# US 2026/0114320 A1 · Die to wafer direct hybrid bonding method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0114320 A1
- Document ID: US20260114320A1
- Status: Published application
- Kind: A1
- Application number: 19/142,842
- Filed: 2023-12-22
- Published: 2026-04-23
- Earliest claimed: 2022-12-28
- Assignees: Commissariat A L'energie Atomique Et Aux Energies Alternatives; SET Corporation
- Applicants: Commissariat A L'energie Atomique Et Aux Energies Alternatives; Set Corporation
- Inventors: Frank FOURNEL; Loic SANCHEZ; Noura NADI; Nicolas RAYNAUD; Antoine SARCIAT; Tifenn KERBIRIOU; Clément CASTAN
- Web page: https://patentgrep.com/patent/US20260114320A1

## CPC

- H10W 80/163: {using active alignment, e.g. detecting marks and correcting position}
- H10W 90/00: Package configurations
- H10W 46/00: Marks applied to devices, e.g. for alignment or identification
- H10W 46/301: {for alignment}
- H10W 72/0711: {Apparatus therefor}
- H10W 72/072: {of bump connectors}
- H10W 72/90: Bond pads, in general
- H10W 80/00: Direct bonding of chips, wafers or substrates
- H10W 80/016: {Cleaning}
- H10W 80/331: {characterised by the application of energy for connecting}
- H10W 99/00: Subject matter not provided for in other groups of this subclass
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A die to wafer direct hybrid bonding method includes providing at least one die comprising a first copper pad and a first silicon oxide layer, providing a wafer comprising a second copper pad and a second silicon oxide layer, and handling the die so as to position the face of the die facing the zone for receiving the die on the wafer, by aligning the first and second pads. At least one water drop is deposited in the zone for receiving the die and/or on the face of the die. Pressure on the die is applied to form, from the water drop, a water film between the face and the zone for receiving the die.

## Claims

### Claim at position 1

1-16. (canceled)

### Claim 17

A die to wafer direct bonding method, comprising:
providing at least one die having a first flat face, providing at least one wafer having a second flat face comprising a zone for receiving the die,
handling the die, so as to position the first face of the die facing the zone for receiving the die on the second face of the wafer by aligning the die opposite the wafer,
putting the first face of the die in contact with the zone for receiving the die, so as to bond the die on the second face of the wafer,
before putting into contact, a deposition of at least one water drop in the zone for receiving the die on the second face of the wafer and/or on the first face of the die, and during the handling of the die and after deposition of the water drop, an application of a pressure on the die configured to form, from the deposited water drop, a water film between the first face and the zone for receiving the die, the application of the pressure on the die being configured, such that the position of the die opposite the wafer is not modified, due to presence of water between the die and the wafer,
drying after application of pressure, to remove the water film and bring the die into contact with the wafer, the drying being carried out at a temperature strictly less than 100° C., and
after the drying, performing annealing configured to reinforce the bonding of the die on the wafer,
wherein the second face has a peripheral zone at a perimeter of the zone for receiving the die, the peripheral zone and the zone for receiving the die both being hydrophilic.

### Claim 18 (depends on 17)

The method according to claim 17, wherein:
the die comprises at least one first pad based upon a first material and a first layer based upon a second material, and the first flat face is formed by exposed parts of the first pad and of the first layer,
the wafer comprises at least one second pad based upon the first material and a second layer based upon the second material, and the zone for receiving the die is formed by exposed parts of the second pad and of the second layer, and
the method being a die to wafer direct hybrid bonding method.

### Claim 19 (depends on 18)

The method according to claim 18, wherein the first material is chosen from among copper, titanium, nickel, gold, and tungsten, and wherein the second material is chosen from among SiO2, Si3N4, SiCN, Al2O3, TiN, TaN, and WN.

### Claim 20 (depends on 17)

The method according to claim 17, wherein the first flat face comprises first alignment marks and the second flat face comprises second alignment marks, and wherein the alignment of the die opposite the wafer is performed via the first and second alignment marks.

### Claim 21 (depends on 20)

The method according to claim 20, wherein the second alignment marks are disposed in the zone for receiving the die, and wherein the deposition of the at least one water drop is configured such that the at least one water drop does not totally cover the second alignment marks.

### Claim 22 (depends on 17)

The method according to claim 17, wherein the water film extends over the second face, outside of the zone for receiving the die.

### Claim 23 (depends on 17)

The method according to claim 17, wherein the water film extends over the second face, by remaining within the zone for receiving the die.

### Claim 24 (depends on 17)

The method according to claim 17, wherein the water film has a thickness less than 5 μm.

### Claim 25 (depends on 17)

The method according to claim 17, wherein the deposited water drop initially occupies, before application of pressure, a surface on the zone for receiving the die which is smaller, than a surface corresponding to the zone for receiving the die, and the application of pressure spreads the water drop on and outside of the zone for receiving the die, to form the water film between the first face and the zone for receiving the die.

### Claim 26 (depends on 17)

The method according to claim 17, wherein the deposited water drop has a volume less than or equal to 100 μL.

### Claim 27 (depends on 17)

The method according to claim 17, wherein the deposited water drop has a volume of between 8 nL and 10 μL.

### Claim 28 (depends on 17)

The method according to claim 17, wherein the pressure applied is maintained for a duration of between 100 ms and 10 s.

### Claim 29 (depends on 17)

The method according to claim 17, wherein a relative humidity of the atmosphere is controlled so as to be greater than or equal to 80% during the handling of the die.

### Claim 30 (depends on 17)

The method according to claim 17, wherein the drying step is carried out at ambient temperature.

### Claim 31 (depends on 17)

The method according to claim 17, wherein the annealing step is carried out at a temperature greater than or equal to 300° C. for a duration greater than or equal to 2 hours.

### Claim 32 (depends on 17)

The method according to claim 17, wherein the water film has a thickness less than 50 nm.