# US 2026/0116755 A1 · Method for recovering high-efficiency lithium from low-concentration lithium waste liquid and lithium carbonate produced thereby

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0116755 A1
- Document ID: US20260116755A1
- Status: Published application
- Kind: A1
- Application number: 19/145,145
- Filed: 2023-12-28
- Published: 2026-04-30
- Earliest claimed: 2023-01-03
- Assignees: Korea Institute of Geoscience and Mineral Resources
- Applicants: Korea Institute Of Geoscience And Mineral Resources
- Inventors: Tae-Gong RYU; Jun-Ho SHIN; Jae-Min JEONG
- Web page: https://patentgrep.com/patent/US20260116755A1

## CPC

- C01B 25/301: {Preparation from liquid orthophosphoric acid or from an acid solution or suspension of orthophosphates}
- C01D 7/00: Carbonates of sodium, potassium or alkali metals in general
- C01D 15/02: Oxides; Hydroxides
- C01D 15/06: Sulfates; Sulfites
- C01D 15/08: Carbonates; Bicarbonates
- C22B 3/08: Sulfuric acid {, other sulfurated acids or salts thereof}
- C22B 3/24: by adsorption on solid substances, e.g. by extraction with solid resins
- C22B 26/12: Obtaining lithium
- C25C 1/02: of light metals
- C25C 3/02: of alkali or alkaline earth metals
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- Y02P 10/20: Recycling
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01D: COMPOUNDS OF ALKALI METALS, i.e. LITHIUM, SODIUM, POTASSIUM, RUBIDIUM, CAESIUM, OR FRANCIUM (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides C01B17/22; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia and cyanogen, containing nitrogen and other non-metals C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; phosphides C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C25C: PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY OR REFINING OF METALS; APPARATUS THEREFOR
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present invention provides a method for recovering high-efficiency lithium from a low-concentration lithium waste liquid, and lithium carbonate produced thereby, the method comprising the steps of: adsorbing lithium-containing metal ions from a lithium waste liquid onto an electrode in an electric adsorption system, and desorbing the metal ions adsorbed on the electrode with a desorption solution (S10); preparing an insoluble lithium compound by adding an aluminum source to the desorption solution (S20); preparing a leachate by acid leaching or roasting/water leaching of the insoluble lithium compound (S30); and producing at least one of lithium phosphate, liquid sulfate, and lithium carbonate from the leachate.

## Claims

### Claim 1

A method for recovering high-efficiency lithium from a low-concentration lithium waste liquid, comprising:
a step (S10) of adsorbing lithium-containing metal ions from a lithium waste liquid onto an electrode in an electric adsorption system, and desorbing the metal ions adsorbed on the electrode with a desorption solution, wherein the lithium waste liquid has a lithium content of 100 ppm or less;
a step (S20) of preparing an insoluble lithium compound by adding an aluminum source to the desorption solution;
a step (S30) of preparing a leachate by acid leaching or roasting/water leaching of the insoluble lithium compound;
a step of heat-treating the roasted insoluble lithium compound; and
a step (S40) of producing at least one selected from the group consisting of lithium phosphate, lithium sulfate, and lithium carbonate from the leachate,
wherein, in step (S10), lithium ion concentration in the desorption solution ranges from 500 to 1000 ppm,
wherein, in step (S20), the insoluble lithium compound is Li—Al-LDH(LiAl2(OH)7·2H2O),
wherein, in step (S30), a 1.5 M sulfuric acid solution is used in the acid leaching, and wherein the heat-treating step is performed at a temperature of 700° C.

### Claim 2

(canceled)

### Claim 3 (depends on 1)

The method of claim 1,
wherein, in step S10, the adsorption and the desorption are performed in an alternating manner, once or 2 to 20 times repeatedly under a potential of 1 V to 2 V, and
wherein a residual solution remaining on the electrode is removed between the adsorption and the desorption and after the desorption.

### Claim 4 (depends on 1)

The method of claim 1,
wherein the aluminum source includes at least one selected from the group consisting of aluminum, sodium aluminate, aluminum hydroxide, alumina, aluminum chloride, and aluminum sulfate.

### Claim 5 (depends on 1)

The method of claim 1,
wherein, in step S20, the aluminum source is added to the desorption solution and reacted such that a molar ratio of Al to Li ranges from 1 to 4, to precipitate the insoluble lithium compound.

### Claim 6 (depends on 1)

The method of claim 1,
wherein, when the leachate is prepared by the acid leaching of the insoluble lithium compound,
the insoluble lithium compound and a sulfuric acid solution are mixed and reacted such that a solid-to-liquid ratio (g/L) of the insoluble lithium compound to the sulfuric acid solution ranges from 50 to 500,
and a molar concentration of the sulfuric acid solution ranges from 0.5 M to 5 M.

### Claim 7 (depends on 1)

The method of claim 1,
wherein, when the leachate is prepared by the roasting/water leaching of the insoluble lithium compound,
the roasting performed prior to the water leaching is sulfuric acid roasting or salt roasting.

### Claim 8 (depends on 7)

The method of claim 7,
wherein, when the sulfuric acid roasting is performed,
the insoluble lithium compound and a sulfuric acid solution are mixed such that a solid-to-liquid ratio (g/L) of the insoluble lithium compound to the sulfuric acid solution ranges from 100 to 2000, and reacted at a temperature of 200° C. to 400° C. for 30 minutes to 2 hours to produce a sulfuric acid roasting conversion product,
and a molar concentration of the sulfuric acid solution ranges from 1 M to 5 M.

### Claim 9 (depends on 8)

The method of claim 8,
wherein the sulfuric acid roasting conversion product is heat-treated at a temperature of 600° C. to 1000° C. for 1 hour to 5 hours prior to the water leaching.

### Claim 10 (depends on 7)

The method of claim 7,
wherein, when the salt roasting is performed, at least one reactant selected from the group consisting of chlorides (Me-Cl) and sulfates (Me-SO4) is mixed with the insoluble lithium compound,
wherein, when a chloride is used as the reactant, a molar ratio of Li to Cl is adjusted to range from 0.5 to 1.5,
wherein, when a sulfate is used as the reactant, a molar ratio of Li to SO4 is adjusted to range from 1.6 to 2.5, and
wherein the reactant mixed with the insoluble lithium compound is reacted at a temperature of 500° C. to 900° C. for 3 hours to 5 hours.

### Claim 11 (depends on 1)

The method of claim 1,
wherein the water leaching is performed once or 2 to 10 times repeatedly.

### Claim 12 (depends on 1)

The method of claim 1,
wherein step S40 includes:
a step (S41) of producing lithium phosphate from the leachate;
a step (S42) of producing a lithium sulfate solution from the lithium phosphate; and
a step (S43) of producing lithium carbonate from the lithium sulfate solution.

### Claim 13 (depends on 12)

The method of claim 12,
wherein, in step S41, a phosphate source and a sodium source are added to the leachate such that a molar ratio of Li to PO4 ranges from 2 to 4 and a molar ratio of Na to PO4 ranges from 2 to 4, and the leachate mixed with the phosphate source and the sodium source is reacted for 4 hours to 30 hours.

### Claim 14 (depends on 12)

The method of claim 12,
wherein, in step S42, the lithium phosphate is mixed with a sulfate (Me-SO4) solution dissolved in distilled water and reacted such that a molar ratio of Li to SO4 ranges from 1 to 3 and a solid-to-liquid ratio (g/L) of the lithium phosphate to the sulfate solution ranges from 80 to 320, to produce the lithium sulfate solution.

### Claim 15 (depends on 14)

The method of claim 14,
wherein the sulfate includes at least one selected from the group consisting of MgSO4, (NH4)2SO4, and Al2(SO4)3.

### Claim 16 (depends on 14)

The method of claim 14,
wherein step S43 includes:
a step of removing impurities by adding an alkaline agent to the lithium sulfate solution; and
a step of producing the lithium carbonate by adding a carbonate source to the lithium sulfate solution from which the impurities have been removed.

### Claim 17 (depends on 16)

The method of claim 16,
wherein, in the step of removing impurities by adding an alkaline agent to the lithium sulfate solution,
calcium hydroxide is added to the lithium sulfate solution to precipitate and remove aluminum, and
sodium hydroxide is added to adjust the pH to 11 or higher to remove calcium ions.

### Claim 18 (depends on 16)

The method of claim 16,
wherein, in the step of producing the lithium carbonate by adding a carbonate source to the lithium sulfate solution from which the impurities have been removed,
the carbonate source is added such that a molar ratio of Li to CO3 ranges from 1.5 to 2.5, and
the lithium carbonate is precipitated by stirring the mixture at a temperature of 40° C. to 90° C. for 1 hour to 24 hours.

### Claim 19 (depends on 16)

The method of claim 16,
wherein the carbonate source includes at least one selected from the group consisting of sodium carbonate (Na2CO3), sodium bicarbonate (NaHCO3), potassium carbonate (K2CO3), potassium bicarbonate (KHCO3), calcium carbonate (CaCO3), magnesium carbonate (MgCO3), and barium carbonate (BaCO3).

### Claim 20 (depends on 1)

Lithium carbonate produced by the method of claim 1.