# US 2026/0116812 A1 · Opaque quartz glass having high absorption in the infrared range

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0116812 A1
- Document ID: US20260116812A1
- Status: Published application
- Kind: A1
- Application number: 19/376,304
- Filed: 2025-10-31
- Published: 2026-04-30
- Earliest claimed: 2024-10-31
- Assignees: Heraeus Quarzglas GmbH & Co. KG
- Applicants: Heraeus Quarzglas GmbH & Co. KG
- Inventors: Andreas GÖTZENDORFER; Nadine TSCHOLITSCH; Jörg HAMMERSCHMIDT; Torsten JENEK; Frank WESSELY
- Web page: https://patentgrep.com/patent/US20260116812A1

## CPC

- C03C 10/0009: {containing silica as main constituent}
- C03C 14/004: {the non-glass component being in the form of particles or flakes}
- C03B 19/06: by sintering, {e.g. by cold isostatic pressing of powders and subsequent sintering, by hot pressing of powders, by sintering slurries or dispersions not undergoing a liquid phase reaction}
- C03B 19/066: {for the production of quartz or fused silica articles (other processes specially adapted for the production of quartz or fused silica articles C03B20/00)}
- H10P 72/0436: {mainly by radiation}
- C03C 2214/16: Microcrystallites, e.g. of optically or electrically active material
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A composite material comprising a matrix which is made of quartz glass and into which regions of a silicon carbide-containing phase are embedded. A method for producing the composite material having the following method steps: providing a mixture comprising amorphous quartz glass particles and a silicon carbide-containing powder as a suspension; forming a shaped body by means of a slip casting method starting from the suspension produced to obtain a green body; drying the green body; and, sintering the dried green body. A use of a composite material for producing a part for components of process chambers in which semiconductor wafers are processed into chips, for systems in which high-temperature processes are carried out, for components which are heated by means of radiation and for components which block thermal radiation.

## Claims

### Claim 1

A composite material comprising a matrix which is made of quartz glass and into which regions of a silicon carbide-containing phase are embedded.

### Claim 2 (depends on 1)

The composite material according to claim 1, wherein the composite material has an absorption of a 3 mm thick disk at 1500 nm of greater than 40%, more preferably greater than 50%.

### Claim 3 (depends on 1)

The composite material according to claim 1, wherein the composite material has a hemispherical reflection of a 3 mm thick disk at 1500 nm of less than 60%, more preferably less than 50%.

### Claim 4 (depends on 1)

The composite material according to claim 1, wherein the composite material has a transmission of a 3 mm thick disk of less than 10%, more preferably less than 1%, even more preferably less than 0.6%, in the wavelength range from 0.4 to 2.5 μm.

### Claim 5 (depends on 1)

The composite material according to claim 1, wherein the composite material has a change in the absorption capacity/emissivity of a 3 mm disk at a wavelength of 1.5 μm between room temperature (20° C.) and 1000° C. of less than 0.3, more preferably less than 0.2, particularly preferably less than 0.1.

### Claim 6 (depends on 1)

The composite material according to claim 1, wherein the weight proportion of the silicon carbide-containing phase, in each case based on the matrix made of quartz glass, is 0.25 to 10 wt. %, more preferably 0.5 to 9 wt. %, even more preferably 1 to 8 wt. %, even more preferably 1.5 to 7 wt. %, even more preferably 2 to 6 wt. %, even more preferably 2.5 to 5 wt. %.

### Claim 7 (depends on 1)

The composite material according to claim 1, wherein the d50 value of the particle size distribution of the silicon carbide particles is 0.1 to 100 μm, more preferably 0.5 to 75 μm, even more preferably 1 to 50 μm, even more preferably 2 to 25 μm.

### Claim 8 (depends on 1)

The composite material according to claim 1, wherein the composite material has metal impurities of less than 100 ppm, more preferably less than 50 ppm, even more preferably less than 25 ppm, the metal impurities being determined by optical emission spectroscopy with inductively coupled plasma.

### Claim 9 (depends on 1)

The composite material according to claim 1, wherein the composite material has a porosity of less than 8%, more preferably less than 6%, even more preferably less than 5%, the porosity being defined as the pore volume based on the total volume of the composite material.

### Claim 10 (depends on 1)

The composite material according to claim 1, wherein the composite material has a carbon content of less than 0.1 wt. %, more preferably less than 0.075 wt. %, even more preferably less than 0.05 wt. %, in each case based on the total weight of the composite material.

### Claim 11 (depends on 1)

The composite material according to claim 1, wherein the composite material is free of carbon.

### Claim 12 (depends on 1)

A method for producing the composite material according to claim 1, having the following method steps:
a. providing a mixture comprising amorphous quartz glass particles and a silicon carbide-containing powder as a suspension;
b. forming a shaped body by means of a slip casting method starting from the suspension produced in method step a. to obtain a green body;
c. drying the green body; and
d. sintering the dried green body resulting from method step c.

### Claim 13 (depends on 12)

The method according to claim 12, wherein the grain size distribution of the quartz glass particles in the suspension has a d90 value of less than 100 μm, more preferably less than 75 μm, even more preferably less than 50 μm, in each case determined by laser diffraction according to ISO 2019:13320.

### Claim 14 (depends on 12)

The method according to claim 12, wherein the solids content in the aqueous suspension consisting of quartz glass particles is more than 50 wt. %, more preferably more than 65 wt. %, even more preferably more than 75 wt. %.

### Claim 15 (depends on 1)

A use of a composite material according to claim 1 for producing a part for components of process chambers in which semiconductor wafers are processed into chips, for systems in which high-temperature processes are carried out, for components which are heated by means of radiation and for components which block thermal radiation.