# US 2026/0101830 A1 · Uv cure technology for bonding film surface activation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0101830 A1
- Document ID: US20260101830A1
- Status: Published application
- Kind: A1
- Application number: 19/347,187
- Filed: 2025-10-01
- Published: 2026-04-09
- Earliest claimed: 2024-10-09
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Xinyi LU; Han WANG; Bo XIE; Monika Halim JAMIESON; Chi-I LANG; Li-Qun XIA
- Web page: https://patentgrep.com/patent/US20260101830A1

## CPC

- H10W 99/00: Subject matter not provided for in other groups of this subclass
- H10W 72/90: Bond pads, in general
- H10W 80/041: {Thermally treating}
- H10W 80/327: {characterised by the direct bonding of insulating parts, e.g. of silicon oxide layers}
- H10W 90/794: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Embodiments described herein generally relate to processes for back end of line advanced packaging assembly. More particularly, embodiments described herein relate to processes for activating silicon surfaces for hydrophilic silicon direct bonding applications. In at least one embodiment, a method for activating a substrate is provided. The method includes providing a substrate into a process chamber, the substrate including a plurality of patterned structures, at least one metal layer and a silicon surface, and curing the silicon surface of the substrate. The curing process includes flowing one or more gases into the process chamber, the one or more gases including ozone, and providing UV light while operating the process chamber at a temperature of about 25° C. to about 300° C. A plurality of oxygen radicals are formed from the ozone and reacted with the silicon surface of the substrate to form an activated surface.

## Claims

### Claim 1

A method of activating a substrate, comprising:
providing a substrate into a process chamber, the substrate comprising a plurality of patterned structures, at least one metal layer, and a silicon surface;
curing the silicon surface of the substrate, wherein the curing comprises:
flowing one or more gases into the process chamber, the one or more gases comprising ozone;
providing UV light while operating the process chamber at a temperature of about 25° C. to about 300° C.;
forming a plurality of oxygen radicals from the ozone; and
reacting the silicon surface of the substrate with the plurality of oxygen radicals to form an activated surface.

### Claim 2 (depends on 1)

The method of claim 1, wherein the UV light has a wavelength of about 200 nm to about 500 nm.

### Claim 3 (depends on 1)

The method of claim 1, wherein the ozone is flowed into the process chamber at a flow rate of about 1,000 sccm to about 10,000 sccm.

### Claim 4 (depends on 1)

The method of claim 1, wherein the silicon surface of the substrate is cured for about 1 minute to about 20 minutes.

### Claim 5 (depends on 1)

The method of claim 1, wherein the process chamber is operated at a pressure of about 3 Torr to about 760 Torr while providing the UV light.

### Claim 6 (depends on 1)

The method of claim 1, wherein the one or more gases further comprise helium, and the helium is flowed into the process chamber at a flow rate of about 1,000 sccm to about 20,000 sccm.

### Claim 7 (depends on 1)

The method of claim 1, wherein the one or more gases further comprise argon, and the argon is flowed into the process chamber at a flow rate of about 1,000 sccm to about 20,000 sccm.

### Claim 8 (depends on 1)

The method of claim 1, wherein the substrate comprises a plurality of materials disposed below the silicon surface, two or more of the materials of the plurality of materials having different coefficients of thermal expansion.

### Claim 9 (depends on 1)

The method of claim 1, wherein the activated surface has a higher concentration of silicon hydroxide (SiOH) than the silicon surface.

### Claim 10 (depends on 1)

The method of claim 1, wherein the activated surface has a higher k than the silicon surface.

### Claim 11

A method of activating a substrate for direct bonding, comprising:
providing a substrate into a process chamber, the substrate being a back end of line (BEOL) semiconductor comprising a silicon surface;
flowing one or more gases into the process chamber, the one or more gases comprising ozone;
providing UV light while operating the process chamber at a temperature of about 150° C. to about 250° C. and a pressure of about 6 Torr to about 25 Torr; and
curing the silicon surface of the substrate to form an activated surface.

### Claim 12 (depends on 11)

The method of claim 11, wherein the UV light has a wavelength of about 200 nm to about 500 nm.

### Claim 13 (depends on 11)

The method of claim 11, wherein the ozone is flowed into the process chamber at a flow rate of about 1,000 sccm to about 10,000 sccm.

### Claim 14 (depends on 11)

The method of claim 11, wherein the silicon surface of the substrate is cured for about 1 minute to about 20 minutes.

### Claim 15 (depends on 11)

The method of claim 11, wherein the one or more gases further comprise helium, and the helium is flowed into the process chamber at a flow rate of about 1,000 sccm to about 20,000 sccm.

### Claim 16 (depends on 11)

The method of claim 11, wherein the one or more gases further comprise argon, and the argon is flowed into the process chamber at a flow rate of about 1,000 sccm to about 20,000 sccm.

### Claim 17 (depends on 11)

The method of claim 11, wherein the substrate comprises a plurality of materials disposed below the silicon surface, two or more of the materials of the plurality of materials having different coefficients of thermal expansion.

### Claim 18

A method for direct bonding, comprising:
providing a substrate into a process chamber, the substrate being a back end of line (BEOL) semiconductor comprising a silicon surface;
curing the silicon surface, wherein the curing comprises:
flowing one or more gases into the process chamber, the one or more gases comprising ozone;
providing UV light while operating the process chamber at a temperature of about 25° C. to about 300° C.;
forming a plurality of oxygen radicals from the ozone;
reacting the silicon surface of the substrate with the plurality of oxygen radicals to form an activated surface; and
bonding the activated surface to a carrier substrate.

### Claim 19 (depends on 18)

The method of claim 18, wherein the process chamber is operated at a temperature of about 150° C. to about 250° C. and a pressure of about 6 Torr to about 25 Torr while providing the UV light.

### Claim 20 (depends on 18)

The method of claim 18, wherein the carrier substrate is a wafer.