# US 2026/0109789 A1 · Devulcanized rubber, process for producing devulcanized rubber, and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0109789 A1
- Document ID: US20260109789A1
- Status: Published application
- Kind: A1
- Application number: 19/122,790
- Filed: 2023-10-17
- Published: 2026-04-23
- Earliest claimed: 2022-10-27
- Assignees: Evonik Operations GmbH
- Applicants: Evonik Operations GmbH
- Inventors: Roland Krafczyk; Christian Mani; Rupert Schnell; Alexander Paasche
- Web page: https://patentgrep.com/patent/US20260109789A1

## CPC

- C08C 19/085: {Devulcanisation}
- C08J 11/22: by treatment with organic oxygen-containing compounds
- C08L 17/00: Compositions of reclaimed rubber
- C08J 2317/00: Characterised by the use of reclaimed rubber
- Y02W 30/62: Plastics recycling; Rubber recycling
- C08C: TREATMENT OR CHEMICAL MODIFICATION OF RUBBERS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

Subject matter of the invention is a devulcanized rubber having a TAVP of <2.7. The devulcanized rubber is produced by comminuting vulcanized rubber and reacting it at temperatures between 140-180° C. for 4 to 7 minutes with vinylsilane as devulcanizing agent and with a concentration of vinylsilane of 4 to 6 wt %, based on the vulcanized rubber, and with an energy input during the reaction of >140 kNm.

## Claims

### Claim 1

A devulcanized rubber obtained by reaction of vulcanized rubber with vinylsilane,
wherein a Total Area of Visible Particles (TAVP) of the devulcanized rubber is <2.7%.

### Claim 2 (depends on 1)

The devulcanized rubber according to claim 1, comprising:
butadiene and/or styrene structural units.

### Claim 3 (depends on 1)

The devulcanized rubber according to claim 1, which contains 10-200 phr of silica.

### Claim 4 (depends on 1)

The devulcanized rubber according to claim 1, which has an NWB of >50%.

### Claim 5 (depends on 1)

The devulcanized rubber according to claim 1, which has an fsol of ≥12.0%.

### Claim 6 (depends on 1)

Process A process for producing the devulcanized rubber according to claim 1, comprising:
comminuting and reacting the vulcanized rubber with vinylsilane as devulcanizing agent at temperatures between 140-180° C. for 4 to 7 minutes with a concentration of devulcanizing agent of 4 to 6 wt %, based on the vulcanized rubber, and with an energy input during the reaction of >140 kNm.

### Claim 7 (depends on 6)

The process for producing the devulcanized rubber according to claim 6, comprising:
comminuting the vulcanized rubber by waterjet, cryogenic or ambient-mechanical milling.

### Claim 8 (depends on 6)

The process for producing the devulcanized rubber according to claim 6, comprising:
swelling, before adding the vinylsilane, the comminuted vulcanized rubber with oil.

### Claim 9 (depends on 6)

The process for producing the devulcanized rubber according to claim 6, wherein the vinylsilane comprises a vinyltrialkoxysilane.

### Claim 10 (depends on 6)

The process for producing the devulcanized rubber according to claim 6, comprising:
the vinylsilane in amounts of 1-20 wt %, based on the vulcanized rubber.

### Claim 11 (depends on 6)

The process for producing the devulcanized rubber according to claim 6, wherein the vinylsilane is used together with peroxides.

### Claim 12 (depends on 6)

The process for producing the devulcanized rubber according to claim 6, wherein peroxides comprise dicumyl peroxide and/or benzoyl peroxide.

### Claim 13 (depends on 6)

The process for producing the devulcanized rubber according to claim 6, comprising:
the peroxides in amounts of 1-20 wt %, based on the vinylsilane.

### Claim 14 (depends on 6)

The process for producing the devulcanized rubber according to claim 6, comprising:
comminuting vulcanized rubber from scrap tyres, and
swelling the comminuted rubber with oil, and
devulcanizing the comminuted rubber with vinyltriethoxysilane and dicumyl peroxide.

### Claim at position 15

15-16. (canceled)

### Claim 17 (depends on 1)

A vulcanized rubber mixture, comprising:
the devulcanized rubber according to claim 1.

### Claim 18 (depends on 1)

The devulcanized rubber according to claim 1, which contains 20-120 phr of silica.

### Claim 19 (depends on 6)

The process for producing the devulcanized rubber according to claim 6, wherein the vinylsilane comprises vinyltriethoxysilane.

### Claim 20 (depends on 6)

The process for producing the devulcanized rubber according to claim 6, comprising:
the vinylsilane in amounts of 3-10 wt %, based on the vulcanized rubber.

### Claim 21 (depends on 6)

The process for producing the devulcanized rubber according to claim 6, comprising:
the peroxides in amounts of 1-10 wt %, based on the vinylsilane.