# US 2026/0103839 A1 · Method For Producing Transfer Medium And Transfer Recording Method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0103839 A1
- Document ID: US20260103839A1
- Status: Published application
- Kind: A1
- Application number: 19/353,937
- Filed: 2025-10-09
- Published: 2026-04-16
- Earliest claimed: 2024-10-10
- Assignees: Seiko Epson Corporation
- Applicants: Seiko Epson Corporation
- Inventors: Takayoshi KAGATA; Kunihiro FUJITA; Haruka SATO
- Web page: https://patentgrep.com/patent/US20260103839A1

## CPC

- D06P 5/003: {Transfer printing}
- D06P 3/24: Polyamides; Polyurethanes
- D06P 3/32: leather {skins}
- D06P 3/52: Polyesters
- D06P 3/60: Natural or regenerated cellulose
- D06P 3/8223: {mixtures of fibres containing hydroxyl and ester groups}
- D06P 5/30: Ink jet printing
- D06P: DYEING OR PRINTING TEXTILES; DYEING LEATHER, FURS OR SOLID MACROMOLECULAR SUBSTANCES IN ANY FORM

## Abstract

A method for producing a transfer medium according to the present disclosure includes: forming a first layer by adhering an image forming ink to a transfer sheet; and forming a second layer by adhering an adhesive ink on top of the first layer. The transfer sheet includes a substrate and an ink receiving layer containing resin. The ink receiving layer has a thickness of 7 μm or more. A total amount of adhesion of the image forming ink and the adhesive ink per unit area of the transfer sheet is 110 g/m2 or more.

## Claims

### Claim 1

A method for producing a transfer medium comprising:
forming a first layer by adhering an image forming ink to a transfer sheet; and
forming a second layer by adhering an adhesive ink on top of the first layer, wherein
the transfer sheet includes a substrate and an ink receiving layer containing resin,
the ink receiving layer has a thickness of 7 μm or more, and
a total amount of adhesion of the image forming ink and the adhesive ink per unit area of the transfer sheet is 110 g/m2 or more.

### Claim 2 (depends on 1)

The method for producing a transfer medium according to claim 1, wherein the ink receiving layer further contains an inorganic oxide particle.

### Claim 3 (depends on 2)

The method for producing a transfer medium according to claim 2, wherein the inorganic oxide particle has a maximum particle diameter of 5 μm or more.

### Claim 4 (depends on 2)

The method for producing a transfer medium according to claim 2, wherein the ink receiving layer contains, as the resin, at least one selected from the group consisting of acrylic resin, vinyl acetate resin, and urethane resin.

### Claim 5 (depends on 1)

The method for producing a transfer medium according to claim 1, wherein, the forming the first layer uses a color ink and a white ink as the image forming ink, and
the white ink is adhered on top of the color ink on at least a portion of the transfer sheet.

### Claim 6 (depends on 1)

The method for producing a transfer medium according to claim 1, further comprising drying the transfer sheet by heating the transfer sheet having the first layer and the second layer to 100° C. or more.

### Claim 7 (depends on 1)

The method for producing a transfer medium according to claim 1, wherein an amount of adhesion of the image forming ink per unit area of the transfer sheet is 30 g/m2 or more and 200 g/m2 or less.

### Claim 8 (depends on 1)

The method for producing a transfer medium according to claim 1, wherein an amount of adhesion of the adhesive ink per unit area of the transfer sheet is 30 g/m2 or more and 500 g/m2 or less.

### Claim 9 (depends on 1)

A transfer recording method comprising thermally transferring the ink receiving layer, the first layer, and the second layer included in the transfer medium produced by the method for producing a transfer medium according to claim 1 onto a transfer target medium.

### Claim 10

A transfer recording method comprising:
forming a first layer by adhering an image forming ink to a transfer sheet including a substrate and an ink receiving layer containing resin and an inorganic oxide particle having a maximum particle diameter of 5 μm or more;
forming a second layer by adhering an adhesive ink on top of the first layer;
drying the transfer sheet by heating the transfer sheet having the first layer and the second layer to 100° C. or more; and
thermally transferring the ink receiving layer, the first layer, and the second layer included in the transfer medium produced through the forming the first layer, the forming the second layer, and the drying, onto a transfer target medium, wherein
the ink receiving layer contains, as the resin, at least one selected from the group consisting of acrylic resin, vinyl acetate resin, and urethane resin,
the ink receiving layer has a thickness of 7 μm or more, and
the forming the first layer uses a color ink and a white ink as the image forming ink,
the white ink is adhered on top of the color ink on at least a portion of the transfer sheet,
an amount of adhesion of the image forming ink per unit area of the transfer sheet is 30 g/m2 or more and 200 g/m2 or less,
an amount of adhesion of the adhesive ink per unit area of the transfer sheet is 30 g/m2 or more and 500 g/m2 or less, and
a total amount of adhesion of the image forming ink and the adhesive ink per unit area of the transfer sheet is 110 g/m2 or more.