at a second forging ratio of 6.7 to 7.2, the secondary drawing-out is performed at a third forging ratio of 3.3 to 3.6, and the secondary upsetting is performed at a fourth forging ratio of 3.8 to 4.1; and the primary drawing-out and the primary upsetting are performed at a first temperature ranging from 1,080° C. to 1,260° C., and the secondary drawing-out and the secondary upsetting are performed at a second temperature ranging from 980° C. to 1,080° C.;
step S3: ingot punching: reheating the forged ingot obtained in the step S2, followed by punching to obtain a punched forging;
step S4: drawing-out and rounding: reheating the punched forging obtained in the step S3, and performing drawing-out and rounding on a shaft body of the punched forging to obtain a finished forging, wherein the punched forging is reheated to 1,200° C. to 1,220° C. at a second heating rate of 50° C./hour to 60° C./hour and then subjected to the drawing-out: the drawing-out is performed with a first anvil width ratio of 0.6 to 0.8, a first reduction of 80 mm to 100 mm, a 90° clockwise turning mode, and a first feed of 0.4 to 0.6 of a first anvil width to obtain a drawn-out forging: the drawn-out forging is reheated to 1,200° C. to 1,220° C. before the drawn-out forging is subjected to the rounding; and the rounding is performed at a third temperature of 700° C. to 980° C. with a second anvil width ratio of 0.8 to 0.9, a second reduction of 10 mm to 20 mm, and a second feed of 0.7 to 0.8 of a second anvil width; and
step S5: post-forging controlled cooling: placing the finished forging obtained in the step S4 into a first thermal insulation barrel for slow cooling, and air-cooling the finished forging to a room temperature to obtain the hollow wind turbine main shaft.

### Claim 2 (depends on 1)

The profiling forging process of the hollow wind turbine main shaft according to claim 1, wherein the formula comprises the following alloying elements in mass percentage: C: 0.36% to 0.42%, Si: 0.15% to 0.25%, Mn: 1.21% to 1.73%, Ni: 1.27% to 2.11%, P: ≤0.02%, S: ≤0.02%, Cr: 0.91% to 1.18%, Mo: 0.22% to 0.29%, Cu: ≤0.1%, V: 0.03% to 0.12%, Sn: ≤0.002%, Sb: ≤0.001%, and Fe: the balance.

### Claim 3 (depends on 1)

The profiling forging process of the hollow wind turbine main shaft according to claim 1, wherein in the step S1, the ingot is hot-fed in a second thermal insulation barrel at 850° C. to 880° C. after demoulding of the ingot.

### Claim 4 (depends on 1)

The profiling forging process of the hollow wind turbine main shaft according to claim 1, wherein in the step S3, the punching is performed with a punch pointing downward and comprises a primary punching and a secondary back-side punching, wherein the primary punching is performed at a fourth temperature of 1,150° C. to 1,180° C. until the forged ingot is punched to a depth of ⅔ of the forged ingot; and then, the forged ingot is reheated to 1,150° C. to 1,180° C. at a third heating rate of 80° C./hour to 90° C./hour, and the forged ingot is turned 180° for the secondary back-side punching until the forged ingot is punched through.

### Claim 5 (depends on 1)

The profiling forging process of the hollow wind turbine main shaft according to claim 1, wherein in the step S5, the finished forging is slowly cooled to 180° C. to 200° C. at a slow cooling rate of 5° C./hour to 10° C./hour in the first thermal insulation barrel, and taken out of the first thermal insulation barrel and air-cooled to the room temperature.

### Claim 6 (depends on 1)

A hollow wind turbine main shaft obtained by the profiling forging process of the hollow wind turbine main shaft according to claim 1.

### Claim 7 (depends on 6)

The hollow wind turbine main shaft according to claim 6, wherein a microstructure distribution of the hollow wind turbine main shaft is a complex phase structure comprising a matrix phase and a grain-boundary MnNi phase.

### Claim 8 (depends on 6)

The hollow wind turbine main shaft according to claim 6, wherein the hollow wind turbine main shaft has a tensile strength of 921 MPa to 981 MPa, a yield strength of 803 MPa to 936 MPa, a hardness of 336 HB to 391 HB, and a −40° C. impact energy AKV/J of 105 to 109.

### Claim 9 (depends on 6)

A use of the hollow wind turbine main shaft according to claim 6 in a wind turbine generator system.

### Claim 10 (depends on 6)

A wind turbine generator system, comprising the hollow wind turbine main shaft according to claim 6.

### Claim 11 (depends on 1)

The profiling forging process of the hollow wind turbine main shaft according to claim 1, wherein a microstructure distribution of the hollow wind turbine main shaft is a complex phase structure comprising a matrix phase and a grain-boundary MnNi phase.

### Claim 12 (depends on 1)

The profiling forging process of the hollow wind turbine main shaft according to claim 1, wherein the hollow wind turbine main shaft has a tensile strength of 921 MPa to 981 MPa, a yield strength of 803 MPa to 936 MPa, a hardness of 336 HB to 391 HB, and a −40° C. impact energy AKV/J of 105 to 109.