# US 2026/0116829 A1 · Aluminum/ceramic bonding substrate and method for producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0116829 A1
- Document ID: US20260116829A1
- Status: Published application
- Kind: A1
- Application number: 19/005,457
- Filed: 2024-12-30
- Published: 2026-04-30
- Earliest claimed: 2020-07-29
- Assignees: Dowa Metaltech Co., Ltd.; Mitsubishi Electric Corporation
- Applicants: Dowa Metaltech Co, Ltd.; Mitsubishi Electric Corporation
- Inventors: Koji Kobayashi; Takuma Tsubota; Hideyo Osanai; Daisuke Oya
- Web page: https://patentgrep.com/patent/US20260116829A1

## CPC

- C04B 37/021: {in a direct manner, e.g. direct copper bonding [DCB]}
- C22C 21/08: with silicon
- H05K 3/101: {by casting or moulding of conductive material}
- B32B 15/04: comprising metal as the main or only constituent of a layer, {which is} next to another layer of {the same or of} a {different material (next to a bituminous or tarry layer B32B11/08; next to a water-setting substance layer B32B13/06; next to a glass layer B32B17/061; next to a cellulosic plastic layer B32B23/042)}
- C04B 2235/6565: Cooling rate
- C04B 2235/6584: at an oxygen percentage below that of air
- C04B 2235/95: Products characterised by their size, e.g. microceramics
- C04B 2237/343: Alumina or aluminates
- C04B 2237/365: Silicon carbide
- C04B 2237/366: Aluminium nitride
- C04B 2237/368: Silicon nitride
- C04B 2237/402: Aluminium
- C04B 2237/704: of one or more of the ceramic layers or articles
- C04B 2237/706: of one or more of the metallic layers or articles
- H05K 2203/128: Molten metals, e.g. casting thereof, or melting by heating and excluding molten solder
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM

## Abstract

There is provided an aluminum/ceramic bonding substrate having a ceramic substrate, an aluminum plate of an aluminum alloy which is bonded directly to one side of the ceramic substrate, an aluminum base plate of the aluminum alloy which is bonded directly to the other side of the ceramic substrate, and a plate-shaped reinforcing member which has a higher strength than that of the aluminum base plate and which is arranged in the aluminum base plate to be bonded directly to the aluminum base plate, wherein the aluminum alloy contains 0.01 to 0.2% by weight of magnesium, 0.01 to 0.1% by weight of silicon, and the balance being aluminum and unavoidable impurities.

## Claims

### Claim at position 1

1-9. (canceled)

### Claim 10

A method for producing an aluminum/ceramic bonding substrate, the method comprising the steps of:
arranging a ceramic substrate and a reinforcing member in a mold so that the ceramic substrate is apart from the reinforcing member;
injecting a molten metal of an aluminum alloy so that the molten metal contacts both sides of the ceramic substrate and the surface of the reinforcing member in the mold;
cooling the mold to solidify the molten metal to form an aluminum plate of the aluminum alloy on one side of the ceramic substrate to allow the aluminum plate to be bonded directly to the one side of the ceramic substrate while forming an aluminum base plate of the aluminum alloy on the other side of the ceramic substrate to allow the aluminum base plate to be bonded directly to the other side of the ceramic substrate and while arranging the reinforcing member so as to be surrounded by the aluminum base plate to be bonded directly to the aluminum base plate,
wherein the aluminum alloy contains 0.01 to 0.2% by weight of magnesium, 0.01 to 0.1% by weight of silicon, and the balance being aluminum and unavoidable impurities.

### Claim 11 (depends on 10)

A method for producing an aluminum/ceramic bonding substrate as set forth in claim 10, wherein said aluminum alloy contains 0.01 to 0.1% by weight of titanium.

### Claim 12 (depends on 10)

A method for producing an aluminum/ceramic bonding substrate as set forth in claim 10, wherein said reinforcing member is made of a metal or ceramic, which has a higher melting point than that of said aluminum alloy.

### Claim 13 (depends on 10)

A method for producing an aluminum/ceramic bonding substrate as set forth in claim 10, wherein said ceramic substrate is made of at least one selected from the group consisting of alumina, aluminum nitride, silicon nitride and silicon carbide.