# US 2026/0101728 A1 · Wafer processing method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2026/0101728 A1
- Document ID: US20260101728A1
- Status: Published application
- Kind: A1
- Application number: 19/331,765
- Filed: 2025-09-17
- Published: 2026-04-09
- Earliest claimed: 2024-10-04
- Assignees: Disco Corporation
- Applicants: Disco Corporation
- Inventors: Akira Mizutani; Hayato Iga
- Web page: https://patentgrep.com/patent/US20260101728A1

## CPC

- H10P 90/123: {by grinding or lapping}
- B23K 26/53: for modifying or reforming the material inside the workpiece, e.g. for producing break initiation cracks
- H10P 52/00: Grinding, lapping or polishing of wafers, substrates or parts of devices
- H10P 72/0428: {Apparatus for mechanical treatment or grinding or cutting}
- H10P 90/128: {by edge treatment, e.g. chamfering}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

A wafer processing method for removing a chamfered portion of a first wafer that includes producing a provisionally bonded wafer in which first and second wafers are weakly bonded; forming a ring-shaped modified layer by applying a laser beam to an inner side adjacent to a chamfered portion formed at an outer periphery of the first wafer of the provisionally bonded wafer, and detaching the chamfered portion from the second wafer, with the modified layer serving as a starting point; and producing a completely strongly bonded wafer by annealing the provisionally bonded wafer. The wafer processing method further includes grinding and thinning the first wafer, with the second wafer being held on a chuck table constituting a grinding apparatus, and removing the chamfered portion of the first wafer that is detached from the second wafer, with the modified layer serving as a starting point.

## Claims

### Claim 1

A wafer processing method for bonding a first wafer and a second wafer and processing the first wafer, the wafer processing method comprising:
producing a provisionally bonded wafer in which a first wafer and a second wafer are provisionally bonded with a relatively weak bonding force;
forming a ring-shaped modified layer by applying a laser beam to an inner side adjacent to a chamfered portion formed at an outer periphery of the first wafer of the provisionally bonded wafer, and detaching the chamfered portion from the second wafer, with the modified layer serving as a starting point; and
producing a completely bonded wafer with an increased bonding force obtained by annealing the provisionally bonded wafer,
the wafer processing method further comprising, after the forming the modified layer or after the producing the completely bonded wafer, grinding and thinning the first wafer, with the second wafer being held on a chuck table constituting a grinding apparatus, and removing the chamfered portion of the first wafer that is detached from the second wafer, with the modified layer serving as a starting point.

### Claim 2 (depends on 1)

The wafer processing method of claim 1, wherein the forming the modified layer includes forming a radial modified layer extending outward from the ring-shaped modified layer.

### Claim 3 (depends on 1)

The wafer processing method of claim 1, further comprising, after the producing the provisionally bonded wafer, facilitating chamfered portion detachment by supplying a fluid including at least one of water, water vapor, or mist to an interface of the chamfered portion, at which the first wafer and the second wafer are bonded, so that the fluid enters a region where the chamfered portion can be removed so as to weaken a bonding force.

### Claim 4 (depends on 3)

The wafer processing method of claim 3, wherein the facilitating chamfered portion detachment includes applying an external force to the interface when supplying the fluid to the interface.

### Claim 5 (depends on 1)

The wafer processing method of claim 1, wherein after the producing the provisionally bonded wafer and before the forming the modified layer, pre-grinding is performed to grind the first wafer so as to remove a layer that interferes with a laser beam that is applied in the forming the modified layer.

### Claim 6 (depends on 1)

The wafer processing method of claim 1, wherein
the first wafer and the second wafer are silicon wafers,
in the provisionally bonded wafer, Si and Si are bonded via OH, and
in the completely bonded wafer, Si and Si are bonded via O.