# US 2026/0109638 A1 · Plasma-resistant glass, inner chamber component for semiconductor manufacturing process and methods for manufacturing glass and component

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0109638 A1
- Document ID: US20260109638A1
- Status: Published application
- Kind: A1
- Application number: 19/116,612
- Filed: 2023-08-18
- Published: 2026-04-23
- Earliest claimed: 2022-10-13
- Assignees: Hansol IONES Co., Ltd.
- Applicants: Hansol Iones Co., Ltd.
- Inventors: Seo Yeon JEON; Kyung Min LEE; Hye Won SEOK; Dae Gean KIM
- Web page: https://patentgrep.com/patent/US20260109638A1

## CPC

- C03C 3/085: containing an oxide of a divalent metal
- C03B 11/12: Cooling, heating, or insulating the plunger, the mould, or the glass-pressing machine; {cooling or heating of the glass in the mould}(C03B9/38 takes precedence)
- C03C 3/062: with less than 40% silica by weight
- C03C 4/0092: {for glass with improved high visible transmittance, e.g. extra-clear glass}
- C03C 15/00: Surface treatment of glass, not in the form of fibres or filaments, by etching (etching or surface-brightening compositions, in general C09K13/00)
- H01J 37/32: Gas-filled discharge tubes (heating by discharge H05B)
- H01J 37/32467: {Material}
- H10P 72/00: Handling or holding of wafers, substrates or devices during manufacture or treatment thereof
- C03C 2201/54: containing beryllium, magnesium or alkaline earth metals
- C03C 2203/10: Melting processes
- C03C 2203/52: Heat-treatment
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The present disclosure relates to plasma-resistant glass, an inner chamber component for a semiconductor manufacturing process, and methods for manufacturing the glass and the component, and specifically, to plasma-resistant glass, an inner chamber component for a semiconductor manufacturing process, and methods for manufacturing the glass and the component, wherein the contents of plasma-resistant glass components in the plasma-resistant glass are adjusted and SrO is added to achieve a lower melting temperature, the thermal expansion coefficient of the plasma-resistant glass is reduced to prevent damage from thermal shock during high-temperature use, and the plasma-resistant glass has improved light transmittance and durability.

## Claims

### Claim 1

Plasma-resistant glass formed by melting a composition including 30% by weight or greater and 80% by weight or less of SiO2, 5% by weight or greater and 35% by weight or less of Al2O3 and 10% by weight or greater and 50% by weight or less of SrO.

### Claim 2 (depends on 1)

The plasma-resistant glass of claim 1, wherein the composition includes only SiO2, Al2O3, SrO and inevitable impurities, the content of the SiO2 is 30% by weight or greater and 68% by weight or less, the content of the Al2O3 is 5% by weight or greater and 25% by weight or less, and the content of the SrO is 15% by weight or greater and 50% by weight or less.

### Claim 3 (depends on 1)

The plasma-resistant glass of claim 1, which has light transmittance of 80% or greater and 100% or less.

### Claim 4 (depends on 1)

The plasma-resistant glass of claim 1, which has Vickers hardness of 650 HV or greater and 1,000 HV or less.

### Claim 5 (depends on 1)

The plasma-resistant glass of claim 1, which has a glass transition temperature of 600° C. or higher and 850° C. or lower.

### Claim 6 (depends on 1)

The plasma-resistant glass of claim 1, which has a thermal expansion coefficient of 4.0×10−6 m/(m° C.) or greater and 6.0×10−6 m/(m° C.) or less.

### Claim 7 (depends on 1)

The plasma-resistant glass of claim 1, which has an etching rate by mixed plasma of fluorine and argon (Ar) of greater than 0 nm/min and 20 nm/min or less.

### Claim 8 (depends on 1)

The plasma-resistant glass of claim 1, which has a melting point of 1,500° C. or higher and 1,750° C. or lower.

### Claim 9 (depends on 1)

An inner chamber component for a semiconductor manufacturing process manufactured with the plasma-resistant glass of claim 1.

### Claim 10 (depends on 9)

The inner chamber component of claim 9, which is any one of a focus ring, an edge ring, a cover ring, a ring shower, an insulator, an EPD window, an electrode, a view port, an inner shutter, an electro static chuck, a heater, a chamber liner, a shower head, a boat for CVD (chemical vapor deposition), a wall liner, a shield, a cold pad, a source head, an outer liner, a deposition shield, an upper liner, an exhaust plate and a mask frame.

### Claim 11

A method for manufacturing plasma-resistant glass, the method comprising:
melting a composition including 30% by weight or greater and 80% by weight or less of SiO2, 5% by weight or greater and 35% by weight or less of Al2O3 and 10% by weight or greater and 50% by weight or less of SrO; and
cooling the melted composition.

### Claim 12 (depends on 11)

The method of claim 11, wherein a melting temperature in the melting of a composition is 1,400° C. or higher and 1,700° C. or lower.

### Claim 13 (depends on 1)

A method for manufacturing an inner chamber component for a semiconductor manufacturing process, the method comprising:
melting the plasma-resistant glass of claim 1;
injecting the melted plasma-resistant glass into a mold; and
annealing the injected plasma-resistant glass.

### Claim 14 (depends on 13)

The method of claim 13, wherein a melting temperature in the melting of the plasma-resistant glass is 1,500° C. or higher and 1,750° C. or lower.

### Claim 15 (depends on 13)

The method of claim 13, wherein a temperature in the annealing is 400° C. or higher and 900° C. or lower.