# US 2026/0101800 A1 · Semiconductor device and method of manufacturing semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0101800 A1
- Document ID: US20260101800A1
- Status: Published application
- Kind: A1
- Application number: 19/308,602
- Filed: 2025-08-25
- Published: 2026-04-09
- Earliest claimed: 2024-10-04
- Assignees: Fuji Electric Co., Ltd.
- Applicants: Fuji Electric Co., Ltd.
- Inventors: Tsunehiro NAKAJIMA
- Web page: https://patentgrep.com/patent/US20260101800A1

## CPC

- H10W 72/90: Bond pads, in general
- H10W 72/019: {of bond pads}
- H10W 72/01938: {in gaseous form, e.g. by CVD or PVD}
- H10W 72/923: {Bond pads having multiple stacked layers}
- H10W 72/952: {comprising metals or metalloids, e.g. PbSn, Ag or Cu}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A semiconductor device, including: a semiconductor substrate with a main surface; and a surface electrode provided at the main surface of the semiconductor substrate, the surface electrode having a nickel (Ni) film that includes a fibrous-structure Ni film, the fibrous-structure Ni film containing Ni crystal grains grown to form a fibrous shape.

## Claims

### Claim 1

A semiconductor device, comprising:
a semiconductor substrate with a main surface; and
a surface electrode provided at the main surface of the semiconductor substrate, the surface electrode having a nickel (Ni) film that includes a fibrous-structure Ni film, the fibrous-structure Ni film containing Ni crystal grains grown to form a fibrous shape.

### Claim 2 (depends on 1)

The semiconductor device according to claim 1, wherein
the Ni film further includes a columnar-structure Ni film in contact with the fibrous-structure Ni film, the columnar-structure Ni film containing Ni crystal grains grown to form a columnar shape.

### Claim 3 (depends on 1)

The semiconductor device according to claim 1, wherein
a percentage of a thickness of the fibrous-structure Ni film relative to a thickness of the Ni film is 50% or more but not more than 100%.

### Claim 4 (depends on 2)

The semiconductor device according to claim 2, wherein
the Ni crystal grains of the fibrous-structure Ni film have crystal particle sizes that are larger than those of the Ni crystal grains of the columnar-structure Ni film.

### Claim 5 (depends on 1)

The semiconductor device according to claim 1, wherein
the Ni crystal grains of the fibrous-structure Ni film have crystal particle sizes that are each 0.02 μm or more but not more than 0.2 μm.

### Claim 6 (depends on 2)

The semiconductor device according claim 2, wherein
the Ni crystal grains of the columnar-structure Ni film have crystal particle sizes that are each 0.01 μm or more but not more than 0.05 μm.

### Claim 7

A method of manufacturing a semiconductor device having
a semiconductor substrate with a main surface, and
a surface electrode provided at the main surface of the semiconductor substrate,
the method comprising:
as a deposition process, forming a nickel (Ni) film as the surface electrode, the Ni film being formed at the main surface of the semiconductor substrate, wherein
the deposition process includes performing a first sputtering at a temperature of 25 degrees C or higher but not more than 50 degrees C.

### Claim 8 (depends on 7)

The method of manufacturing the semiconductor device according to claim 7, wherein
the deposition process includes performing the first sputtering under an argon (Ar) atmosphere at a gas pressure of 0.2 Pa or more but not more than 1.2 Pa.

### Claim 9 (depends on 7)

The method of manufacturing the semiconductor device according to claim 7, wherein
the Ni film includes a first portion and a second portion that are mutually exclusive,
the first sputtering forms the first portion of the Ni film, and
the deposition process further includes subsequently performing a second sputtering under a temperature of 100 degrees C or higher but not more than 180 degrees C, to thereby form the second portion of the Ni film.