# US 2026/0110105 A1 · Method for forming simultaneously superhydrophobic and superoleophobic surface on 6000-series aluminum alloy omitting pre-patterning step in anodization process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0110105 A1
- Document ID: US20260110105A1
- Status: Published application
- Kind: A1
- Application number: 18/850,424
- Filed: 2022-12-06
- Published: 2026-04-23
- Earliest claimed: 2022-03-30
- Assignees: Dong-Eui University Industrial-Academic Cooperation Foundation
- Applicants: Dong-Eui University Industrial-Academic Cooperation Foundation
- Inventors: Chanyoung JEONG
- Web page: https://patentgrep.com/patent/US20260110105A1

## CPC

- C25D 11/24: Chemical after-treatment
- B05D 5/08: to obtain an anti-friction or anti-adhesive surface (rendering particulate materials free-flowing in general, e.g. making them hydrophobic B01J2/30)
- C09D 183/04: Polysiloxanes
- C25D 11/04: of aluminium or alloys based thereon
- C25D 11/08: containing inorganic acids
- C25D 11/12: Anodising more than once, e.g. in different baths
- C25D 11/18: After-treatment, e.g. pore-sealing
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

A method for manufacturing a superhydrophilic anodized film on a 6000-series aluminum alloy, according to the present invention, enables the manufacture of a uniform anodized film even without a pre-patterning step, thus reducing manufacturing costs, and can impart superhydrophobicity and superoleophobicity to the anodized film due to a coating composition using a crosslinked PDMS derivative represented by Chemical Formula 1 and an organic solvent in a specific mixing ratio, wherein the coating composition is prepared at low cost and enables adjustment of the thickness of a coating film to several nanometers to several tens of nanometers, and thus can also be applied to the coating of microstructured oxide films.

## Claims

### Claim 1

A manufacturing method of an oleophobic and hydrophobic film on a 6000 series aluminum alloy, comprising:
a step of performing primary anodic oxidation on a 6000 series aluminum alloy for 1 to 10 minutes at 35 to 45 V (step 1);
a step of performing pore expansion (pore widening) by immersing the alloy in 0.05 to 1.0 M phosphoric acid (H3PO4) solution for 10 to 60 minutes (Step 2); and
a step of performing secondary anodic oxidation for 1 to 10 minutes at 35 to 45 V (step 3); and
a step of coating with a coating composition including a cross-linked polydimethylsiloxane (PDMS) derivative represented by Chemical Formula 1 and an organic solvent (step 4),
wherein prior to step 1, a pre-patterning process is omitted.
(In Chemical Formula 1, x and y are each an integer of 1 to 30).

### Claim 2 (depends on 1)

The manufacturing method of claim 1, wherein the 6000 series aluminum alloy is one or more selected from a group consisting of Al 6061, Al 6060, Al 6063, Al 6005, Al6005A, Al 6262, and Al 6020.

### Claim 3 (depends on 1)

The manufacturing method of claim 1, wherein the anodic oxide film formed on the 6000 series aluminum alloy surface through steps 1 to 3 has a pillar-on-pore shape in which pillars are formed on a porous structure.

### Claim 4 (depends on 1)

The manufacturing method of claim 1, wherein in the pre-patterning process, the 6000 series aluminum alloy is anodic oxidized and then etched to remove the anodic oxide film to remain a microstructure pattern on a surface of the 6000 series aluminum alloy.

### Claim 5 (depends on 1)

The manufacturing method of claim 1, comprising:
a step of performing primary anodic oxidation on a 6000 series aluminum alloy for 4 to 8 minutes at 38 to 42 V (step 1);
a step of performing pore widening by immersing the alloy in 0.05 to 0.15 M phosphoric acid (H3PO4) solution for 35 to 45 minutes (step 2); and
a step of performing secondary anodic oxidation for 4 to 8 minutes at 38 to 42 V (step 3).

### Claim 6 (depends on 5)

The manufacturing method of claim 5, comprising:
a step of performing primary anodic oxidation on a 6000 series aluminum alloy for 5 to 7 minutes at 39 to 41 V (step 1);
a step of performing pore widening by immersing the alloy in 0.06 to 0.14 M phosphoric acid (H3PO4) solution for 38 to 42 minutes (step 2); and
a step of performing secondary anodic oxidation for 5 to 7 minutes at 39 to 41 V (step 3).

### Claim 7 (depends on 6)

The manufacturing method of claim 6, comprising:
a step of performing primary anodic oxidation on a 6000 series aluminum alloy for 5.8 to 6.2 minutes at 39.5 to 40.5 V (step 1);
a step of performing pore widening by immersing the alloy in 0.095 to 0.105 M phosphoric acid (H3PO4) solution for 39 to 41 minutes (step 2); and
a step of secondarily anodizing for 5.8 to 6.2 minutes at 39.5 to 40.5 V (step 3).

### Claim 8 (depends on 1)

The manufacturing method of claim 1, wherein an organic solvent in step 4 is one of pentane, hexane, heptane, and octane.

### Claim 9 (depends on 1)

The manufacturing method of claim 1, wherein the coating composition used in the step 4 contains 0.01 to 10 parts by weight of a cross-linked PDMS (Polydimethylsiloxane) derivative represented by Chemical Formula 1, based on 10 parts by weight of the organic solvent.

### Claim 10 (depends on 9)

The manufacturing method of claim 9, wherein the coating composition used in the step 4 contains 0.04 to 5 parts by weight of a cross-linked PDMS (Polydimethylsiloxane) derivative represented by Chemical Formula 1, based on 10 parts by weight of the organic solvent.

### Claim 11 (depends on 10)

The manufacturing method of claim 10, wherein the coating composition used in the step 4 contains 0.04 to 2 parts by weight of a cross-linked PDMS (Polydimethylsiloxane) derivative represented by Chemical Formula 1, based on 10 parts by weight of the organic solvent.

### Claim 12 (depends on 11)

The manufacturing method of claim 11, wherein the coating composition used in the step 4 contains 0.04 to 1 parts by weight of a cross-linked PDMS (Polydimethylsiloxane) derivative represented by Chemical Formula 1, based on 10 parts by weight of the organic solvent.

### Claim 13 (depends on 12)

The manufacturing method of claim 12, wherein the coating composition used in the step 4 contains 0.05 to 0.17 parts by weight of a cross-linked PDMS (Polydimethylsiloxane) derivative represented by Chemical Formula 1, based on 10 parts by weight of the organic solvent.

### Claim 14 (depends on 1)

The manufacturing method of claim 1, wherein the coating composition used in the step 4 does not contain a polydimethylsiloxane (PDMS) derivative represented by the following Chemical Formula 2.
(in Chemical Formula 2, m is an integer of 1 to 100)

### Claim 15 (depends on 1)

A 6000 series aluminum alloy with an oleophobic and hydrophobic film manufactured by the manufacturing method of claim 1.