# US 2026/0106214 A1 · Sulfide solid electrolyte, method of preparing the same and application

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0106214 A1
- Document ID: US20260106214A1
- Status: Published application
- Kind: A1
- Application number: 19/305,671
- Filed: 2025-08-20
- Published: 2026-04-16
- Earliest claimed: 2024-10-11
- Assignees: AESC Japan Ltd.
- Applicants: AESC Japan Ltd.
- Inventors: Le Yu; Ming Wu; Qian Li; Wenbin Lyu
- Web page: https://patentgrep.com/patent/US20260106214A1

## CPC

- H01M 10/0562: Solid materials
- C01B 25/455: containing halogen {(completely halogenated alkali metal phosphates C01D, e.g. lithium hexafluorophosphate C01D15/005)}
- C01D 15/00: Lithium compounds
- C01G 15/006: {Compounds containing gallium, indium or thallium, with or without oxygen or hydrogen, and containing two or more other elements}
- C01G 29/006: {Compounds containing bismuth, with or without oxygen or hydrogen, and containing two or more other elements}
- C01G 30/023: {of ammonium, alkali or alkaline-earth metals or magnesium}
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2002/52: containing elements as dopants
- C01P 2002/54: one element only
- C01P 2004/03: obtained by SEM
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2006/40: Electric properties
- H01M 2300/0068: inorganic
- H01M 2300/008: Halides
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01D: COMPOUNDS OF ALKALI METALS, i.e. LITHIUM, SODIUM, POTASSIUM, RUBIDIUM, CAESIUM, OR FRANCIUM (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides C01B17/22; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia and cyanogen, containing nitrogen and other non-metals C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; phosphides C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A sulfide solid electrolyte, a method of preparing the same, and an application are provided. The sulfide solid electrolyte has a molecular formula of LiaP1-bMbScOdXe, where 5<a<6, 0<b<1, 1.5<c<5, 0<d<2.5, 4<c+d<5, 1<e<2, M is selected from one or more of Al, Ga, In, Ti, Sc, As, Sb, Bi, V, or Nb, and X is selected from one or more of Cl, Br, or I. Through the sulfide solid electrolyte, the method of preparing the same, and the application provided by the disclosure, the stability of ionic conductivity of the sulfide solid electrolyte is increased, the air stability is enhanced, and the electrolyte/active material interface properties are improved, so that the service life and safety of an all-solid-state lithium-ion battery are increased.

## Claims

### Claim 1

A sulfide solid electrolyte, having a molecular formula of LiaP1-bMbScOdXe, wherein 5<a<6, 0<b<1, 1.5<c<5, 0<d<2.5, 4<c+d<5, 1<e<2, M is selected from one or more of Al, Ga, In, Ti, Sc, As, Sb, Bi, V, or Nb, and X is selected from one or more of Cl, Br, or I.

### Claim 2 (depends on 1)

The sulfide solid electrolyte according to claim 1, wherein M is selected from one or more of Sb, In, or Bi.

### Claim 3 (depends on 1)

The sulfide solid electrolyte according to claim 1, wherein X is selected from Cl, and a value range of b is 0<b≤0.1.

### Claim 4 (depends on 1)

A method of preparing the sulfide solid electrolyte according to claim 1, comprising:
according to a chemical formula of the sulfide solid electrolyte, mixing a Li source, a P source, a M source, a S source, and a X source according to a stoichiometric ratio, placing the mixture in a ball mill jar for ball milling to obtain sulfide solid electrolyte precursor powder; and
calcining the sulfide solid electrolyte precursor powder at a predetermined temperature to obtain the sulfide solid electrolyte.

### Claim 5 (depends on 4)

The method of preparing the sulfide solid electrolyte according to claim 4, wherein the Li source is selected from one or more of LiCl, LiBr, LiI, or Li2S, the P source is selected from one or more of elemental P, P2S5, P4S6, PCl5, or PBr5, the M source is selected from one or more of oxide of M or sulfide of M, the S source is selected from one or more of elemental S, Li2S, P2S5, P4S6, As2S5, As2S3, Sb2S5, Sb2S3, Bi2S5, Bi2S3, Al2S3, Ga2S3, In2S3, or Sc2S3, the X source is selected from one or more of LiCl, PCl5, LiBr, PBr5, LiI, or I2, and the O element in the chemical formula is derived from the oxide of M.

### Claim 6 (depends on 4)

The method of preparing the sulfide solid electrolyte according to claim 4, wherein ball milling time is 1 h to 48 h, a ball milling rotation speed is 50 rpm to 1,500 rpm, and a ball-to-material ratio is 1:1 to 100:1.

### Claim 7 (depends on 4)

The method of preparing the sulfide solid electrolyte according to claim 4, wherein the predetermined temperature is 400° C. to 600° C., and time of the calcining treatment is 1 h to 18 h.

### Claim 8 (depends on 1)

An all-solid-state lithium-ion battery, at least comprising:
a positive electrode sheet comprising a halide solid electrolyte comprising Li2.35Zr0.65Fe0.35Cl5Br0.5I0.5;
a negative electrode sheet; and
a solid electrolyte membrane disposed between the adjacent positive electrode sheet and negative electrode sheet, wherein the solid electrolyte membrane comprises the sulfide solid electrolyte according to claim 1.

### Claim 9 (depends on 8)

The all-solid-state lithium-ion battery according to claim 8, wherein the positive electrode sheet comprises a positive active material selected from one or more of lithium nickel cobalt manganese oxide, lithium nickel oxide, lithium manganese oxide, lithium nickel manganese oxide, lithium cobalt oxide, or lithium nickel cobalt aluminum oxide.

### Claim 10 (depends on 8)

A electronic apparatus, comprising the all-solid-state lithium-ion battery according to claim 8.