# US 2026/0117115 A1 · Corrosion inhibitor composition and method for inhibiting corrosion in geothermal well system

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0117115 A1
- Document ID: US20260117115A1
- Status: Published application
- Kind: A1
- Application number: 19/365,737
- Filed: 2025-10-22
- Published: 2026-04-30
- Earliest claimed: 2024-10-24
- Assignees: Chemtreat, Inc.
- Applicants: Chemtreat, Inc.
- Inventors: Patrick WOOD
- Web page: https://patentgrep.com/patent/US20260117115A1

## CPC

- C09K 8/54: Compositions for in situ inhibition of corrosion in boreholes or wells
- C09D 5/086: {Organic or non-macromolecular compounds}
- C09D 7/45: Anti-settling agents
- C09D 7/63: organic
- C23F 11/10: using organic inhibitors
- C23F 11/126: {Aliphatic acids}
- C23F 11/141: {Amines; Quaternary ammonium compounds}
- C23F 11/142: {Hydroxy amines}
- C23F 11/144: {Aminocarboxylic acids}
- C23F 11/145: {Amides; N-substituted amides}
- C23F 11/149: {Heterocyclic compounds containing nitrogen as hetero atom}
- C23F 11/1673: {Esters of phosphoric or thiophosphoric acids}
- E21B 41/02: in situ inhibition of corrosion in boreholes or wells
- C09K 2208/32: Anticorrosion additives
- F03G 4/069: {characterised by the brine or scale treatment, e.g. brine desalination, scale deposit prevention or corrosion-proofing}
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C23F: NON-MECHANICAL REMOVAL OF METALLIC MATERIAL FROM SURFACE (working metal by laser beams B23K26/00; desurfacing by applying flames B23K7/00; working of metal by electro-erosion B23H; producing decorative effects by removing surface material, e.g. by engraving, by etching, B44C1/22; electrolytic etching or polishing C25F); INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL; MULTI-STEP PROCESSES FOR SURFACE TREATMENT OF METALLIC MATERIAL INVOLVING AT LEAST ONE PROCESS PROVIDED FOR IN CLASS C23 AND AT LEAST ONE PROCESS COVERED BY SUBCLASS C21D OR C22F OR CLASS C25
- E21B: EARTH OR ROCK DRILLING; OBTAINING OIL, GAS, WATER, SOLUBLE OR MELTABLE MATERIALS OR A SLURRY OF MINERALS FROM WELLS
- F03G: SPRING, WEIGHT, INERTIA OR LIKE MOTORS; MECHANICAL-POWER PRODUCING DEVICES OR MECHANISMS, NOT OTHERWISE PROVIDED FOR OR USING ENERGY SOURCES NOT OTHERWISE PROVIDED FOR (arrangements in connection with power supply in vehicles from force of nature B60K16/00; electric propulsion with power supply in vehicles from force of nature B60L8/00)

## Abstract

A method for inhibiting corrosion of a corrodible metal surface that contacts a water stream in a geothermal well system. The method includes introducing into the water stream a corrosion inhibitor composition comprising: (i) a cationic surfactant, such as an imidazoline and/or a fatty amine ethoxylate, and (ii) an anionic surfactant.

## Claims

### Claim 1

A method for inhibiting corrosion of a corrodible metal surface that contacts a water stream in a geothermal well system, the method comprising:
introducing into the water stream a corrosion inhibitor composition comprising: (i) a cationic surfactant including at least one of an imidazoline and a fatty amine ethoxylate, and (ii) an anionic surfactant.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the anionic surfactant is selected from the group consisting of an alkyl ether carboxylate, acyl sarcosine, an alkyl amphoacetate, and an alkyl sulfonate.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the anionic surfactant is selected from the group consisting of a linear or branched chain, alkoxylated C6-C36 alkyl ether carboxylate, oleoyl sarcosine, and sodium cocoamphoacetate.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the corrosion inhibitor composition further comprises a mercaptan.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the mercaptan is dialkyl dithiophosphate, mercaptoalkyl alcohol, or thioglycolic acid.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the water stream of the geothermal system is injected through an injection inlet to a subterranean production well, where the water stream is heated, and then the heated water stream is produced above ground through a production outlet.

### Claim 7 (depends on 6)

The method according to claim 6, wherein the water stream is heated to a temperature in a range of 150° C. to 500° C.

### Claim 8 (depends on 6)

The method according to claim 6, wherein steam from the heated water stream is delivered to a turbine to generate electric power.

### Claim 9 (depends on 6)

The method according to claim 6, wherein the heated water stream is liquid water and/or water vapor.

### Claim 10 (depends on 6)

The method according to claim 6, wherein the water stream produced by the production well has a calcium concentration in a range of 100 ppm to 40,000 ppm.

### Claim 11 (depends on 6)

The method according to claim 6, wherein the corrosion inhibitor composition is introduced into the water stream before the water stream is injected through the injection inlet of the geothermal well system to the subterranean production well, or the corrosion inhibitor composition is introduced into the water stream through a capillary tube that extends towards the production well.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the corrosion inhibitor composition forms a protective film on the corrodible metal surface.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the corrosion inhibitor composition is stable at temperatures in a range of 150° C. to 500° C.

### Claim 14 (depends on 1)

The method according to claim 1, wherein the corrosion inhibitor composition is introduced into the water stream in an amount in a range of from 0.1 ppm to 40 ppm.

### Claim 15 (depends on 1)

The method according to claim 1, wherein the corrosion inhibitor composition is introduced into the water stream in an amount in a range of from 1 ppm to 30 ppm.