# US 2026/0101730 A1 · Damage-less hydrogen treatment for molybdenum oxide reduction

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0101730 A1
- Document ID: US20260101730A1
- Status: Published application
- Kind: A1
- Application number: 18/910,618
- Filed: 2024-10-09
- Published: 2026-04-09
- Earliest claimed: 2024-10-09
- Applicants: Applied Materials, Inc.
- Inventors: Ruinan ZHOU; Jiajie CEN; Hsien-Lung YANG; Shashank S. SHARMA; Archana KUMAR
- Web page: https://patentgrep.com/patent/US20260101730A1

## CPC

- H10P 95/00: Generic processes or apparatus for manufacture or treatments not covered by the other groups of this subclass
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

In some embodiments, a method includes positioning a semiconductor structure within a processing chamber. The semiconductor structure includes a first layer disposed over a substrate surface. The semiconductor structure further includes a second layer disposed over the first layer. The second layer has a hardmask layer. The semiconductor structure further includes one or more second dielectric layers disposed over the second layer. The one or more second dielectric layers have a gap formed over a portion of the second layer. The semiconductor structure further includes a metal material disposed within the gap formed over the second layer. The metal material has a molybdenum oxide (MoOx) layer. The method further includes flowing a process gas into the processing chamber, and performing a redox operation on a portion of the semiconductor structure to reduce the MoOx to molybdenum (Mo). The redox operation includes applying a microwave energy to the process gas.

## Claims

### Claim 1

A method, comprising:
positioning a semiconductor structure within a processing volume of a processing chamber, the semiconductor structure comprising:
a first layer disposed over a substrate surface, the first layer comprising a first dielectric layer;
one or more second dielectric layers disposed over the first layer, wherein the one or more second dielectric layers comprise a gap formed through the one or more second dielectric layers; and
a metal material disposed within the gap and a portion of the first layer, the metal material comprising a molybdenum oxide (MoOx) layer;
flowing a process gas into the processing volume of the processing chamber; and
performing a redox operation on a portion of the semiconductor structure to reduce the MoOx to molybdenum (Mo), wherein the redox operation comprises applying a microwave energy to the process gas.

### Claim 2 (depends on 1)

The method of claim 1, wherein the application of the microwave energy does not generate a plasma within the processing volume.

### Claim 3 (depends on 2)

The method of claim 2, wherein the process gas is selected from the group consisting of hydrogen (H2), and water (H2O).

### Claim 4 (depends on 3)

The method of claim 3, wherein the microwave energy is provided at a frequency greater than 2.0 GHz.

### Claim 5 (depends on 1)

The method of claim 1, wherein
the process gas is selected from the group consisting of hydrogen (H2), and water (H2O),
a temperature within the processing chamber is about 100° C. to about 500° C., and
the microwave energy is applied at a power of about 0.1 W to about 150 W.

### Claim 6 (depends on 5)

The method of claim 5, wherein a pressure within the processing chamber is about 10 Torr to about 760 Torr.

### Claim 7

A method, comprising:
positioning a semiconductor structure within a processing volume of a processing chamber, the semiconductor structure comprising:
a first layer disposed over a substrate surface, the first layer comprising a tungsten based material,
one or more dielectric layers disposed over the first layer, wherein the one or more dielectric layers comprise a gap formed over a portion of the first layer, and
a metal material disposed within the gap over the first layer, the metal material comprising a molybdenum oxide (MoOx) layer; and
performing a redox operation on a portion of the semiconductor structure to reduce the MoOx to molybdenum (Mo), wherein performing the redox operation comprises:
flowing a process gas into the processing chamber; and
applying a microwave energy to the process gas disposed within the processing volume, wherein the application of the microwave energy does not generate a plasma within the processing volume.

### Claim 8 (depends on 7)

The method of claim 7, wherein the process gas is selected from the group consisting of hydrogen (H2), and water (H2O).

### Claim 9 (depends on 7)

The method of claim 7, wherein the microwave energy is applied at a frequency greater than about 2.0 GHz and at a power of about 0.1 W to about 150 W.

### Claim 10 (depends on 9)

The method of claim 9, wherein the process gas is selected from the group consisting of hydrogen (H2), and water (H2O).

### Claim 11 (depends on 7)

The method of claim 7, wherein the process gas is flowed into the processing chamber at a gas flow rate of about 0.01 sccm to about 45,000 sccm.

### Claim 12 (depends on 11)

The method of claim 11, wherein a temperature within the processing chamber is about 100° C. to about 500° C.

### Claim 13 (depends on 12)

The method of claim 12, wherein a pressure within the processing chamber is about 10 Torr to about 760 Torr.

### Claim 14 (depends on 13)

The method of claim 13, wherein the redox operation is performed for about 1 s to about 360 s.

### Claim 15

A method, comprising:
positioning a semiconductor structure within a processing chamber, the semiconductor structure comprising:
one or more dielectric layers disposed on a surface of a hardmask layer;
a gap formed through the one or more dielectric layers and the hardmask layer, the one or more dielectric layers comprising a low-k dielectric material at a first carbon content, and
a metal material disposed within the gap, the metal material comprising a first thickness and a first molybdenum oxide (MoOx) content;
flowing a process gas into the processing chamber; and
performing a redox operation on the semiconductor structure by applying a microwave energy to the process gas to form a processed semiconductor structure, the processed semiconductor structure comprising:
the low-k dielectric material at a second carbon content, and
the metal material comprising a second thickness and a second MoOx content, and
the process of applying the microwave energy to the process gas does not generate a plasma.

### Claim 16 (depends on 15)

The method of claim 15, wherein the first carbon content is about 0.001% to about 1% greater than the second carbon content.

### Claim 17 (depends on 15)

The method of claim 15, wherein the second thickness is about 60% to about 90% of the first thickness.

### Claim 18 (depends on 15)

The method of claim 15, wherein the second MoOx content is about 80% to about 99.9% less than the first MoOx content.

### Claim 19 (depends on 15)

The method of claim 15, wherein
the microwave energy is applied at a frequency greater than about 2.0 GHz and at a power of about 0.1 W to about 150 W, and
the process gas is selected from the group consisting of hydrogen (H2), and water (H2O).

### Claim 20 (depends on 19)

The method of claim 19, wherein a pressure within the processing chamber during the redox operation is about 10 Torr to about 760 Torr.