# US 2026/0115677 A1 · Composition and process for pelletizing carbon-based materials for proppant and industrial applications

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0115677 A1
- Document ID: US20260115677A1
- Status: Published application
- Kind: A1
- Application number: 19/431,176
- Filed: 2025-12-23
- Published: 2026-04-30
- Earliest claimed: 2019-03-28
- Assignees: Carbo Ceramics Inc.
- Applicants: Carbo Ceramics, Inc.
- Inventors: Minjung CHO; Todd Roper; Thu Lieng
- Web page: https://patentgrep.com/patent/US20260115677A1

## CPC

- B01J 2/06: in a liquid medium
- B01J 6/001: {Calcining}
- C01B 33/40: Clays
- C04B 33/04: Clay; Kaolin
- C04B 33/13: Compounding ingredients (C04B33/36, C04B35/71 take precedence {; pigments for ceramics C09C1/0009})
- C04B 35/10: based on aluminium oxide
- C04B 35/14: based on silica
- C04B 35/62695: {Granulation or pelletising (devices for shaping artificial aggregates from ceramic mixtures B28B1/004)}
- C04B 35/62839: {Carbon}
- C09K 8/805: {Coated proppants}
- C10B 57/005: {After-treatment of coke, e.g. calcination desulfurization}
- C01P 2006/40: Electric properties
- C04B 2235/3217: Aluminum oxide or oxide forming salts thereof, e.g. bauxite, alpha-alumina
- C04B 2235/3418: Silicon oxide, silicic acids or oxide forming salts thereof, e.g. silica sol, fused silica, silica fume, cristobalite, quartz or flint
- C04B 2235/42: Non metallic elements added as constituents or additives, e.g. sulfur, phosphor, selenium or tellurium
- C04B 2235/425: Graphite
- C04B 2235/95: Products characterised by their size, e.g. microceramics
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- C10B: DESTRUCTIVE DISTILLATION OF CARBONACEOUS MATERIALS FOR PRODUCTION OF GAS, COKE, TAR, OR SIMILAR MATERIALS (cracking oils C10G; underground gasification of minerals E21B43/295)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS

## Abstract

A method for producing an electrically-conductive pellet includes reducing a size of a first material. The method also includes wetting the first material to produce a first slurry. The method also includes introducing the first slurry into a fluidizer to produce a first pellet. The method also includes reducing a size of a second material. The second material is an electrically-conductive material. The method also includes wetting the second material to produce a second slurry. The method also includes applying the second slurry to the first pellet.

## Claims

### Claim 1

A method for producing a pellet, comprising:
reducing a size of a material;
wetting the material with water and alginate to produce a slurry; and
flowing the slurry through a nozzle to produce a droplet of the slurry and the droplet falls into a solution to solidify the slurry into a pellet.

### Claim 2 (depends on 1)

The method of claim 1, wherein the material is selected from the group consisting of coke, metal, graphite, and combinations thereof.

### Claim 3 (depends on 1)

The method of claim 1, wherein the material comprises a blend of clay and coke.

### Claim 4 (depends on 1)

The method of claim 1, wherein the pellet has an electrical conductivity of about 100 S/m to about 4000 S/m.

### Claim 5 (depends on 1)

The method of claim 1, further comprising heating the pellet to a temperature of about 1,200° C. to about 1,450° C. to provide a sintered pellet.

### Claim 6 (depends on 5)

The method of claim 5, wherein the pellet has an electrical conductivity of about 100 S/m to about 4000 S/m.

### Claim 7

A method for producing an electrically-conductive pellet, comprising:
reducing a size of a first material, wherein the first material is alumina, silica, kaolin ore, or bauxite ore or combinations thereof;
wetting the first material to produce a first slurry;
introducing the first slurry into a fluidizer to produce a first pellet;
reducing a size of a second material, wherein the second material comprises an electrically-conductive material;
wetting the second material to produce a second slurry;
applying the second slurry to the first pellet to provide an electrically conductive pellet; and
calcining the electrically-conductive pellet to provide a calcined electrically-conductive pellet comprising a core that is a calcined first material and a shell comprising calcined electrically-conductive material.

### Claim 8 (depends on 7)

The method of claim 7, wherein the electrically conductive material is selected from the group consisting of metal, graphite, and combinations thereof.

### Claim 9 (depends on 7)

The method of claim 7, wherein the second material comprises a blend of clay and petroleum coke.

### Claim 10 (depends on 7)

The method of claim 7, wherein an average cross-sectional length of the calcined electrically-conductive pellet is about 200 μm to about 4000 μm.

### Claim 11 (depends on 7)

The method of claim 7, wherein a bulk density of the calcined electrically-conductive pellet is about 0.3 g/cm3 to about 2.0 g/cm3.

### Claim 12 (depends on 7)

The method of claim 7, wherein an electrical conductivity of the calcined electrically-conductive pellet is about 100 S/m to about 3000 S/m.

### Claim 13 (depends on 7)

The method of claim 7, further comprising:
reducing a size of a third material, wherein the third material comprises a combination of the first material and the second material; and
wetting the third material to produce a third slurry.

### Claim 14 (depends on 13)

The method of claim 13, further comprising applying the third material to the first pellet before the second slurry is applied such that the third material is positioned at least partially between the first pellet and the second material.

### Claim 15 (depends on 7)

The method of claim 7, further comprising:
reducing a size of a third material, wherein the third material comprises a combination of the first material and the second material;
wetting the third material to produce a third slurry;
applying the third material to the first pellet before the second slurry is applied such that the third material is positioned at least partially between the first pellet and the second material; and
calcining the electrically-conductive pellet after the second and third materials have been applied to the first pellet.

### Claim 16 (depends on 15)

The method of claim 15, wherein:
an average cross-sectional length of the calcined electrically-conductive pellet is about 300 μm to about 2000 μm,
a bulk density of the calcined electrically-conductive pellet is about 0.5 g/cm3 to about 1.6 g/cm3, and
an electrical conductivity of the calcined electrically-conductive pellet is about 500 S/m to about 2000 S/m.

### Claim 17 (depends on 15)

The method of claim 15, wherein an average cross-sectional length of the calcined electrically-conductive pellet is from about 300 μm to about 2000 μm.

### Claim 18 (depends on 15)

The method of claim 15, wherein a bulk density of the calcined electrically-conductive pellet is about 0.5 g/cm3 to about 1.6 g/cm3.

### Claim 19 (depends on 15)

The method of claim 15, wherein an electrical conductivity of the electrically-conductive pellet is about 500 S/m to about 2000 S/m.

### Claim 20 (depends on 7)

The method of claim 7, wherein calcining is performed at a temperature of about 1,200° C. to about 1,450° C. to provide a sintered pellet.