# US 2026/0107745 A1 · Method of forming a thin film using hydrogen treatment

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0107745 A1
- Document ID: US20260107745A1
- Status: Published application
- Kind: A1
- Application number: 19/351,418
- Filed: 2025-10-07
- Published: 2026-04-16
- Earliest claimed: 2024-10-10
- Assignees: ASM IP Holding B.V.
- Applicants: ASM IP Holding B.V.
- Inventors: Estiaque Haidar Shourov; Balaji Kannan; Jian-Wei Liang; Mojtaba Samiee; Madhan Kumar Arulanandam; Ali Al janabi; Wei Li
- Web page: https://patentgrep.com/patent/US20260107745A1

## CPC

- H10P 95/00: Generic processes or apparatus for manufacture or treatments not covered by the other groups of this subclass
- C23C 16/34: Nitrides {(C23C16/303 takes precedence)}
- C23C 16/45525: {Atomic layer deposition [ALD]}
- C23C 16/56: After-treatment
- H10P 14/412: {Deposition of metallic or metal-silicide materials}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A substrate processing method for forming a thin film includes providing or forming a transition metal nitride film on a substrate in a reaction chamber and exposing the transition metal nitride film to a hydrogen treatment to form a treated transition metal compound film. The hydrogen treatment may lower the resistivity of the transition metal nitride film and/or be used to desirably tune other properties and/or composition of the transition metal nitride film.

## Claims

### Claim 1

A method of forming a thin film comprising:
providing a substrate in a reaction chamber;
depositing a transition metal nitride film on the substrate, wherein the depositing the transition metal nitride film comprises:
pulsing a transition metal precursor, wherein the transition metal precursor comprises a metalorganic precursor comprising at least one amido group, and
pulsing a nitrogen reactant; and
exposing the transition metal nitride film to a hydrogen treatment form a treated transition metal compound film, wherein the treated transition metal compound film comprises less nitrogen than the transition metal nitride film,
wherein a pressure during the exposing the transition metal nitride film to the hydrogen treatment is less than about 200 Torr, and
wherein a temperature within the reaction chamber during the exposing the transition metal nitride film to the hydrogen treatment is from about 300 °C to about 550 °C.

### Claim 2 (depends on 1)

The method of claim 1, wherein the transition metal nitride film comprises molybdenum.

### Claim 3 (depends on 1)

The method of claim 1, wherein the exposing the transition metal nitride film to the hydrogen treatment comprises exposing transition metal nitride to H2.

### Claim 4 (depends on 1)

The method of claim 1, wherein the exposing the transition metal nitride film to the hydrogen treatment is a thermal process.

### Claim 5 (depends on 1)

The method of claim 1, wherein a pressure during the exposing the transition metal nitride film to the hydrogen treatment is from about 100 Torr to about 200 Torr.

### Claim 6 (depends on 1)

The method of claim 1, wherein the treated transition metal compound film is represented by the formula MxNyCzOw, where M is one or more transition metals; x is between about 0.75 to about 1.25, y is between about 0.15 to about 0.35, z is between about 0.6 to about 0.8, and w is between about 0.4 to 0.6.

### Claim 7 (depends on 1)

The method of claim 1, wherein a temperature during the exposing the transition metal nitride film to the hydrogen treatment is from about 400 °C to about 525 °C.

### Claim 8 (depends on 1)

The method of claim 1, wherein the exposing the transition metal nitride film to the hydrogen treatment comprises exposing the transition metal nitride film to hydrogen for about 0.1 minutes to about 40 minutes.

### Claim 9 (depends on 1)

The method of claim 1, wherein the depositing the transition metal nitride film comprises an atomic layer deposition (ALD) process.

### Claim 10 (depends on 1)

The method of claim 1, wherein the depositing the transition metal nitride film comprises repeating the pulsing the transition metal precursor and the pulsing the nitrogen reactant until the transition metal nitride film reaches a predetermined thickness.

### Claim 11 (depends on 1)

The method of claim 1, wherein the transition metal nitride film has a thickness less than about 100 Angstroms.

### Claim 12

A method of forming a thin film comprising:
providing a substrate in a reaction chamber;
depositing a transition metal nitride film on the substrate, wherein the transition metal nitride film comprises a transition metal, oxygen, carbon, and nitrogen, wherein the transition metal nitride film has a resistivity from about 2600 μΩ cm to about 4000 μΩ cm; and
exposing the transition metal nitride film to a hydrogen treatment to form a treated transition metal compound film, wherein the treated transition metal compound film has a resistivity from about 300 μΩ cm to about 600 μΩ cm,
wherein the treated transition metal compound film comprises substantially the same amount of the transition metal, oxygen, and carbon as the transition metal nitride film.

### Claim 13 (depends on 12)

The method of claim 12, wherein the transition metal nitride film comprises an atomic percentage of nitrogen between about 20 at % and about 40 at%.

### Claim 14 (depends on 13)

The method of claim 13, wherein the treated transition metal compound film comprises an atomic percentage of nitrogen between about 5 at % and about 30 at%.

### Claim 15 (depends on 12)

The method of claim 12, wherein the transition metal nitride film comprises an atomic percentage of carbon between about 15 at % and about 35 at %.

### Claim 16 (depends on 12)

The method of claim 12, wherein a ratio between the transition metal and carbon in the transition metal nitride film is within about 10% of a ratio between transition metal and carbon in the treated transition metal compound film.

### Claim 17 (depends on 12)

The method of claim 12, wherein the exposing the transition metal nitride film to the hydrogen treatment lowers the number of C═C bonds in the transition metal nitride film.

### Claim 18 (depends on 12)

The method of claim 12, wherein the exposing the transition metal nitride film to the hydrogen treatment at least partially overlaps with the depositing the transition metal nitride film.

### Claim 19 (depends on 12)

The method of claim 12, wherein the transition metal nitride film has a thickness less than about 100 Angstroms.

### Claim 20 (depends on 12)

The method of claim 12, wherein the depositing the transition metal nitride film comprises:
pulsing a transition metal precursor, wherein the transition metal precursor comprises a metalorganic precursor, and
pulsing a nitrogen reactant.