# US 2026/0107674 A1 · Organic photovoltaic materials, devices, and methods

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0107674 A1
- Document ID: US20260107674A1
- Status: Published application
- Kind: A1
- Application number: 19/340,355
- Filed: 2025-09-25
- Published: 2026-04-16
- Earliest claimed: 2022-08-22
- Assignees: The Florida State University Research Foundation, Inc.
- Applicants: Florida State University Research Foundation, Inc.
- Inventors: Vincent O. Eze; Okenwa Okoli
- Web page: https://patentgrep.com/patent/US20260107674A1

## CPC

- H10K 85/113: {Heteroaromatic compounds comprising sulfur or selene, e.g. polythiophene}
- H10K 85/215: {comprising substituents, e.g. PCBM}
- H10K 85/626: {containing more than one polycyclic condensed aromatic rings, e.g. bis-anthracene}
- H10K 85/657: {Polycyclic condensed heteroaromatic hydrocarbons}
- H10K 30/30: comprising bulk heterojunctions, e.g. interpenetrating networks of donor and acceptor material domains
- H10K 30/50: Photovoltaic [PV] devices
- H10K 71/12: using liquid deposition, e.g. spin coating
- Y02E 10/549: Organic PV cells
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Organic photovoltaic materials (OPV) and devices using the same are provided, as well as methods of fabricating and using the same. An OPV material can be used as a photo-absorbing layer for mechanoluminescent (ML) light (e.g., in a flexible organic ML photodiode). The OPV material can include, for example, a blend of a donor polymer (e.g., P3HT) and a non-halogenated, non-fullerene acceptor (e.g., Y6).

## Claims

### Claim 1

A pressure sensor, comprising:
an organic photovoltaic (OPV) layer comprising a composite material;
a first electrode disposed on the OPV layer;
a charge transport layer disposed under the OPV layer;
a second electrode disposed under the charge transport layer; and
a mechanoluminescent (ML) layer comprising an ML material and configured to emit light to be absorbed by the OPV layer upon application of stress to the ML layer,
wherein the layer comprising the ML material is disposed on at least one of the first electrode, the OPV layer, the charge transport layer, and the second electrode,
wherein the composite material comprises:
a donor polymer; and
a non-fullerene acceptor, and
wherein the donor polymer is poly(3-hexylthiophene-2,5-diyl (P3HT).

### Claim 2 (depends on 1)

The pressure sensor according to claim 1, wherein the non-fullerene acceptor is (2,2′-((2Z,2′Z)-((12,13-bis(2-ethylhexyl)-3,9-diundecyl-12,13-dihydro-[1,2,5]thiadiazolo[3,4-e]thieno[2,″3″:4′,5′]thieno[2′,3′:4,5]pyrrolo[3,2-g]thieno[2′,3′:4,5]thieno[3,2]indole-2,10-diyl)bis(methanylylidene))bis(5,6-difluoro-3-oxo-2,3-dihydro-1H-indene-2,1-diylidene)) dimalononitile) (Y6).

### Claim 3 (depends on 2)

The pressure sensor according to claim 2, wherein a weight ratio of donor polymer to non-fullerene acceptor is in a range of from 0.5:1 to 1.5:1.

### Claim 4 (depends on 3)

The pressure sensor according to claim 3, wherein the weight ratio of donor polymer to non-fullerene acceptor is about 1:1.

### Claim 5 (depends on 3)

The pressure sensor according to claim 3, wherein the donor polymer is dispersed in the non-fullerene acceptor, or the non-fullerene acceptor is dispersed in the donor polymer.

### Claim 6 (depends on 1)

The pressure sensor according to claim 1, wherein a weight ratio of donor polymer to non-fullerene acceptor is in a range of from 0.5:1 to 1.5:1.

### Claim 7 (depends on 1)

The pressure sensor according to claim 1, wherein the OPV layer is disposed between the charge transport layer and the first electrode, and
wherein the charge transport layer is disposed between the second electrode and the OPV layer.

### Claim 8 (depends on 1)

The pressure sensor according to claim 1, wherein the non-fullerene acceptor is a non-halogenated non-fullerene acceptor.

### Claim 9 (depends on 1)

The pressure sensor according to claim 1, wherein the weight ratio of donor polymer to non-fullerene acceptor is about 1:1.

### Claim 10 (depends on 1)

The pressure sensor according to claim 1, wherein the donor polymer is substantially evenly dispersed in the fullerene acceptor, or the non-fullerene acceptor is substantially evenly dispersed in the donor polymer.

### Claim 11 (depends on 1)

The pressure sensor according to claim 1, wherein the composite material is in the form of a flexible film.

### Claim 12 (depends on 1)

The pressure sensor according to claim 1, further comprising a substrate on which the second electrode is disposed,
wherein the second electrode is disposed between the substrate and the charge transport layer.

### Claim 13 (depends on 1)

The pressure sensor according to claim 1, wherein the second electrode comprises indium tin oxide,
wherein the charge transport layer comprises SnO2, and
wherein the first electrode comprises silver (Ag), gold (Au), or a combination thereof.

### Claim 14 (depends on 1)

The pressure sensor according to claim 1, wherein the second electrode is in direct physical contact with the charge transport layer,
wherein the charge transport layer is in direct physical contact with the OPV layer, and
wherein the OPV layer is in direct physical contact with the first electrode.

### Claim 15 (depends on 10)

The pressure sensor according to claim 10, wherein the pressure sensor is flexible.

### Claim 16 (depends on 10)

The pressure sensor according to claim 10, wherein the non-fullerene acceptor is Y6,
wherein the OPV exhibits a rectification ratio in a range of from 3.6×103 to 4×103, and
wherein the pressure sensor has a response time of 100 milliseconds (ms) or less when exposed to a 470 nanometer (nm) light pulse.

### Claim 17 (depends on 1)

The pressure sensor according to claim 1, wherein the ML layer comprises zinc sulfide (ZnS) and copper (Cu).

### Claim 18

A method of fabricating a pressure sensor, the method comprising:
providing a mixture comprising a liquid, a donor polymer, and a non-fullerene acceptor;
disposing the mixture on a charge transport layer;
removing at least a portion of the liquid from the mixture to form an organic photovoltaic (OPV) layer on the charge transport layer;
disposing a first electrode on the OPV layer;
disposing a second electrode on the charge transport layer; and
providing a mechanoluminescent (ML) layer comprising an ML material and configured to emit light to be absorbed by the OPV layer upon application of stress to the ML layer,
wherein the ML layer is disposed on at least one of the first electrode, the OPV layer, the charge transport layer, and the second electrode, and
wherein the donor polymer is poly(3-hexylthiophene-2,5-diyl (P3HT).

### Claim 19 (depends on 18)

The method according to claim 18, wherein the liquid is a polar organic solvent,
wherein the disposing of the mixture on the charge transport layer comprises spin-coating the mixture on the surface,
wherein the removing of the at least a portion of the liquid comprises annealing the mixture,
wherein the non-fullerene acceptor is (2,2′-((2Z,2′Z)-((12,13-bis(2-ethylhexyl)-3,9-diundecyl-12,13-dihydro-[1,2,5]thiadiazolo[3,4-e]thieno[2,″3″:4′,5′]thieno[2′,3′:4,5]pyrrolo[3,2-g]thieno[2′,3′:4,5]thieno[3,2]indole-2,10-diyl)bis(methanylylidene))bis(5,6-difluoro-3-oxo-2,3-dihydro-1H-indene-2,1-diylidene)) dimalononitile) (Y6),
wherein a weight ratio of donor polymer to non-fullerene acceptor is in a range of from 0.5:1 to 1.5:1,
wherein the donor polymer is dispersed in the non-fullerene acceptor, or the non-fullerene acceptor is dispersed in the donor polymer,
wherein the OPV layer is disposed between the charge transport layer and the first electrode, and
wherein the charge transport layer is disposed between the second electrode and the OPV layer.

### Claim 20 (depends on 19)

The method according to claim 19, wherein the weight ratio of donor polymer to non-fullerene acceptor is about 1:1,
wherein the second electrode comprises indium tin oxide,
wherein the charge transport layer comprises SnO2,
wherein the first electrode comprises silver (Ag), gold (Au), or a combination thereof,
wherein the second electrode is in direct physical contact with the charge transport layer,
wherein the charge transport layer is in direct physical contact with the OPV layer,
wherein the OPV layer is in direct physical contact with the first electrode,
wherein the pressure sensor is flexible,
wherein the OPV exhibits a rectification ratio in a range of from 3.6×103 to 4×103,
wherein the pressure sensor has a response time of 100 milliseconds (ms) or less when exposed to a 470 nanometer (nm) light pulse, and
wherein the ML layer comprises zinc sulfide (ZnS) and copper (Cu).