# US 2026/0103820 A1 · Method for preparing fullerene single-crystal films and uses field of technology

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0103820 A1
- Document ID: US20260103820A1
- Status: Published application
- Kind: A1
- Application number: 18/873,715
- Filed: 2023-07-26
- Published: 2026-04-16
- Earliest claimed: 2023-07-05
- Assignees: Zhejiang University
- Applicants: Zhejiang University
- Inventors: Hanying LI; Yujie ZHAO; Boyu PENG
- Web page: https://patentgrep.com/patent/US20260103820A1

## CPC

- C30B 7/06: using non-aqueous solvents
- H10K 85/215: {comprising substituents, e.g. PCBM}
- C30B 29/02: Elements
- C30B 29/60: characterised by shape
- H10K 30/30: comprising bulk heterojunctions, e.g. interpenetrating networks of donor and acceptor material domains
- H10K 30/50: Photovoltaic [PV] devices
- H10K 71/12: using liquid deposition, e.g. spin coating
- H10K 71/15: characterised by the solvent used
- H10K 71/191: {characterised by provisions for the orientation or alignment of the layer to be deposited}
- H10K 85/211: {Fullerenes, e.g. C60}
- H10K 99/00: Subject matter not provided for in other groups of this subclass
- H10K 10/484: {characterised by the channel regions}
- H10K 30/20: comprising organic-organic junctions, e.g. donor-acceptor junctions
- Y02E 10/549: Organic PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10K: ORGANIC ELECTRIC SOLID-STATE DEVICES
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present disclosure relates to the field of organic semiconductor technology, it relates to a method for preparing fullerene single-crystal films and uses. A method for preparing fullerene single-crystal films using a gas-liquid-solid three-phase interface, including the following steps: 1) mixing fullerene and solvent to form a mixture; 2) employing a solution shear method to induce crystallization growth of the fullerene in mixture on a substrate surface, thereby obtaining the fullerene single-crystal films. The present disclosure prepares large-area fullerene single-crystal films by directly controlling the nucleation density of fullerenes at the three-phase line and utilizing the continuous movement of the three-phase line. The resulting films have the advantages of uniform alignment, high uniformity, and high coverage. Additionally, they exhibit excellent electronic transport properties, meeting the application requirements in the field of optoelectronics.

## Claims

### Claim 1

A method for preparing fullerene single-crystal films using a gas-liquid-solid three-phase interface, comprising:
1) mixing fullerene and solvent to form a mixture; and
2) employing a solution shear method to induce crystallization growth of the fullerene in mixture on a substrate surface, thereby obtaining the fullerene single-crystal films.

### Claim 2 (depends on 1)

The method according to claim 1, further comprising at least one of following technical features:
A1) the fullerene is one or more of C60, C70, C76, C78, C80, and C84;
A2) the solvent is one or more of ortho-xylene, 2-methylthiophene, 2-chlorothiophene, 2-chloro-furan, 3-methylthiophene, 2-ethylthiophene, meta-xylene, meta-difluorobenzene, chlorobenzene, ortho-dichlorobenzene, 1,2,4-trichlorobenzene, tetrahydronaphthalene, 1-methylnaphthalene, carbon disulfide, 1,1,2,2-tetrachloroethane, carbon tetrachloride, 2-methoxythiophene, phenethyl ether, 2-chloro-3-methylthiophene, and 2,5-dichlorothiophene;
A3) a concentration of the fullerene, based on a total volume of the mixture, is 0.2 mg/mL to 20 mg/mL, preferably 0.4 mg/ml to 10 mg/mL;
A4) a material of the substrate is one or more of silicon, indium tin oxide, glass, quartz, sapphire, polyimide, and polyethylene terephthalate; and
A5) a temperature for the crystallization growth is 20° C. to 120° C., preferably 25° C. to 60° C.

### Claim 3 (depends on 2)

The method according to claim 2, wherein a wetting layer is provided on the substrate.

### Claim 4 (depends on 3)

The method according to claim 3, wherein a material of the wetting layer is one or more of benzocyclobutene, polyvinyl alcohol, cross-linked polymethyl methacrylate, cross-linked polystyrene, aluminum oxide, titanium oxide, zinc oxide, ethoxylated polyethyleneimine, phenyltrichlorosilane, gold, and aluminum.

### Claim 5 (depends on 1)

The method according to claim 1, wherein step 2), the solution shear method comprises using a shear tool positioned above the substrate, such that the mixture is located between the shear tool and the substrate, and either the substrate or the shear tool is operated at a certain linear velocity.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the shear tool is one or more of stainless-steel bar, stainless steel wire bar, polytetrafluoroethylene bar, scrapers, and coating heads;
wherein a distance between the shear tool and the substrate is 20 μm to 400 μm, preferably 50 μm to 200 μm; and
wherein the certain linear velocity in the solution shear method is 1 μm/s to 1 mm/s, preferably 5 μm/s to 200 μm/s.

### Claim 7 (depends on 1)

Fullerene single-crystal films obtained by the method for preparing fullerene single-crystal films using a gas-liquid-solid three-phase interface according to claim 1.

### Claim 8 (depends on 7)

Use of the fullerene single-crystal films according to claim 7 in an optoelectronic device.

### Claim 9 (depends on 7)

An optoelectronic device, wherein the optoelectronic device comprises the fullerene single-crystal films according to claim 7.

### Claim 10 (depends on 9)

The optoelectronic device according to claim 9, wherein the optoelectronic device is one or more of organic field-effect transistors, organic solar cells, organic complementary inverters, organic circuits, organic light-emitting diodes, organic memory devices, organic photodetectors, and organic thermoelectric devices.