# US 2026/0108964 A1 · Brazed lap joint, method for manufacturing brazed lap joint, and vehicle component

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0108964 A1
- Document ID: US20260108964A1
- Status: Published application
- Kind: A1
- Application number: 19/117,602
- Filed: 2023-12-15
- Published: 2026-04-23
- Earliest claimed: 2022-12-23
- Assignees: Nippon Steel Corporation
- Applicants: Nippon Steel Corporation
- Inventors: Seiji FURUSAKO; Shinji KODAMA; Yoshinari ISHIDA; Masahiro MATSUBA
- Web page: https://patentgrep.com/patent/US20260108964A1

## CPC

- B23K 1/19: taking account of the properties of the materials to be soldered
- B23K 9/173: and of a consumable electrode
- B23K 35/0227: {Rods or wires (B23K35/0244 takes precedence)}
- B23K 35/302: {Cu as the principal constituent}
- B32B 15/013: {one layer being formed of an iron alloy or steel, another layer being formed of a metal other than iron or aluminium}
- C22C 9/00: Alloys based on copper
- C22C 9/01: with aluminium as the next major constituent
- B23K 2101/006: {Vehicles}
- B23K 2101/34: Coated articles {; Surface treated articles}
- B23K 2103/04: Steel {or steel} alloys
- C22C 9/05: with manganese as the next major constituent
- C22C 9/10: with silicon as the next major constituent
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A brazed lap joint according to an aspect of the present invention includes: a first steel sheet and a second steel sheet, the first steel sheet and the second steel sheet being stacked; a zinc-based-plated layer, the zinc-based-plated layer being an overlapping surface of the first steel sheet and the second steel sheet; and a brazed zone including a brazing metal joining an end surface of the first steel sheet and a surface of the second steel sheet, and a heat-affected zone around the brazing metal, in which a concentration of B atoms at a prior austenite grain boundary of the second steel sheet excluding the brazed zone is 2.0 atm % or more, an average effective grain size of the second steel sheet excluding the brazed zone is 7.0 μm or less, an average effective grain size of the second steel sheet in a root portion, a toe portion, and a middle portion between the root portion and the toe portion is 15.0 μm or less, a Vickers hardness of the brazing metal is 250 or less, and a leg length of the brazed lap joint on the second steel sheet side is 2.0 mm or more.

## Claims

### Claim 1

A brazed lap joint comprising:
a first steel sheet and a second steel sheet, the first steel sheet and the second steel sheet being stacked;
a zinc-based-plated layer, the zinc-based-plated layer being an overlapping surface of the first steel sheet and the second steel sheet; and
a brazed zone including a brazing metal joining an end surface of the first steel sheet and a surface of the second steel sheet, and a heat-affected zone around the brazing metal, wherein
a concentration of B atoms at a prior austenite grain boundary of the second steel sheet excluding the brazed zone is 2.0 atm % or more,
an average effective grain size of the second steel sheet excluding the brazed zone is 7.0 μm or less,
an average effective grain size of the second steel sheet in a root portion, a toe portion, and a middle portion between the root portion and the toe portion is 15.0 μm or less,
a Vickers hardness of the brazing metal is 250 or less, and
a leg length of the brazed lap joint on the second steel sheet side is 2.0 mm or more.

### Claim 2 (depends on 1)

The brazed lap joint according to claim 1, wherein
a tensile strength of the second steel sheet is 980 MPa or more.

### Claim 3

A method for manufacturing a brazed lap joint in which a zinc-based-plated layer is present on an overlapping surface and an end surface of a first steel sheet and a surface of a second steel sheet are brazed, the method comprising:
bringing a metal platen whose inside is cooled by cooling water into close contact with the second steel sheet; and
performing brazing using, as a filler metal, a brazing wire containing Cu as a main component and having a diameter of 0.8 to 1.4 mm, so that an amount of brazing heat input Q calculated by the following formula becomes 190 to 270 J/mm:
Q
=
V
×
I
/
v
where V is a voltage in units of V, I is a current in units of A, and v is a brazing rate in units of mm/s,
wherein a concentration of B atoms at a prior austenite grain boundary of the second steel sheet is 2.0 atm % or more, and an average effective grain size of the second steel sheet is 7.0 μm or less.

### Claim 4 (depends on 3)

The method for manufacturing a brazed lap joint according to claim 3, wherein
a tensile strength of the second steel sheet is 980 MPa or more.

### Claim 5 (depends on 3)

The method for manufacturing a brazed lap joint according to claim 3, wherein
the brazing is MIG brazing.

### Claim 6 (depends on 1)

A vehicle component comprising the brazed lap joint according to claim 1.