# US 2026/0108913 A1 · Non-dichroic thin film coatings

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0108913 A1
- Document ID: US20260108913A1
- Status: Published application
- Kind: A1
- Application number: 18/924,046
- Filed: 2024-10-23
- Published: 2026-04-23
- Earliest claimed: 2024-10-23
- Assignees: Lockheed Martin Corporation
- Applicants: Lockheed Martin Corporation
- Inventors: Kevie Overton Dowhower; Thomas Joseph Ives
- Web page: https://patentgrep.com/patent/US20260108913A1

## CPC

- B05D 5/065: {having colour interferences or colour shifts or opalescent looking, flip-flop, two tones}
- G02B 5/0833: {comprising inorganic materials only}
- B05D 1/62: {Plasma-deposition of organic layers (plasma deposition in general C23C14/00, C23C16/00)}
- C23C 14/0652: {Silicon nitride}
- C23C 14/542: {Controlling the film thickness or evaporation rate}
- C23C 14/548: {Controlling the composition}
- C23C 16/345: {Silicon nitride}
- C23C 16/52: Controlling or regulating the coating process {(C23C16/45557, C23C16/279 take precedence)}
- G02B 5/285: {comprising deposited thin solid films (G02B5/281 - G02B5/289 take precedence; multilayered film filters for fibre optic multiplexing G02B6/29361)}
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A non-dichroic coating thin film structure, consisting of a Bragg-reflector structure and a graded index layer, is deposited on a substrate. The Bragg-reflector structure includes several pairs of layers: each pair has a first layer of a first material with a first refractive index and a quarter-wavelength thickness determined by a target wavelength, positioned adjacent to a second layer of a second material with a second refractive index, having a quarter-wavelength thickness. The first refractive index is at least 0.5 higher than that of the second. Over the Bragg-reflector structure, a graded index layer with a continuously changing refractive index is deposited, transitioning from a third refractive index to the first refractive index. The thickness of the graded index layer is selected such that the reflection coefficient for light in the visible spectrum of 400-700 nanometers varies by no more than 25 percent for this wavelength range.

## Claims

### Claim 1

A non-dichroic coating thin film structure deposited over a substrate, the non-dichroic coating thin film structure comprising:
a Bragg-reflector structure deposited over the substrate and having a plurality of pairs of layers, each pair having a first layer and a second layer;
the first layer comprising a first material of a first refractive index and having a first thickness of a quarter of a target wavelength determined within the first layer, the first layer positioned adjacent to the second layer;
the second layer comprising a second material of a second refractive index and having a second thickness of the quarter of the target wavelength determined within the second layer, wherein the first refractive index is at least 0.5 higher than the second refractive index; and
a graded index layer of a continuously changing graded refractive index deposited over the Bragg-reflector structure, wherein the graded refractive index changes continuously from a third refractive index to the first refractive index, and wherein a thickness of the graded index layer is selected such that a reflection coefficient for a light of a visible wavelength varies by no more than 25 percent for a visible wavelength range of 400-700 nanometers.

### Claim 2 (depends on 1)

The non-dichroic coating thin film structure of claim 1, wherein the target wavelength is determined based on a color of the substrate.

### Claim 3 (depends on 2)

The non-dichroic coating thin film structure of claim 2, wherein the target wavelength corresponds to a color that is complementary to the color of the substrate.

### Claim 4 (depends on 1)

The non-dichroic coating thin film structure of claim 1, wherein the first refractive index is in a range between 2.5 and 3.5.

### Claim 5 (depends on 1)

The non-dichroic coating thin film structure of claim 1, wherein the second refractive index is in a range between 1.5 and 2.5.

### Claim 6 (depends on 1)

The non-dichroic coating thin film structure of claim 1, wherein the third refractive index is in a range between 1.5 and 2.5.

### Claim 7 (depends on 1)

The non-dichroic coating thin film structure of claim 1, wherein the graded index layer is selected from a composite material comprising variable molar fractions of silicon and nitrogen.

### Claim 8 (depends on 1)

The non-dichroic coating thin film structure of claim 1, wherein the graded index layer comprises a silicon nitride layer is deposited using a chemical vapor deposition, and wherein variable molar fractions of silicon and nitrogen are determined by a mass flow rate of silane and ammonia gases.

### Claim 9 (depends on 8)

The non-dichroic coating thin film structure of claim 8, wherein the chemical vapor deposition is plasma enhanced to reduce a substrate temperature to a few hundred degrees of Celsius.

### Claim 10 (depends on 1)

The non-dichroic coating thin film structure of claim 1, wherein the thickness of the Bragg-reflector structure is about one and a half micron and wherein the thickness of the graded index layer is further determined based on a reflectivity requirement of the non-dichroic coating thin film structure.

### Claim 11 (depends on 1)

The non-dichroic coating thin film structure of claim 1, having a reflectivity of more than ten percent.

### Claim 12 (depends on 1)

The non-dichroic coating thin film structure of claim 1, wherein the graded refractive index has a linear profile.

### Claim 13 (depends on 1)

The non-dichroic coating thin film structure of claim 1, wherein the Bragg-reflector layer is a first Bragg-reflector layer, the non-dichroic coating thin film structure further comprising a second Bragg-reflector layer deposited between the substrate and the first Bragg-reflector layer, the second Bragg-reflector layer configured to reflect a light at a second target wavelength that is different than the target wavelength of the first Bragg-reflector layer by at least a hundred of nanometers.

### Claim 14 (depends on 1)

The non-dichroic coating thin film structure of claim 1, wherein a composition of the graded index layer is selected such that it is about fifty percent reflective at the thickness of about 0.1 microns.

### Claim 15

A system for depositing a non-dichroic coating thin film, the system comprising a control system having a processor for executing instructions that cause, the control system to transmit signals to operate mass flow controllers for a deposition of precursor gases, and for maintaining a temperature and pressure control within a reaction chamber, the instructions causing the processor to perform operations comprising:
receiving optical properties of a substrate including a color of the substrate obtained from spectrophotometer measurements;
receiving a reflectance requirement for the substrate;
based on the received optical properties and the reflectance requirement, selecting a formula for the deposition of the non-dichroic coating thin film over the substrate, wherein the selecting of the formula comprises determining a set of parameters for the non-dichroic coating thin film, the non-dichroic coating thin film comprising:
a Bragg-reflector structure deposited over the substrate and having a plurality of pairs of layers, each pair having a first layer and a second layer;
the first layer comprising a first material of a first refractive index and having a first thickness of a quarter of a target wavelength determined within the first layer, the first layer adjacent to the second layer;
the second layer comprising a second material of a second refractive index and having a second thickness of the quarter of the target wavelength determined within the second layer, wherein the first refractive index is at least 0.5 higher than the second refractive index;
a graded index layer of a continuously changing graded refractive index deposited over the Bragg-reflector structure, wherein the graded refractive index changes continuously from a third refractive index to the first refractive index; and
wherein the determining the set of parameters comprises:
determining the target wavelength; and
determining a thickness of the graded index layer.

### Claim 16 (depends on 15)

The system of claim 15, wherein the determining the set of parameters further comprises determining the first and the second material.

### Claim 17 (depends on 15)

The system of claim 15, wherein the determining the set of parameters comprises determining a third material having the third refractive index and determining a grading profile for the graded index layer.

### Claim 18 (depends on 15)

The system of claim 15, wherein the determining the set of parameters includes determining time dependent mass flow rates for releasing the precursor gases and selecting time dependent pressure and temperature for the reaction chamber.

### Claim 19 (depends on 15)

The system of claim 15, wherein the determining the set of parameters includes determining a time duration for the deposition of the precursor gases.

### Claim 20 (depends on 15)

The system of claim 15, wherein the reflectance requirement comprises required ranges for a reflectance coefficient for a set of wavelengths in a range of 400 to 700 nanometers.

### Claim 21 (depends on 15)

The system of claim 15, wherein the optical properties of the substrate comprise reflectance of the substrate to visible light in a range of 400 to 700 nanometers and scattering of the visible light from the substrate.